Volumn 39-40, Issue , 1998, Pages 427-432

Hydrogen and helium retention properties of B4C and SiC converted graphites

Author keywords

[No Author keywords available]

Indexed keywords

BORON CARBIDE; DESORPTION; GRAPHITE; HELIUM; HYDROGEN; HYDROGEN BONDS; ION BEAMS; ION BOMBARDMENT; SILICON CARBIDE; SPECTROSCOPIC ANALYSIS;

EID: 0032158126     PISSN: 09203796     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0920-3796(98)00156-2     Document Type: Article
Times cited : (28)

References (27)
  • 1
    • 0026156243 scopus 로고
    • Plasma-surface interactions of graphite as nuclear fusion material
    • T. Yamashina, T. Hino, Plasma-surface interactions of graphite as nuclear fusion material, Appl. Surf. Sci. 48-49 (1991) 483-497.
    • (1991) Appl. Surf. Sci. , vol.48-49 , pp. 483-497
    • Yamashina, T.1    Hino, T.2
  • 2
    • 0344095240 scopus 로고
    • Properties required for isotropic graphite as first wall component of fusion device
    • T. Hino, T. Yamashina, Properties required for isotropic graphite as first wall component of fusion device, Tanso (in Japanese) 130 (1987) 118-123.
    • (1987) Tanso (in Japanese) , vol.130 , pp. 118-123
    • Hino, T.1    Yamashina, T.2
  • 4
    • 0026414592 scopus 로고
    • Chemical sputtering and radiation enhanced sublimation of graphite due to hydrogen ions
    • T. Hino, T. Yamashina, S. Fukuda, Y. Takasugi, Chemical sputtering and radiation enhanced sublimation of graphite due to hydrogen ions, J. Nucl. Mater. 186 (1991) 54-60.
    • (1991) J. Nucl. Mater. , vol.186 , pp. 54-60
    • Hino, T.1    Yamashina, T.2    Fukuda, S.3    Takasugi, Y.4
  • 5
    • 0346878159 scopus 로고
    • Schemes for reduction of helium ash in a fusion reactor
    • T. Hino, Schemes for reduction of helium ash in a fusion reactor, Bull. Fac. Eng. Hokkaido Univ. 175 (1995) 51-57.
    • (1995) Bull. Fac. Eng. Hokkaido Univ. , vol.175 , pp. 51-57
    • Hino, T.1
  • 8
    • 0040908855 scopus 로고
    • Erosion and redeposition behavior of selected net-candidate materials under high-flux hydrogen, deuterium plasma bombardment in PISCES
    • E. Franconi, Y. Hirooka, R.W. Conn, W.K. Leung, B. Labombard, R.E. Nygren, Erosion and redeposition behavior of selected net-candidate materials under high-flux hydrogen, deuterium plasma bombardment in PISCES, J. Nucl. Mater. 162-164 (1989) 892-897.
    • (1989) J. Nucl. Mater. , vol.162-164 , pp. 892-897
    • Franconi, E.1    Hirooka, Y.2    Conn, R.W.3    Leung, W.K.4    Labombard, B.5    Nygren, R.E.6
  • 9
    • 0000163708 scopus 로고
    • A boronization system in the JT-60U Tokamak: Application of a new method using a less hazardous substance
    • M. Saidoh, H. Hiratsuka, T. Arai, Y. Neyatani, M. Shimada, T. Koike, A boronization system in the JT-60U Tokamak: Application of a new method using a less hazardous substance, Fusion Eng. Des. 22 (1993) 3276-3281.
    • (1993) Fusion Eng. Des. , vol.22 , pp. 3276-3281
    • Saidoh, M.1    Hiratsuka, H.2    Arai, T.3    Neyatani, Y.4    Shimada, M.5    Koike, T.6
  • 13
    • 3342974844 scopus 로고
    • A comparison of Tokamak operation with metallic getters (Ti, Cr, Be) and boronization
    • J. Winter, A comparison of Tokamak operation with metallic getters (Ti, Cr, Be) and boronization, J. Nucl. Mater. 176-177 (1990) 14.
    • (1990) J. Nucl. Mater. , vol.176-177 , pp. 14
