Volumn 241, Issue 1-2, 1998, Pages 141-150

Development and healing of matrix microcracks in fibre reinforced glass matrix composites: Assessment by internal friction

Author keywords

Fibre reinforced glass; Internal friction; Matrix microcracks

Indexed keywords

ANNEALING; BENDING STRENGTH; CRACK INITIATION; ELASTIC MODULI; GLASS; INTERNAL FRICTION; MICROCRACKS; QUENCHING; RESONANCE; THERMAL CYCLING;

EID: 0031685861     PISSN: 09215093     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0921-5093(97)00482-6     Document Type: Article
Times cited : (26)

References (65)
  • 2
    • 0030243139 scopus 로고    scopus 로고
    • Models of high-temperature, environmentally assisted embrittlement in ceramic-matrix composites
    • A.G. Evans, F.W. Zok, R.M. McMeeking, Z.Z. Du, Models of high-temperature, environmentally assisted embrittlement in ceramic-matrix composites, J. Am. Ceram. Soc. 79 (1996) 2345-2352.
    • (1996) J. Am. Ceram. Soc. , vol.79 , pp. 2345-2352
    • Evans, A.G.1    Zok, F.W.2    McMeeking, R.M.3    Du, Z.Z.4
  • 3
    • 85162576323 scopus 로고    scopus 로고
    • U.S. Patent No. 4615987, October 7, 1986
    • K. Chyung, U.S. Patent No. 4615987, October 7, 1986.
    • Chyung, K.1
  • 4
    • 0022793146 scopus 로고
    • Tension and flexural strength of silicon carbide fiber-reinforced glass ceramics
    • K.M. Prewo, Tension and flexural strength of silicon carbide fiber-reinforced glass ceramics, J. Mater. Sci. 21 (1986) 3590-3600.
    • (1986) J. Mater. Sci. , vol.21 , pp. 3590-3600
    • Prewo, K.M.1
  • 5
    • 0024641443 scopus 로고
    • Fibre reinforced glasses
    • H. Hegeler, R. Brückner, Fibre reinforced glasses, J. Mater. Sci. 24 (1989) 1191-1194.
    • (1989) J. Mater. Sci. , vol.24 , pp. 1191-1194
    • Hegeler, H.1    Brückner, R.2
  • 7
    • 0028465291 scopus 로고
    • Effect of hot-pressing time and post-heat treatment on the microstructure and mechanical properties of SiC-fibre-reinforced glass-ceramic composites
    • H.-H. Shin, R.F. Speyer, Effect of hot-pressing time and post-heat treatment on the microstructure and mechanical properties of SiC-fibre-reinforced glass-ceramic composites, J. Mater. Sci. 29 (1994) 3630-3636.
    • (1994) J. Mater. Sci. , vol.29 , pp. 3630-3636
    • Shin, H.-H.1    Speyer, R.F.2
  • 8
    • 0027308347 scopus 로고
    • Preparation and properties of a SiC fibre-reinforced glass-ceramic matrix composite
    • B.L. Metcalfe, I.W. Donald, D.J. Bradley, Preparation and properties of a SiC fibre-reinforced glass-ceramic matrix composite, Br. Ceram. Trans. 92 (1993) 13-20.
    • (1993) Br. Ceram. Trans. , vol.92 , pp. 13-20
    • Metcalfe, B.L.1    Donald, I.W.2    Bradley, D.J.3
  • 9
    • 0029537805 scopus 로고
    • High temperature mechanical and thermal stability of silicate matrix composites
    • S. Sutherland, K.P. Plucknett, M.H. Lewis, High temperature mechanical and thermal stability of silicate matrix composites, Comp. Eng. 5 (1995) 1367-1378.
    • (1995) Comp. Eng. , vol.5 , pp. 1367-1378
    • Sutherland, S.1    Plucknett, K.P.2    Lewis, M.H.3
  • 10
    • 0000813180 scopus 로고
    • Interfacial characterization of glass matrix/nicalon SiC fibre composites: A thermodynamic approach
    • P.M. Benson, K.E. Spear, G.C. Pantano, Interfacial characterization of glass matrix/nicalon SiC fibre composites: a thermodynamic approach, Ceram. Eng. Sci. Proc. 9 (1988) 663-670.
