1
-
-
0024668142
-
Dependence of the vickers indentation fracture toughness on the surface crack length
-
1. Ponton, C. B. and Rawlings, R. D., Dependence of the vickers indentation fracture toughness on the surface crack length. Br. Ceram. Trans. J., 1989, 88, 83-90.
-
(1989)
Br. Ceram. Trans. J.
, vol.88
, pp. 83-90
-
-
Ponton, C.B.1
Rawlings, R.D.2
-
2
-
-
0025401101
-
Fracture resistance behaviour of a silicon carbide whisker reinforced alumina with different porosities
-
2. Krause Jr, R. F. and Fuller Jr, E. R., Fracture resistance behaviour of a silicon carbide whisker reinforced alumina with different porosities. J. Am. Ceram. Soc., 1990, 73(3), 559-566.
-
(1990)
J. Am. Ceram. Soc.
, vol.73
, Issue.3
, pp. 559-566
-
-
Krause R.F., Jr.1
Fuller E.R., Jr.2
-
4
-
-
0025399256
-
R-curve behaviour and thermal shock resistance of ceramics
-
4. Swain, M. V., R-curve behaviour and thermal shock resistance of ceramics. J. Am. Ceram. Soc., 1990, 73(3), 621-628.
-
(1990)
J. Am. Ceram. Soc.
, vol.73
, Issue.3
, pp. 621-628
-
-
Swain, M.V.1
-
5
-
-
0025507465
-
Technique for the R-curve determination of Y-TZP using indentation-produced flaws
-
5. Anderson, R. M. and Braun, L. M., Technique for the R-curve determination of Y-TZP using indentation-produced flaws. J. Am. Ceram. Soc., 1990, 73(10), 3059-3062.
-
(1990)
J. Am. Ceram. Soc.
, vol.73
, Issue.10
, pp. 3059-3062
-
-
Anderson, R.M.1
Braun, L.M.2
-
6
-
-
84925270777
-
Rising crack growth resistance R-curve behaviour of toughened alumina and silicon nitride
-
6. Ramachandran, N. and Shetty, D. K., Rising crack growth resistance R-curve behaviour of toughened alumina and silicon nitride. J. Am. Ceram. Soc., 1991, 74(10), 2634-2641.
-
(1991)
J. Am. Ceram. Soc.
, vol.74
, Issue.10
, pp. 2634-2641
-
-
Ramachandran, N.1
Shetty, D.K.2
-
7
-
-
0025414937
-
Cyclic fatigue-crack propagation in magnesia-partially stabilized zirconia ceramics
-
7. Dauskardt, R. H., Marshall, D. B. and Ritchie, R. O., Cyclic fatigue-crack propagation in magnesia-partially stabilized zirconia ceramics. J. Am. Ceram. Soc., 1990, 73(4), 893-903.
-
(1990)
J. Am. Ceram. Soc.
, vol.73
, Issue.4
, pp. 893-903
-
-
Dauskardt, R.H.1
Marshall, D.B.2
Ritchie, R.O.3
-
8
-
-
0026797011
-
Cyclic fatigue crack growth in a SiC-whisker-reinforced alumina ceramic composite: Long and small crack behaviour
-
8. Dauskardt, R. H., James, M. R., Porter, J. R. and Ritchie, R. O., Cyclic fatigue crack growth in a SiC-whisker-reinforced alumina ceramic composite: long and small crack behaviour. J. Am. Ceram. Soc., 1992, 75(4), 759-771.
-
(1992)
J. Am. Ceram. Soc.
, vol.75
, Issue.4
, pp. 759-771
-
-
Dauskardt, R.H.1
James, M.R.2
Porter, J.R.3
Ritchie, R.O.4
-
9
-
-
0019717650
-
-
ed. H. H. Hausner, H. W. Antes and G. D. Smith. Plenum, New York
-
9. Sadahiro, T. and Takatsu, S., In Modern Developments in Powder Metallurgy, Vol. 14, ed. H. H. Hausner, H. W. Antes and G. D. Smith. Plenum, New York, 1981, pp. 561-572.