    • Winter, J.1
  • 17
    • 0030165039 scopus 로고    scopus 로고
    • Hydrogen retention properties of SiC converted graphite
    • Y. Yamauchi, T. Hino, Y. Hirohata, T. Yamashina, Hydrogen retention properties of SiC converted graphite, Vacuum 47 (1996) 973-975.
    • (1996) Vacuum , vol.47 , pp. 973-975
    • Yamauchi, Y.1    Hino, T.2    Hirohata, Y.3    Yamashina, T.4
  • 18
    • 84970079277 scopus 로고
    • Saturation and isotropic replacement of deuterium in low-Z materials
    • B.L. Doyle, W.R. Wampler, D.K. Brice, S.T. Picraux, Saturation and isotropic replacement of deuterium in low-Z materials, J. Nucl. Mater. 93-94 (1980) 511-557.
    • (1980) J. Nucl. Mater. , vol.93-94 , pp. 511-557
    • Doyle, B.L.1    Wampler, W.R.2    Brice, D.K.3    Picraux, S.T.4
  • 20
    • 0344957378 scopus 로고
    • Quantitative mass spectrometric analysis of mixed gases released from various materials
    • Y. Nakayama, S. Fukuda, T. Yamashina, Quantitative mass spectrometric analysis of mixed gases released from various materials (in Japanese), J. Vac. Soc. Jpn. 32 (1989) 301-304.
    • (1989) J. Vac. Soc. Jpn. , vol.32 , pp. 301-304
    • Nakayama, Y.1    Fukuda, S.2    Yamashina, T.3
  • 21
    • 0342778780 scopus 로고
    • Thermal desorption of gases
    • P.A. Redhead, Thermal desorption of gases, Vacuum 12 (1962) 203-211.
    • (1962) Vacuum , vol.12 , pp. 203-211
    • Redhead, P.A.1
  • 22
    • 0000870241 scopus 로고
    • Desorption processes of hydrogen and methane from clean and metal-deposited graphite irradiated by hydrogen ions
    • S. Fukuda, T. Hino, T. Yamashina, Desorption processes of hydrogen and methane from clean and metal-deposited graphite irradiated by hydrogen ions, J. Nucl. Mater. 162-164 (1989) 997-1003.
    • (1989) J. Nucl. Mater. , vol.162-164 , pp. 997-1003
    • Fukuda, S.1    Hino, T.2    Yamashina, T.3
  • 23
    • 0000575069 scopus 로고
    • Hydrogen trapping and transport in carbon
    • W. Möller, Hydrogen trapping and transport in carbon, J. Nucl. Mater. 162-164 (1989) 138-150.
    • (1989) J. Nucl. Mater. , vol.162-164 , pp. 138-150
    • Möller, W.1
  • 24
    • 0024035594 scopus 로고
    • Graphite as plasma facing material
    • A. Miyahara, T. Tanabe, Graphite as plasma facing material, J. Nucl. Mater. 155-157 (1988) 49.
    • (1988) J. Nucl. Mater. , vol.155-157 , pp. 49
    • Miyahara, A.1    Tanabe, T.2
  • 26
    • 0008366940 scopus 로고
    • Helium re-emission, desorption and microstructure evolution of graphites under helium ion implantation
    • V. Kh. Alimov, B.M.U Scherzer, V.N. Chernikov, H. Ullmaier, Helium re-emission, desorption and microstructure evolution of graphites under helium ion implantation, J. Appl. Phys. 78 (1) (1995) 137-148.
    • (1995) J. Appl. Phys. , vol.78 , Issue.1 , pp. 137-148
    • Alimov, V.Kh.1    Scherzer, B.M.U.2    Chernikov, V.N.3    Ullmaier, H.4
  • 27
    • 0020205920 scopus 로고
    • Retention, re-emission and thermal desorption of He implanted into pyrolotic graphite
    • W. Möller, B.M.U. Scherzer, J. Ehrenberg, Retention, re-emission and thermal desorption of He implanted into pyrolotic graphite, J. Nucl. Mater. 111-112 (1982) 669-673.
    • (1982) J. Nucl. Mater. , vol.111-112 , pp. 669-673
    • Möller, W.1    Scherzer, B.M.U.2    Ehrenberg, J.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.