메뉴 건너뛰기




Volumn 34, Issue 2 PART 2, 1998, Pages 575-587

Effect of diamondlike carbon coating and surface topography on the performance of metal evaporated magnetic tapes

Author keywords

Friction; Hard carbon; Tape drives; Wear

Indexed keywords

CARBON; COATINGS; FRICTION; MAGNETIC TAPE STORAGE; PERFORMANCE; TAPE DRIVES; WEAR OF MATERIALS;

EID: 0032022094     PISSN: 00189464     EISSN: None     Source Type: Journal    
DOI: 10.1109/20.661494     Document Type: Article
Times cited : (22)

References (15)
  • 4
    • 0030245156 scopus 로고    scopus 로고
    • "Tribological evaluation of the streaming mode performance of metal evaporated and metal particle tapes,"
    • S. T. Patton and B. Bhushan, "Tribological evaluation of the streaming mode performance of metal evaporated and metal particle tapes," IEEE Trans. Magn., vol. 32, pp. 3684-3686, 1996.
    • (1996) IEEE Trans. Magn. , vol.32 , pp. 3684-3686
    • Patton, S.T.1    Bhushan, B.2
  • 5
    • 0031430328 scopus 로고    scopus 로고
    • "Friction, wear, and magnetic performance of metal evaporated and particulate magnetic tapes,"
    • S. T. Patton and B. Bhushan, "Friction, wear, and magnetic performance of metal evaporated and particulate magnetic tapes," Proc. Inst. Mech. Eng. Part J: J. Eng. Tribal., vol. 211, 1997.
    • (1997) Proc. Inst. Mech. Eng. Part J: J. Eng. Tribal. , vol.211
    • Patton, S.T.1    Bhushan, B.2
  • 6
    • 0027303507 scopus 로고
    • "Wear mechanisms of Co-Cr sputter deposited magnetic tapes in helical scan video tape recorders,"
    • H. Osaki, H. Uchiyama, and N. Honda, "Wear mechanisms of Co-Cr sputter deposited magnetic tapes in helical scan video tape recorders," IEEE Trans. Magn., vol. 29, pp. 41-58, 1993.
    • (1993) IEEE Trans. Magn. , vol.29 , pp. 41-58
    • Osaki, H.1    Uchiyama, H.2    Honda, N.3
  • 7
    • 0029405916 scopus 로고
    • "Advanced metal evaporated tape,"
    • T. Kawana, S. Onodera, and T. Samoto, "Advanced metal evaporated tape," IEEE Trans. Magn., vol. 31, pp. 2865-2870, 1995.
    • (1995) IEEE Trans. Magn. , vol.31 , pp. 2865-2870
    • Kawana, T.1    Onodera, S.2    Samoto, T.3
  • 8
    • 0000591312 scopus 로고    scopus 로고
    • "Environmental effects on the pause mode performance of metal evaporated and metal particle tapes,"
    • S. T. Patton and B. Bhushan, "Environmental effects on the pause mode performance of metal evaporated and metal particle tapes," J. Appl. Phys., vol. 79, pp. 5802-5804, 1996.
    • (1996) J. Appl. Phys. , vol.79 , pp. 5802-5804
    • Patton, S.T.1    Bhushan, B.2
  • 9
    • 0031188555 scopus 로고    scopus 로고
    • "Environmental effects on the streaming mode performance of metal evaporated and metal particle tapes,"
    • S. T. Patton and B. Bhushan, "Environmental effects on the streaming mode performance of metal evaporated and metal particle tapes," IEEE Trans. Magn., vol. 33, pp. 2513-2530, 1997.
    • (1997) IEEE Trans. Magn. , vol.33 , pp. 2513-2530
    • Patton, S.T.1    Bhushan, B.2
  • 10
    • 0029676451 scopus 로고    scopus 로고
    • "Friction and wear of metal particle, barium ferrite, and metal evaporated tapes in rotary head recorders,"
    • S. T. Patton and B. Bhushan, "Friction and wear of metal particle, barium ferrite, and metal evaporated tapes in rotary head recorders," ASME J. Tribal., vol. 118, pp. 21-32, 1996.
    • (1996) ASME J. Tribal. , vol.118 , pp. 21-32
    • Patton, S.T.1    Bhushan, B.2
  • 11
    • 0028550052 scopus 로고
    • "Running characteristics of MIG heads against MP, barium ferrite and ME tapes,"
    • T. Tsuchiya and B. Bhushan, "Running characteristics of MIG heads against MP, barium ferrite and ME tapes," IEEE Trans. Magn., vol. 30, pp. 4182-4184, 1994.
    • (1994) IEEE Trans. Magn. , vol.30 , pp. 4182-4184
    • Tsuchiya, T.1    Bhushan, B.2
  • 12
    • 0029392248 scopus 로고
    • "Effect of interchanging tapes and head contour on the durability of metal evaporated, metal particle, and barium ferrite magnetic tapes,"
    • S. T. Patton and B. Bhushan, "Effect of interchanging tapes and head contour on the durability of metal evaporated, metal particle, and barium ferrite magnetic tapes," Tribal. Trans., vol. 38, pp. 801-810, 1995.
    • (1995) Tribal. Trans. , vol.38 , pp. 801-810
    • Patton, S.T.1    Bhushan, B.2
  • 13
    • 0020208416 scopus 로고
    • "The effect of spacing on demagnetization in magnetic recording,"
    • H. N. Bertram and R. Niedermeyer, "The effect of spacing on demagnetization in magnetic recording," IEEE Trans. Magn., vol. MAG-18, pp. 1206-1208, 1982.
    • (1982) IEEE Trans. Magn., Vol. MAG , vol.18 , pp. 1206-1208
    • Bertram, H.N.1    Niedermeyer, R.2
  • 14
    • 0027701141 scopus 로고
    • "Relation between spacing losses and level differences in laminated film heads,"
    • M. Ura, H. Kobayashi, Y. Suehiro, and T. Ozeki, "Relation between spacing losses and level differences in laminated film heads," IEEE Trans. Magn.. vol. 29, pp. 3957-3959, 1993.
    • (1993) IEEE Trans. Magn.. , vol.29 , pp. 3957-3959
    • Ura, M.1    Kobayashi, H.2    Suehiro, Y.3    Ozeki, T.4
  • 15
    • 0013229408 scopus 로고
    • "Measurement of the intrinsic bond strength of brittle thin films on flexible substrates,"
    • Q. Guo, H. Osaki, L. M. Keer, and D. R. Wheeler, "Measurement of the intrinsic bond strength of brittle thin films on flexible substrates," J. Appl. Phys.. vol. 68, pp. 1649-1654, 1990.
    • (1990) J. Appl. Phys.. , vol.68 , pp. 1649-1654
    • Guo, Q.1    Osaki, H.2    Keer, L.M.3    Wheeler, D.R.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.