-
(1981)
Modern Developments in Powder Metallurgy
, vol.14
, pp. 561-572
-
-
Sadahiro, T.1
Takatsu, S.2
-
10
-
-
0021218431
-
Creation of stable cracks in hard metals using bridge indentation
-
10. Warren, R. and Johannesson, B., Creation of stable cracks in hard metals using bridge indentation. Powder Metall, 1984, 27(1), 25-29.
-
(1984)
Powder Metall
, vol.27
, Issue.1
, pp. 25-29
-
-
Warren, R.1
Johannesson, B.2
-
11
-
-
84986376771
-
Fracture toughness anisotrophy and toughening mechanisms of a hot pressed alumina reinforced with silicon carbide whiskers
-
11. Hansson, T., Warren, R. and Wasen, J., Fracture toughness anisotrophy and toughening mechanisms of a hot pressed alumina reinforced with silicon carbide whiskers. J. Am. Ceramic. Soc., 1993, 74(4), 841-848.
-
(1993)
J. Am. Ceramic. Soc.
, vol.74
, Issue.4
, pp. 841-848
-
-
Hansson, T.1
Warren, R.2
Wasen, J.3
-
12
-
-
0024016154
-
Evaluation of fracture toughness for ceramic materials by a single-edged-precracked-beam method
-
12. Nose, T. and Fuji, T., Evaluation of fracture toughness for ceramic materials by a single-edged-precracked-beam method. J. Am. Ceram. Soc, 1988, 71(5), 328.
-
(1988)
J. Am. Ceram. Soc
, vol.71
, Issue.5
, pp. 328
-
-
Nose, T.1
Fuji, T.2
-
13
-
-
0025474782
-
Fracture toughness of ceramic precracked bend bars
-
13. Baron, I., Beals, J. T. and Gary, L., Fracture toughness of ceramic precracked bend bars. J. Am. Ceram. Soc., 1990, 73(8), 2519-2522.
-
(1990)
J. Am. Ceram. Soc.
, vol.73
, Issue.8
, pp. 2519-2522
-
-
Baron, I.1
Beals, J.T.2
Gary, L.3
-
14
-
-
0029673114
-
Fatigue crack growth rate and fracture toughness of 25 wt% silicon carbide whisker reinforced alumina ceramic composite with residual porosity
-
14. Ray, A. K., Fuller Jr, E. R. and Banerjee, S., Fatigue crack growth rate and fracture toughness of 25 wt% silicon carbide whisker reinforced alumina ceramic composite with residual porosity. J. Eur. Ceramic. Soc., 1996, 16, 503-513.
-
(1996)
J. Eur. Ceramic. Soc.
, vol.16
, pp. 503-513
-
-
Ray, A.K.1
Fuller E.R., Jr.2
Banerjee, S.3
-
15
-
-
0028543367
-
Fractography as well as fatigue and fracture of 25 wt% silicon carbide whisker reinforced alumina ceramic composite
-
15. Ray, A. K., Banerjee, S., Fuller Jr, E. R., Das, S. K. and Das, G., Fractography as well as fatigue and fracture of 25 wt% silicon carbide whisker reinforced alumina ceramic composite. Bull. Mat. Sc., 1994, 17(6), 893-910.
-
(1994)
Bull. Mat. Sc.
, vol.17
, Issue.6
, pp. 893-910
-
-
Ray, A.K.1
Banerjee, S.2
Fuller E.R., Jr.3
Das, S.K.4
Das, G.5
-
16
-
-
0029232417
-
Fractography of the fatigued and fractured regions in a silicon carbide whisker reinforced alumina composite
-
16. Ray, A. K., Das, S. K., Roy, P. K. and Banerjee, S., Fractography of the fatigued and fractured regions in a silicon carbide whisker reinforced alumina composite. J. Eur. Ceram Soc., 1995, 15, 191-199.
-
(1995)
J. Eur. Ceram Soc.
, vol.15
, pp. 191-199
-
-
Ray, A.K.1
Das, S.K.2
Roy, P.K.3
Banerjee, S.4
-
17
-
-
0042360518
-
-
American Society for Testing and Materials, Philadelphia, PA
-
17. Brown Jr, W. F. and Srawley, J. E., In ASTM STP 410. American Society for Testing and Materials, Philadelphia, PA, 1966.
