메뉴 건너뛰기




Volumn 80, Issue 2, 1998, Pages 340-344

Quantitative comparison of wear debris from UHMWPE that has and has not been sterilised by gamma irradiation

Author keywords

[No Author keywords available]

Indexed keywords

POLYETHYLENE; STAINLESS STEEL;

EID: 0031912659     PISSN: 0301620X     EISSN: None     Source Type: Journal    
DOI: 10.1302/0301-620X.80B2.8234     Document Type: Article
Times cited : (92)

References (25)
  • 1
    • 0025343488 scopus 로고
    • Effect of femoral head size on the wear of the polyethylene acetabular component
    • Livermore J, Duane L, Murray B. Effect of femoral head size on the wear of the polyethylene acetabular component. J Bone Joint Surg [Am] 1990;72-A:518-28.
    • (1990) J Bone Joint Surg [Am] , vol.72 A , pp. 518-528
    • Livermore, J.1    Duane, L.2    Murray, B.3
  • 2
    • 0027304584 scopus 로고
    • Bone resorption activity of particulate-stimulated macrophages
    • Giant TT, Jacobs JJ, Molnar G, et al. Bone resorption activity of particulate-stimulated macrophages. J Bone Miner Res 1993;8: 1071-9.
    • (1993) J Bone Miner Res , vol.8 , pp. 1071-1079
    • Giant, T.T.1    Jacobs, J.J.2    Molnar, G.3
  • 4
    • 0011965025 scopus 로고    scopus 로고
    • Polyethylene particles of a 'critical size' are necessary for the induction of IL-6 by macrophages in vitro
    • Green T, Fisher J, Ingham E. Polyethylene particles of a 'critical size' are necessary for the induction of IL-6 by macrophages in vitro. Trans 43rd Annual Meeting, ORS Vol. 22. 1997:733.
    • (1997) Trans 43rd Annual Meeting, ORS , vol.22 , pp. 733
    • Green, T.1    Fisher, J.2    Ingham, E.3
  • 5
    • 0027575844 scopus 로고
    • Macroscopic and microscopic wear mechanisms in ultra-high molecular weight polyethylene
    • Cooper JR, Dowson D, Fisher J. Macroscopic and microscopic wear mechanisms in ultra-high molecular weight polyethylene. Wear 1993;162:378-84.
    • (1993) Wear , vol.162 , pp. 378-384
    • Cooper, J.R.1    Dowson, D.2    Fisher, J.3
  • 6
    • 0027983089 scopus 로고
    • Composition and morphology of wear debris in failed uncemented total hip replacement
    • Shanbhag AS, Jacobs JJ, Giant TT, et al. Composition and morphology of wear debris in failed uncemented total hip replacement. J Bone Joint Surg [Br] 1994;76-B:60-7.
    • (1994) J Bone Joint Surg [Br] , vol.76 B , pp. 60-67
    • Shanbhag, A.S.1    Jacobs, J.J.2    Giant, T.T.3
  • 7
    • 0026597636 scopus 로고
    • Size of metallic and polyethylene debris particles in failed cemented total hip replacements
    • Lee J-M, Salvati EA, Betts F, et al. Size of metallic and polyethylene debris particles in failed cemented total hip replacements. J Bone Joint Surg [Br] 1992;74-B:380-4.
    • (1992) J Bone Joint Surg [Br] , vol.74 B , pp. 380-384
    • Lee, J.-M.1    Salvati, E.A.2    Betts, F.3
  • 8
    • 0019979524 scopus 로고
    • Wear of polyethylene in the total hip prosthesis
    • Rose RM, Radin EL. Wear of polyethylene in the total hip prosthesis. Clin Orthop 1982;170:107-15.
    • (1982) Clin Orthop , vol.170 , pp. 107-115
    • Rose, R.M.1    Radin, E.L.2
  • 9
    • 0028929254 scopus 로고
    • Isolation of predominantly submicron-sized UHMWPE wear particles from periprosthetic tissues
    • Campbell P, Ma S, Yeom B, et al. Isolation of predominantly submicron-sized UHMWPE wear particles from periprosthetic tissues. J Biomed Mater Res 1995;29:127-31.
    • (1995) J Biomed Mater Res , vol.29 , pp. 127-131
    • Campbell, P.1    Ma, S.2    Yeom, B.3
  • 10
    • 0028836831 scopus 로고
    • The origin of submicron polyethylene wear debris in total hip arthroplasty
    • McKellop HA, Campbell P, Park SH, et al. The origin of submicron polyethylene wear debris in total hip arthroplasty. Clin Orthop 1995; 311:3-20.
    • (1995) Clin Orthop , vol.311 , pp. 3-20
    • McKellop, H.A.1    Campbell, P.2    Park, S.H.3
  • 12
    • 0011948722 scopus 로고