    • (1988) Ceram. Eng. Sci. Proc. , vol.9 , pp. 663-670
    • Benson, P.M.1    Spear, K.E.2    Pantano, G.C.3
  • 11
    • 0027626885 scopus 로고
    • Acoustic microscopy of ceramic fibre composites part i: Glassmatrix composites
    • C.W. Lawrence, G.A.D. Briggs, C.B. Scruby, J.R.R. Davies, Acoustic microscopy of ceramic fibre composites part i: glassmatrix composites, J. Mater. Sci. 28 (1993) 3635-3644.
    • (1993) J. Mater. Sci. , vol.28 , pp. 3635-3644
    • Lawrence, C.W.1    Briggs, G.A.D.2    Scruby, C.B.3    Davies, J.R.R.4
  • 12
    • 84985059592 scopus 로고
    • Crack initiation in unidirectional brittle matrix composites
    • R.Y. Kim, N. Pagano, Crack initiation in unidirectional brittle matrix composites, J. Am. Ceram. Soc. 74 (1991) 1082-1090.
    • (1991) J. Am. Ceram. Soc. , vol.74 , pp. 1082-1090
    • Kim, R.Y.1    Pagano, N.2
  • 13
    • 0029271785 scopus 로고
    • Multiple cracking of unidirectional and cross-ply ceramic matrix composites
    • W.-S. Kuo, T.-W. Chou, Multiple cracking of unidirectional and cross-ply ceramic matrix composites, J. Am. Ceram. Soc. 78 (1995) 745-755.
    • (1995) J. Am. Ceram. Soc. , vol.78 , pp. 745-755
    • Kuo, W.-S.1    Chou, T.-W.2
  • 14
    • 0027544469 scopus 로고
    • Thermal shock resistance of SiC fibre-reinforced borosilicate glass and lithium aluminosilicate matrix composites
    • Y. Kagawa, N. Kurosawa, T. Kishi, Thermal shock resistance of SiC fibre-reinforced borosilicate glass and lithium aluminosilicate matrix composites, J. Mater. Sci. 28 (1993) 735-741.
    • (1993) J. Mater. Sci. , vol.28 , pp. 735-741
    • Kagawa, Y.1    Kurosawa, N.2    Kishi, T.3
  • 15
    • 0001219286 scopus 로고    scopus 로고
    • Investigation of the cyclic thermal shock behaviour of fibre reinforced glass matrix composites using a non-destructive forced resonance technique
    • in press
    • A.R. Boccaccini, D.H. Pearce, J. Janczak, W. Beier, C.B. Ponton, Investigation of the cyclic thermal shock behaviour of fibre reinforced glass matrix composites using a non-destructive forced resonance technique, Mater. Sci. Technol. 13 (1997) in press.
    • (1997) Mater. Sci. Technol. , vol.13
    • Boccaccini, A.R.1    Pearce, D.H.2    Janczak, J.3    Beier, W.4    Ponton, C.B.5
  • 16
    • 0026812782 scopus 로고
    • Thermal shock behaviour of SiC-fibre reinforced glasses
    • T. Klug, J. Reichert, R. Brückner, Thermal shock behaviour of SiC-fibre reinforced glasses, Glastech. Ber. 65 (1992) 41-49.
    • (1992) Glastech. Ber. , vol.65 , pp. 41-49
    • Klug, T.1    Reichert, J.2    Brückner, R.3
  • 17
    • 0030735868 scopus 로고    scopus 로고
    • Thermal shock behaviour of unidirectional silicon carbide fibre reinforced calcium aluminosilicate
    • M.J. Blisset, P.A. Smith, J.A. Yeomans, Thermal shock behaviour of unidirectional silicon carbide fibre reinforced calcium aluminosilicate, J. Mater. Sci. 32 (1997) 317-325.
