Volumn 29, Issue 11, 1998, Pages 2669-2677

Characterization by thermoelectric power of a commercial aluminum-lron-silicon alloy (8011) during isothermal precipitation

Author keywords

[No Author keywords available]

Indexed keywords

ACTIVATION ENERGY; ADDITION REACTIONS; ALLOYING; CHARACTERIZATION; CRYSTAL MICROSTRUCTURE; IRON; PRECIPITATION (CHEMICAL); REACTION KINETICS; SILICON; STRAIN HARDENING; SUPERSATURATION; THERMOELECTRICITY;

EID: 0032203697     PISSN: 10735623     EISSN: None     Source Type: Journal    
DOI: 10.1007/s11661-998-0307-7     Document Type: Article
Times cited : (30)

References (30)
  • 6
  • 7
  • 23
    • 33645905047 scopus 로고
    • ed., ASM, Metals Park, OH
    • Aluminum, J.E. Hatch, ed., ASM, Metals Park, OH, 1984, pp. 140 and 205-6.
    • (1984) , vol.140 , pp. 205-206
    • Hatch, A.J.E.1
  • 24
    • 33645954821 scopus 로고
    • Ph.D. Thesis, Université de Lyon, Lyon, France
    • J.M. Pelletier: Ph.D. Thesis, Université de Lyon, Lyon, France, 1980.
    • (1980)
    • Pelletier, J.M.1
  • 27
  • 29
    • 0025567867 scopus 로고
    • J. Lendvai: Eng. Mater., 1990, vols. 44-45, pp. 1-16.
    • (1990) Eng. Mater. , vol.44-45 , pp. 1-16
    • Lendvai, J.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.