-
(1966)
ASTM STP 410
-
-
Brown W.F., Jr.1
Srawley, J.E.2
-
18
-
-
0041358787
-
Acoustic emission study for fracture origin of sintered mullite in 4-point bending test
-
18. Yamade, Y. and Kishi, T., Acoustic emission study for fracture origin of sintered mullite in 4-point bending test. The Sumitomo Search, 1991, 45(3), 17-24.
-
(1991)
The Sumitomo Search
, vol.45
, Issue.3
, pp. 17-24
-
-
Yamade, Y.1
Kishi, T.2
-
20
-
-
0025474942
-
Residual stresses in alumina/silicon carbide (whisker) composites by X-ray diffraction
-
20. Abuhasan, A., Balasingh, C. and Predecki, P., Residual stresses in alumina/silicon carbide (whisker) composites by X-ray diffraction. J. Am. Ceram. Soc., 1990, 73(8), 2474-2484.
-
(1990)
J. Am. Ceram. Soc.
, vol.73
, Issue.8
, pp. 2474-2484
-
-
Abuhasan, A.1
Balasingh, C.2
Predecki, P.3
-
21
-
-
84987299776
-
Effect of machining damage on the strength of a glass ceramic
-
21. Cook, R. F., Lawn, B. R., Dabbs, T. P. and Chantikul, P., Effect of machining damage on the strength of a glass ceramic. J. Am. Ceram. Soc., 1981, 64, C121.
-
(1981)
J. Am. Ceram. Soc.
, vol.64
-
-
Cook, R.F.1
Lawn, B.R.2
Dabbs, T.P.3
Chantikul, P.4
-
22
-
-
0020810808
-
Factors influencing residual surface stresses due to a stress-induced phase transformation
-
22. Green, D. J., Lange, F. F. and James, M. R., Factors influencing residual surface stresses due to a stress-induced phase transformation. J. Am. Ceram. Soc., 1983, 66, 623-629.
-
(1983)
J. Am. Ceram. Soc.
, vol.66
, pp. 623-629
-
-
Green, D.J.1
Lange, F.F.2
James, M.R.3
-
23
-
-
84980232774
-
An indentation technique for measuring stresses in tempered glass-surfaces
-
23. Marshall, D. B. and Lawn, B. R., An indentation technique for measuring stresses in tempered glass-surfaces. J. Am. Ceram. Soc., 1977, 60, 86-87.
-
(1977)
J. Am. Ceram. Soc.
, vol.60
, pp. 86-87
-
-
Marshall, D.B.1
Lawn, B.R.2
-
24
-
-
0021455455
-
Crack-size dependence of fracture toughness in transformation-toughened ceramics
-
24. Ikuma, Y. and Virkar, A. V., Crack-size dependence of fracture toughness in transformation-toughened ceramics. J. Mater. Sci., 1984, 19, 2223-2228.
-
(1984)
J. Mater. Sci.
, vol.19
, pp. 2223-2228
-
-
Ikuma, Y.1
Virkar, A.V.2
-
25
-
-
0344292283
-
Acoustic emission studies during indentation on ceramic and ceramic composite
-
ed. C. G. K. Nain, Baldevraj, C. R. L. Murthy and T. Jaykuma, Oxford and IBH Publishing House
-
25. Ray, A. K., Bhattacharya, D. K. and Das, G., Acoustic emission studies during indentation on ceramic and ceramic composite. In Proceedings of 14th World Conference on Non Destructive Testing (WCNDT), Vol. 4, ed. C. G. K. Nain, Baldevraj, C. R. L. Murthy and T. Jaykuma, Oxford and IBH Publishing House, 1996, pp. 2445-2448.
-
(1996)
Proceedings of 14th World Conference on Non Destructive Testing (WCNDT)
, vol.4
, pp. 2445-2448
-
-
Ray, A.K.1
Bhattacharya, D.K.2
Das, G.3
|