    • (1997) J. Mater. Sci. , vol.32 , pp. 317-325
    • Blisset, M.J.1    Smith, P.A.2    Yeomans, J.A.3
  • 18
    • 0001826050 scopus 로고
    • Single and Multiple Fracture in the Properties of Fibre Composites
    • IPC Science and Technology Press, Guildford
    • J. Aveston, G.A. Cooper, A. Kelly, Single and Multiple Fracture in the Properties of Fibre Composites, in: The Properties of Fiber Composites, IPC Science and Technology Press, Guildford, 1971, pp. 15-26
    • (1971) The Properties of Fiber Composites , pp. 15-26
    • Aveston, J.1    Cooper, G.A.2    Kelly, A.3
  • 20
    • 0026745262 scopus 로고
    • Matrix crack initiation in ceramic matrix composites part ii: Models and simulation results
    • A.S.D. Wang, X.G. Huang, M.W. Barsoum, Matrix crack initiation in ceramic matrix composites part ii: models and simulation results, Comp. Sci. Technol. 44 (1992) 271-282.
    • (1992) Comp. Sci. Technol. , vol.44 , pp. 271-282
    • Wang, A.S.D.1    Huang, X.G.2    Barsoum, M.W.3
  • 21
    • 0030127398 scopus 로고    scopus 로고
    • Crack initiation in borosilicate glass-SiC fiber composites
    • R.E. Dutton, N.J. Pagano, R.Y. Kim, Crack initiation in borosilicate glass-SiC fiber composites, J. Am. Ceram. Soc. 79 (1996) 865-872.
    • (1996) J. Am. Ceram. Soc. , vol.79 , pp. 865-872
    • Dutton, R.E.1    Pagano, N.J.2    Kim, R.Y.3
  • 22
    • 0004864682 scopus 로고
    • Progressive microcracking in unidirectional brittle matrix composites
    • N.J. Pagano, R.Y. Kim, Progressive microcracking in unidirectional brittle matrix composites, Mech. Comp. Mater. Struct. 1 (1994) 3-29.
    • (1994) Mech. Comp. Mater. Struct. , vol.1 , pp. 3-29
    • Pagano, N.J.1    Kim, R.Y.2
  • 23
    • 0030084087 scopus 로고    scopus 로고
    • Effect of loading rate on the monotonic tensile behavior of a continuous-fiber-reinforced glass-ceramic matrix composite
    • B.E. Sorensen, J.W. Holmes, Effect of loading rate on the monotonic tensile behavior of a continuous-fiber-reinforced glass-ceramic matrix composite, J. Am. Ceram. Soc. 79 (1996) 313-320.
    • (1996) J. Am. Ceram. Soc. , vol.79 , pp. 313-320
    • Sorensen, B.E.1    Holmes, J.W.2
  • 24
    • 0030243354 scopus 로고    scopus 로고
    • Fracture process of silicon carbide fiber-reinforced glasses
    • H. Tsuda, J. Takahashi, K. Kemmochi, R. Hayashi, Fracture process of silicon carbide fiber-reinforced glasses, J. Am. Ceram. Soc. 79 (1996) 2293-2299.
    • (1996) J. Am. Ceram. Soc. , vol.79 , pp. 2293-2299
    • Tsuda, H.1    Takahashi, J.2    Kemmochi, K.3    Hayashi, R.4
  • 25
    • 0026707105 scopus 로고
    • Matrix crack initiation in ceramic matrix composites, part I: Experiments and test results
    • M.W. Barsoum, P. Kangutkar, A.S.D. Wang, Matrix crack initiation in ceramic matrix composites, part I: experiments and test results, Comp. Sci. Technol. 44 (1992) 257-269.
    • (1992) Comp. Sci. Technol. , vol.44 , pp. 257-269
    • Barsoum, M.W.1    Kangutkar, P.2    Wang, A.S.D.3
  • 26
    • 84985047108 scopus 로고
    • Damage and failure in unidirectional ceramic-matrix composites
    • D.S. Beyerle, S.M. Spearing, F.W. Zok, A.G. Evans, Damage and failure in unidirectional ceramic-matrix composites, J. Am. Ceram. Soc. 75 (1992) 2719-2725.