    • The effects of long term shelf life aging of ultra-high molecular weight polyethylene
    • Furman B, Li S. The effects of long term shelf life aging of ultra-high molecular weight polyethylene. 21st Annual Meeting, Society for Biomaterials 1995: 114.
    • (1995) 21st Annual Meeting, Society for Biomaterials , pp. 114
    • Furman, B.1    Li, S.2
  • 13
  • 18
    • 0030629755 scopus 로고    scopus 로고
    • A study of the combined effects of shelf ageing following irradiation in air and counterface roughness on the wear of UHMWPE
    • Besong AA, Hailey JL, Ingham E, et al. A study of the combined effects of shelf ageing following irradiation in air and counterface roughness on the wear of UHMWPE. J Biomed Mat Eng 1997;7: 59-65.
    • (1997) J Biomed Mat Eng , vol.7 , pp. 59-65
    • Besong, A.A.1    Hailey, J.L.2    Ingham, E.3
  • 19
    • 0031172387 scopus 로고    scopus 로고
    • Comparison of the wear of aged and non-aged ultra-high molecular weight polyethylene sterilized by gamma irradiation and by gas plasma
    • Fisher J, Reeves EA, Isaac GH, Saum KA, Sanford WM. Comparison of the wear of aged and non-aged ultra-high molecular weight polyethylene sterilized by gamma irradiation and by gas plasma. J Mat Sci: Mat in Med 1997;8:375-8.
    • (1997) J Mat Sci: Mat in Med , vol.8 , pp. 375-378
    • Fisher, J.1    Reeves, E.A.2    Isaac, G.H.3    Saum, K.A.4    Sanford, W.M.5
  • 20
    • 0028446277 scopus 로고
    • The effect of sliding velocity on friction and wear of UHMWPE for use in total artificial joints
    • Fisher J, Dowson D, Hamdzah H, Lee HL. The effect of sliding velocity on friction and wear of UHMWPE for use in total artificial joints. Wear 1994;175:219-25.
    • (1994) Wear , vol.175 , pp. 219-225
    • Fisher, J.1    Dowson, D.2    Hamdzah, H.3    Lee, H.L.4
  • 21
    • 0001625324 scopus 로고    scopus 로고
    • Quantitative comparison of polyethylene wear debris, wear rate and head damage in retrieved hip prostheses
    • Tipper JL, Ingham E, Hailey JL, et al. Quantitative comparison of polyethylene wear debris, wear rate and head damage in retrieved hip prostheses. Trans 43rd Annual Meeting, ORS 1997; 22:355.
    • (1997) Trans 43rd Annual Meeting, ORS , vol.22 , pp. 355
    • Tipper, J.L.1    Ingham, E.2    Hailey, J.L.3
  • 22
    • 0346660525 scopus 로고    scopus 로고
    • Wear of ultrahigh molecular weight polyethylene in artificial joints: A new approach to quantification of wear debris
    • Fisher J, Barbour PSM, King M, et al. Wear of ultrahigh molecular weight polyethylene in artificial joints: a new approach to quantification of wear debris. Proc Mat 1997;2:543-4.
    • (1997) Proc Mat , vol.2 , pp. 543-544
    • Fisher, J.1    Barbour, P.S.M.2    King, M.3
  • 23
    • 0346660526 scopus 로고    scopus 로고
    • Accelerated fatigue wear of gamma-sterilized UHMWPE tibial components
    • Trieu HH, Buchanan DJ, Needham DA, et al. Accelerated fatigue wear of gamma-sterilized UHMWPE tibial components. EORS trans 1997;7:106.
    • (1997) EORS Trans , vol.7 , pp. 106
    • Trieu, H.H.1    Buchanan, D.J.2    Needham, D.A.3
  • 24
    • 0346660528 scopus 로고    scopus 로고
    • Ethylene oxide sterilisation of polyethylene cups versus gamma radiation: Different behaviour in vivo
    • Brach Del Prever E, Costa L, Gallinaro P. Ethylene oxide sterilisation of polyethylene cups versus gamma radiation: different behaviour in vivo. EFORT trans 1997:585.
    • (1997) EFORT Trans , pp. 585
    • Brach Del Prever, E.1    Costa, L.2    Gallinaro, P.3
  • 25
    • 0031039389 scopus 로고    scopus 로고
    • Degradation rate of ultra-high molecular weight polyethylene
    • Kurtz SM, Rimnac CM, Bartel DL. Degradation rate of ultra-high molecular weight polyethylene. J Orth Res 1997;15:57-61.
    • (1997) J Orth Res , vol.15 , pp. 57-61
    • Kurtz, S.M.1    Rimnac, C.M.2    Bartel, D.L.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.