Formation of an α-SiAlON layer on β-SiAlON and its effect on mechanical properties

Author keywords

[No Author keywords available]

Indexed keywords

BENDING STRENGTH; HARDNESS; NITRIDES; OXIDATION RESISTANCE; POWDERS; SINTERING; SURFACE TREATMENT; THICKNESS CONTROL; WEAR RESISTANCE;

EID: 0032117176     PISSN: 00027820     EISSN: None     Source Type: Journal    
DOI: 10.1111/j.1151-2916.1998.tb02565.x     Document Type: Article
Times cited : (21)

References (25)
  • 1
    • 0027149646 scopus 로고
    • SiAlON Ceramics: Retrospect and Prospect
    • Boston, MA Edited by I-W. Chen, P. F. Becher, M. Mitomo, G. Petzow, and T.-S. Yen. Materials Research Society, Pittsburgh, PA
    • K. H. Jack, "SiAlON Ceramics: Retrospect and Prospect"; pp. 15-28 in Silicon Nitride Ceramics: Scientific and Technological Advances, Materials Research Society Symposium Proceedings, Vol. 287 (Boston, MA 1992). Edited by I-W. Chen, P. F. Becher, M. Mitomo, G. Petzow, and T.-S. Yen. Materials Research Society, Pittsburgh, PA, 1993.
    • (1992) Silicon Nitride Ceramics: Scientific and Technological Advances, Materials Research Society Symposium Proceedings , vol.287 , pp. 15-28
    • Jack, K.H.1
  • 3
    • 0000422123 scopus 로고
    • Mixed α- and β-(Si-Al-O-N) Materials with Yttria and Neodymia Additions
    • T. Ekström P.-O. Käll, M. Nygren, and P.-O. Olsson, "Mixed α- and β-(Si-Al-O-N) Materials with Yttria and Neodymia Additions,β Mater. Sci. Eng., A. A105/106, 161-68 (1988).
    • (1988) Mater. Sci. Eng., A. , vol.106 A105 , pp. 161-168
    • Ekström, T.1    Käll, P.-O.2    Nygren, M.3    Olsson, P.-O.4
  • 4
    • 0022753987 scopus 로고
    • Microstructural Investigation of Alpha-Beta Yttrium SiAlON Materials
    • C. Chatfield, T. Ekström, and M. Mikus, "Microstructural Investigation of Alpha-Beta Yttrium SiAlON Materials." J. Mater. Sci., 21, 2297-307 (1986).
    • (1986) J. Mater. Sci. , vol.21 , pp. 2297-2307
    • Chatfield, C.1    Ekström, T.2    Mikus, M.3
  • 6
    • 0026243859 scopus 로고
    • Sintering, Properties and Applications of Silicon Nitride and Sialon Ceramics
    • M. Mitomo and Y. Tajima, "Sintering, Properties and Applications of Silicon Nitride and Sialon Ceramics," J. Ceram. Soc. Jpn., 99 [10] 1014-25 (1991).
    • (1991) J. Ceram. Soc. Jpn. , vol.99 , Issue.10 , pp. 1014-1025
    • Mitomo, M.1    Tajima, Y.2
  • 7
    • 84987318407 scopus 로고
    • Strengthening of Alumina by Reactions with Silicon Film on the Surface and Effects of Ion Irradiation
    • S. Noda, H. Doi, T. Hioki, J.-I. Kawamoto, and O. Kamigaito, "Strengthening of Alumina by Reactions with Silicon Film on the Surface and Effects of Ion Irradiation," J. Am. Ceram. Soc., 69 [9] C-210-C-212 (1986).
    • (1986) J. Am. Ceram. Soc. , vol.69 , Issue.9
    • Noda, S.1    Doi, H.2    Hioki, T.3    Kawamoto, J.-I.4    Kamigaito, O.5
  • 8
    • 84987277785 scopus 로고
    • Surface Modification of Ceramics by Partial Infiltration
    • S. J. Glass and D. J. Green, "Surface Modification of Ceramics by Partial Infiltration," Adv. Ceram. Mater., 2 [2] 129-31 (1987).
    • (1987) Adv. Ceram. Mater. , vol.2 , Issue.2 , pp. 129-131
    • Glass, S.J.1    Green, D.J.2
  • 9
    • 0027640878 scopus 로고
    • Surface Strengthening of Alumina-Zirconia Composite by Addition of Molybdenum Dioxide
    • Y.-S. Shin and S.-J. L. Kang, "Surface Strengthening of Alumina-Zirconia Composite by Addition of Molybdenum Dioxide," J. Am. Ceram. Soc., 76 [8] 2142-44 (1993).
    • (1993) J. Am. Ceram. Soc. , vol.76 , Issue.8 , pp. 2142-2144
    • Shin, Y.-S.1    Kang, S.-J.L.2
  • 10
    • 0028207844 scopus 로고
    • Surface Toughening of Liquid Phase Sintered Silicon Carbide by Surface Nitridation