    • (1992) J. Am. Ceram. Soc. , vol.75 , pp. 2719-2725
    • Beyerle, D.S.1    Spearing, S.M.2    Zok, F.W.3    Evans, A.G.4
  • 27
    • 0030193249 scopus 로고    scopus 로고
    • Characterization of failure behaviour of brittle matrix composites at room and elevated temperatures
    • S.J. Zhang, F. Delale, B.M. Liaw, Characterization of failure behaviour of brittle matrix composites at room and elevated temperatures, Mater. Manuf. Process. 11 (1996) 605-633.
    • (1996) Mater. Manuf. Process. , vol.11 , pp. 605-633
    • Zhang, S.J.1    Delale, F.2    Liaw, B.M.3
  • 30
    • 0021652839 scopus 로고
    • Evaluation of Ceramic Fracture Caused by Thermal Shock
    • S.R. Vallurin, D.M.R. Taplin, et al. (Eds.), Pergamon Press, Oxford
    • G.A. Gogotsi, A.N. Negovski, Evaluation of Ceramic Fracture Caused by Thermal Shock, pp. 2701-2709, in S.R. Vallurin, D.M.R. Taplin, et al. (Eds.), Advances in Fracture Research, Vol. 4, Pergamon Press, Oxford, 1984.
    • (1984) Advances in Fracture Research , vol.4 , pp. 2701-2709
    • Gogotsi, G.A.1    Negovski, A.N.2
  • 32
    • 0021411177 scopus 로고
    • Young's modulus and internal friction in alumina subjected to thermal shock
    • K. Matsushita, S. Kuratani, T. Okamoto, M. Shimada, Young's modulus and internal friction in alumina subjected to thermal shock, J. Mater. Sci. Lett. 3 (1984) 345-348.
    • (1984) J. Mater. Sci. Lett. , vol.3 , pp. 345-348
    • Matsushita, K.1    Kuratani, S.2    Okamoto, T.3    Shimada, M.4
  • 33
    • 0012092447 scopus 로고
    • Thermal fatigue in polycrystalline alumina
    • W.J. Lee, E.D. Case, Thermal fatigue in polycrystalline alumina, J. Mater. Sci. 25 (1990) 5043-5054.
    • (1990) J. Mater. Sci. , vol.25 , pp. 5043-5054
    • Lee, W.J.1    Case, E.D.2
  • 34
    • 0024766579 scopus 로고
    • Cyclic thermal shock in SiC-whisker-reinforced alumina composite
    • W.J. Lee, E.D. Case, Cyclic thermal shock in SiC-whisker-reinforced alumina composite, Mater. Sci. Eng. A119 (1989) 113-126.
    • (1989) Mater. Sci. Eng. , vol.A119 , pp. 113-126
    • Lee, W.J.1    Case, E.D.2
  • 35
    • 0012030085 scopus 로고
    • Thermal fatigue in SiC fiber reinforced aluminosilicate glass-ceramic composite
    • R.B. Bhagat, A.H. Clauer, P. Kumar, A.M. Ritter, The Minerals, Metals and Materials Society
    • Y. Kim, W.J. Lee, E.D. Case, Thermal fatigue in SiC fiber reinforced aluminosilicate glass-ceramic composite, in: R.B. Bhagat, A.H. Clauer, P. Kumar, A.M. Ritter, Metal and Ceramic Matrix composites: processing, modeling and mechanical behaviour, The Minerals, Metals and Materials Society, 1990, pp. 479-486
    • (1990) Metal and Ceramic Matrix Composites: Processing, Modeling and Mechanical Behaviour , pp. 479-486
    • Kim, Y.1    Lee, W.J.2    Case, E.D.3
  • 36
    • 0027659030 scopus 로고
    • Nondestructive detection of fatigue cracks in PM 304 stainless steel by internal friction and elasticity
    • S.M. McGuire, M.E. Fine, O. Buck, J.D. Achenbach, Nondestructive detection of fatigue cracks in PM 304 stainless steel by internal friction and elasticity, J. Mater. Res. 8 (1993) 2216-2223.
