메뉴 건너뛰기





Volumn 19, Issue 4, 1998, Pages 293-301

High-temperature slow crack growth, fracture toughness and room-temperature deformation behavior of plasma-sprayed ZrO2-8 wt % Y2O3

Author keywords

[No Author keywords available]

Indexed keywords

CRACK PROPAGATION; CYCLIC LOADS; FRACTURE TOUGHNESS; HIGH TEMPERATURE PROPERTIES; HYSTERESIS; PLASMA SPRAYING; PROTECTIVE COATINGS; STRAIN; STRESS ANALYSIS; THERMAL INSULATING MATERIALS; ZIRCONIA;

EID: 0032313093     PISSN: 01966219     EISSN: None     Source Type: Conference Proceeding    
DOI: None     Document Type: Article
Times cited : (31)