    • P. Greil, H. G. Bossemeyer, A. Klüner, D. L. Jiang, and J. H. She, "Surface Toughening of Liquid Phase Sintered Silicon Carbide by Surface Nitridation," J. Eur. Ceram. Soc., 13, 159-66 (1994).
    • (1994) J. Eur. Ceram. Soc. , vol.13 , pp. 159-166
    • Greil, P.1    Bossemeyer, H.G.2    Klüner, A.3    Jiang, D.L.4    She, J.H.5
  • 11
    • 84986346802 scopus 로고
    • Strengthening of Silicon Carbide Ceramics by Surface Nitridation during Hot Isostatic Pressing
    • D. L. Jiang, J. H. She, S. H. Tan, and P. Greil, "Strengthening of Silicon Carbide Ceramics by Surface Nitridation during Hot Isostatic Pressing," J. Am. Ceram. Soc., 75 [9] 2586-89 (1992).
    • (1992) J. Am. Ceram. Soc. , vol.75 , Issue.9 , pp. 2586-2589
    • Jiang, D.L.1    She, J.H.2    Tan, S.H.3    Greil, P.4
  • 12
    • 0024928299 scopus 로고
    • Surface Nitridation of Silicon Carbide Ceramics
    • T. Arahori and N. Iwamoto, "Surface Nitridation of Silicon Carbide Ceramics," J. Ceram. Soc. Jpn., 97 [11] 1347-53 (1989).
    • (1989) J. Ceram. Soc. Jpn. , vol.97 , Issue.11 , pp. 1347-1353
    • Arahori, T.1    Iwamoto, N.2
  • 13
    • 0025559851 scopus 로고
    • High Temperature Oxidation Protection Coatings for Monolithic or Composite Ceramics
    • J. Desmaison, "High Temperature Oxidation Protection Coatings for Monolithic or Composite Ceramics," Werkst. Korros., 41, 749-50 (1990).
    • (1990) Werkst. Korros. , vol.41 , pp. 749-750
    • Desmaison, J.1
  • 14
    • 0028167191 scopus 로고
    • Improvement of Oxidation Behavior of Dense Silicon Nitride by Surface Modification
    • Chr. Taut, M. Herrmann, G. Groβe, P. Thiele, and Y. Gogotsi, "Improvement of Oxidation Behavior of Dense Silicon Nitride by Surface Modification," J. Eur. Ceram. Soc., 13, 239-46 (1994).
    • (1994) J. Eur. Ceram. Soc. , vol.13 , pp. 239-246
    • Taut, Chr.1    Herrmann, M.2    Große, G.3    Thiele, P.4    Gogotsi, Y.5
  • 16
    • 11644322159 scopus 로고
    • Testing Methods for Fracture Toughness of High Performance Ceramics
    • "Testing Methods for Fracture Toughness of High Performance Ceramics," Korea Industrial Standard L1600, 1990.
    • (1990) Korea Industrial Standard L1600
  • 17
    • 0029289227 scopus 로고
    • Wear and Wear Transition Mechanism in Silicon Carbide during Sliding
    • S.-J. Cho, C.-D. Um, and S.-S. Kim, "Wear and Wear Transition Mechanism in Silicon Carbide during Sliding," J. Am. Ceram. Soc., 78 [4] 1076-78 (1995).
    • (1995) J. Am. Ceram. Soc. , vol.78 , Issue.4 , pp. 1076-1078
    • Cho, S.-J.1    Um, C.-D.2    Kim, S.-S.3
  • 18
    • 0027881865 scopus 로고
    • Phase Transformation from α′-to β′-Sialon by Liquid Infiltration in Y-Si-Al-O-N System
    • S. M. Han, S.-J. L. Kang, and Y.-T. Lee, "Phase Transformation from α′-to β′-Sialon by Liquid Infiltration in Y-Si-Al-O-N System,′ J. Eur. Ceram. Soc., 12, 431-34 (1993).
    • (1993) J. Eur. Ceram. Soc. , vol.12 , pp. 431-434
    • Han, S.M.1    Kang, S.-J.L.2    Lee, Y.-T.3
  • 20
    • 84985155829 scopus 로고
    • Solubility Limits of α′-SiAlON Solid Solutions in the System Si,Al,Y/N,O
    • W.-Y. Sun, T.-Y. Tien, and T.-S. Yen, ′Solubility Limits of α′-SiAlON Solid Solutions in the System Si,Al,Y/N,O," J. Am. Ceram. Soc., 74 [10] 2547-50 (1991).
    • (1991) J. Am. Ceram. Soc. , vol.74 , Issue.10 , pp. 2547-2550
    • Sun, W.-Y.1    Tien, T.-Y.2    Yen, T.-S.3
  • 25
    • 0018492352 scopus 로고
    • Phase Equilibria in the Oxidation of Impure Silicon Nitride
    • R. O. Williams and V. J. Tennery, "Phase Equilibria in the Oxidation of Impure Silicon Nitride," J. Mater. Sci., 14, 1567-71 (1979).
    • (1979) J. Mater. Sci. , vol.14 , pp. 1567-1571
    • Williams, R.O.1    Tennery, V.J.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.