    • (1993) J. Mater. Res. , vol.8 , pp. 2216-2223
    • McGuire, S.M.1    Fine, M.E.2    Buck, O.3    Achenbach, J.D.4
  • 37
    • 0029326150 scopus 로고
    • Internal friction in AlCu-A12O3 metal-matrix composites
    • L. Parrini, R. Schaller, Internal friction in AlCu-A12O3 metal-matrix composites, Metall. Mater. Trans. 26A (1995) 1457-1460.
    • (1995) Metall. Mater. Trans. , vol.26 A , pp. 1457-1460
    • Parrini, L.1    Schaller, R.2
  • 41
    • 0029409322 scopus 로고
    • Measurement of Young's Modulus and damping as a function of temperature in a borosilicate glass-matrix composite with continuous ceramic fibres
    • A. Wolfenden, H.M. Thomas, V. Thomas, K.K. Chawla, Measurement of Young's Modulus and damping as a function of temperature in a borosilicate glass-matrix composite with continuous ceramic fibres, J. Mater. Sci. Lett. 14 (1995) 1555-1557.
    • (1995) J. Mater. Sci. Lett. , vol.14 , pp. 1555-1557
    • Wolfenden, A.1    Thomas, H.M.2    Thomas, V.3    Chawla, K.K.4
  • 42
    • 0028548888 scopus 로고
    • Temperature dependence of dynamic Young's Modulus and mechanical damping in a nextel fiber-reinforced glass composite
    • A. Wolfenden, J.E. Gill, K.K. Chawla, R.U. Vaidya, R. Venkatesh, Temperature dependence of dynamic Young's Modulus and mechanical damping in a nextel fiber-reinforced glass composite, J. Test. Eval. 22 (1994) 571-573.
    • (1994) J. Test. Eval. , vol.22 , pp. 571-573
    • Wolfenden, A.1    Gill, J.E.2    Chawla, K.K.3    Vaidya, R.U.4    Venkatesh, R.5
  • 43
    • 0024036218 scopus 로고
    • Microstructure, chemistry, elastic properties and internal friction of silceram glass-ceramics
    • S. Carter, C.B. Ponton, R.D. Rawlings, P.S. Rogers, Microstructure, chemistry, elastic properties and internal friction of silceram glass-ceramics, J. Mater. Sci. 23 (1988) 2622-2630.
    • (1988) J. Mater. Sci. , vol.23 , pp. 2622-2630
    • Carter, S.1    Ponton, C.B.2    Rawlings, R.D.3    Rogers, P.S.4
  • 44
    • 0003088381 scopus 로고
    • The effects of thermal fatigue on a SiC fibre/aluminosilicate glass composite
    • L.P. Zawada, R.C. Wetherhold, The effects of thermal fatigue on a SiC fibre/aluminosilicate glass composite, J. Mater. Sci. 26 (1991) 648-654.
    • (1991) J. Mater. Sci. , vol.26 , pp. 648-654
    • Zawada, L.P.1    Wetherhold, R.C.2
  • 45
    • 0347591872 scopus 로고
    • (ex PCS)/MAS Composites with a BN Interphase: Microstructure, Mechanical Properties and Oxidation Resistance
    • R. Naslain, J. Lamon, D. Doumengts (Eds.), Woodhead Publishing, Cambridge, UK
    • N. Ricca, A. Guette, G. Camus and J.M. JouinSiC (ex PCS)/MAS Composites with a BN Interphase: Microstructure, Mechanical Properties and Oxidation Resistance, in: R. Naslain, J. Lamon, D. Doumengts (Eds.), High Temperature Ceramic Matrix Composites, Vol. 1, Woodhead Publishing, Cambridge, UK, 1993, pp. 455-462 .
    • (1993) High Temperature Ceramic Matrix Composites , vol.1 , pp. 455-462
    • Ricca, N.1    Guette, A.2    Camus, G.3    JouinSiC, J.M.4
  • 46
    • 0028946184 scopus 로고
    • Nanostructure of interlayers in diffenrent nicalon fibre/glass matrix composites and their effect on mechanical properties
    • A. Hähnel, E. Pippel, J. Woltersdorf, Nanostructure of interlayers in diffenrent nicalon fibre/glass matrix composites and their effect on mechanical properties, J. Microsc. 177 (1995) 264-271.
    • (1995) J. Microsc. , vol.177 , pp. 264-271
    • Hähnel, A.1    Pippel, E.2    Woltersdorf, J.3
  • 47
    • 0028479523 scopus 로고
    • High temperature behavior of salt coated nicalon fiber reinforced calcium aluminosilicate composite
    • S.-W. Wang, R.W. Kowalik, R. Sands, High temperature behavior of salt coated nicalon fiber reinforced calcium aluminosilicate composite, Ceram. Eng. Sci. Proc., 1994, 465-474.
    • (1994) Ceram. Eng. Sci. Proc. , pp. 465-474
    • Wang, S.-W.1    Kowalik, R.W.2    Sands, R.3
  • 48
    • 0000020485 scopus 로고
    • A new method for the determination of the modulus of elasticity and damping
    • F. Förster, A new method for the determination of the modulus of elasticity and damping, Z. Metallk. 29 (1937) 109-115.
    • (1937) Z. Metallk. , vol.29 , pp. 109-115
    • Förster, F.1
  • 52
    • 0030193129 scopus 로고    scopus 로고
    • Thermal shock behaviour of two-dimensional woven fiber-reinforced ceramic composites
    • H. Wang, R.N. Singh, R.A. Lowden, Thermal shock behaviour of two-dimensional woven fiber-reinforced ceramic composites, J. Am. Ceram. Soc. 79 (1996) 1783-1792.
    • (1996) J. Am. Ceram. Soc. , vol.79 , pp. 1783-1792
    • Wang, H.1    Singh, R.N.2    Lowden, R.A.3
  • 53
    • 0029379408 scopus 로고
    • Damage development and moduli reduction in a unidirectional SiC-MAS.L composite tested under uniaxial tensile loading
    • M. Drissi-Habti, Damage development and moduli reduction in a unidirectional SiC-MAS.L composite tested under uniaxial tensile loading, Scr. Metall. Mater. 33 (1995) 967-973.
    • (1995) Scr. Metall. Mater. , vol.33 , pp. 967-973
    • Drissi-Habti, M.1
  • 54
    • 0030259358 scopus 로고    scopus 로고
    • Influence of fiber volume fraction on mechanical behaviour of CVD SiC fiber/SrA12Si2O8 glass-ceramic matrix composites
    • N.P. Bansal, Influence of fiber volume fraction on mechanical behaviour of CVD SiC fiber/SrA12Si2O8 glass-ceramic matrix composites, J. Adv. Mater., 1996, 48-58.
    • (1996) J. Adv. Mater. , pp. 48-58
    • Bansal, N.P.1
  • 55
    • 0030403959 scopus 로고    scopus 로고
    • CVD SiC fiber-reinforced barium aluminosilicate glass-ceramic matrix Composites
    • N.P. Bansal, CVD SiC fiber-reinforced barium aluminosilicate glass-ceramic matrix Composites, Mater. Sci. Eng. A220 (1996) 129-139.
    • (1996) Mater. Sci. Eng. , vol.A220 , pp. 129-139
    • Bansal, N.P.1
  • 56
    • 0041444079 scopus 로고
    • Modeling of the Thermomechanical Behaviour of Glass Matrix Composites
    • R.B. Bhagat, A.H. Clauer, P. Kumar, A.M. Ritter (Eds.), The Minerals, Metals and Materials Society
    • W.-S. Kuo, T.-W. Chou, Modeling of the Thermomechanical Behaviour of Glass Matrix Composites, in: R.B. Bhagat, A.H. Clauer, P. Kumar, A.M. Ritter (Eds.), Metal and Ceramic Matrix Composites: Processing, Moduling and Mechanical Behaviour, The Minerals, Metals and Materials Society, 1990.
    • (1990) Metal and Ceramic Matrix Composites: Processing, Moduling and Mechanical Behaviour
    • Kuo, W.-S.1    Chou, T.-W.2
  • 57
    • 0028392558 scopus 로고
    • The Relation of Dynamic Elastic Moduli, Mechanical Damping and Mass Density to the Microstructure of Some Glass Matrix Composites
    • A. Wolfenden, J.E. Gill, V. Thomas, A.J. Giacomin, L.S. Cook, K.K. Chawla, R. Venkatesh, R.U. Vaidya, The Relation of Dynamic Elastic Moduli, Mechanical Damping and Mass Density to the Microstructure of Some Glass Matrix Composites, J. Mater. Sci. 29 (1994) 1670-1675.
    • (1994) J. Mater. Sci. , vol.29 , pp. 1670-1675
    • Wolfenden, A.1    Gill, J.E.2    Thomas, V.3    Giacomin, A.J.4    Cook, L.S.5    Chawla, K.K.6    Venkatesh, R.7    Vaidya, R.U.8
  • 58
    • 0003683811 scopus 로고
    • Schott Glaswerke, Mainz, Germany
    • Technische Gläser, Product-Information, Schott Glaswerke, Mainz, Germany, 1990.
    • (1990) Product-Information
  • 59
    • 0023132556 scopus 로고
    • Kinetics of crack blunting of glasses
    • K. Hirao, M. Tomozawa, Kinetics of crack blunting of glasses, J. Am. Ceram. Soc. 70 (1987) 43-48.
    • (1987) J. Am. Ceram. Soc. , vol.70 , pp. 43-48
    • Hirao, K.1    Tomozawa, M.2
  • 61
    • 0014758309 scopus 로고
    • Capillarity induced smoothing of glass surfaces by viscous flow
    • D.C. Cassidy, N.A. Gjostein, Capillarity induced smoothing of glass surfaces by viscous flow, J. Am. Ceram. Soc. 53 (1970) 161-168.
    • (1970) J. Am. Ceram. Soc. , vol.53 , pp. 161-168
    • Cassidy, D.C.1    Gjostein, N.A.2
  • 62
    • 0024013578 scopus 로고
    • Crack healing and bending strength of aluminum titanate ceramics at high temperature
    • Y. Ohya, Z. Nakagawa, K. Hamano, Crack healing and bending strength of aluminum titanate ceramics at high temperature, J. Am. Ceram. Soc. 71 (1988) C232-C233.
    • (1988) J. Am. Ceram. Soc. , vol.71
    • Ohya, Y.1    Nakagawa, Z.2    Hamano, K.3
  • 63
    • 0030288499 scopus 로고    scopus 로고
    • Crack healing in silicon nitride and alumina ceramics
    • M. Mitomo, T. Nishimura, M. Tsutsumi, Crack healing in silicon nitride and alumina ceramics, J. Mater. Sci. Lett. 15 (1996) 1976-1978.
    • (1996) J. Mater. Sci. Lett. , vol.15 , pp. 1976-1978
    • Mitomo, M.1    Nishimura, T.2    Tsutsumi, M.3
  • 64
    • 0026003944 scopus 로고
    • Heat treatments as a method of protection for a ceramic fiber-glass composite
    • R.C. Wetherhold, L.P. Zawada, Heat treatments as a method of protection for a ceramic fiber-glass composite, J. Am. Ceram. Soc. 74 (1991) 1997-2000.
    • (1991) J. Am. Ceram. Soc. , vol.74 , pp. 1997-2000
    • Wetherhold, R.C.1    Zawada, L.P.2
  • 65
    • 0023963893 scopus 로고
    • Ceramic coatings for carbon-carbon composites
    • J.R. Strife, J.E. Sheenan, Ceramic coatings for carbon-carbon composites, Ceram. Bull. 67 (1988) 369-374.
    • (1988) Ceram. Bull. , vol.67 , pp. 369-374
    • Strife, J.R.1    Sheenan, J.E.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.