Volumn 18, Issue 1, 1998, Pages 51-57

Mechanical behavior and microstructure of SiC and SiC/TiB2 ceramics

Author keywords

[No Author keywords available]

Indexed keywords

ALUMINA; COMPOSITION EFFECTS; CRACK INITIATION; CRYSTAL MICROSTRUCTURE; DOPING (ADDITIVES); INTERFACES (MATERIALS); SILICON CARBIDE; SINTERING; STRENGTH OF MATERIALS; TITANIUM COMPOUNDS; TOUGHNESS; VOLUME FRACTION;

EID: 0031646694     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/s0955-2219(97)00106-4     Document Type: Article
Times cited : (22)

References (23)
  • 1
    • 0000150475 scopus 로고
    • Super-tough silicon nitride with R-curve behavior
    • Li, C.-W. and Yamanis, J., Super-tough silicon nitride with R-curve behavior. Ceram. Eng. Sci. Proc., 1989, 10, 632-645.
    • (1989) Ceram. Eng. Sci. Proc. , vol.10 , pp. 632-645
    • Li, C.-W.1    Yamanis, J.2
  • 2
    • 84985084859 scopus 로고
    • R-curve behavior and strength of in-situ reinforced silicon nitride with different microstructures
    • Li, C.-W., Lee, D.-J. and Lui, S.-C., R-curve behavior and strength of in-situ reinforced silicon nitride with different microstructures. J. Am. Ceram. Soc., 1992, 75, 1777-1785.
    • (1992) J. Am. Ceram. Soc. , vol.75 , pp. 1777-1785
    • Li, C.-W.1    Lee, D.-J.2    Lui, S.-C.3
  • 5
    • 0028382729 scopus 로고
    • In situ-toughened silicon carbide
    • Padture, N. P., In situ-toughened silicon carbide. J. Am. Ceram. Soc., 1994, 77, 519-523.
    • (1994) J. Am. Ceram. Soc. , vol.77 , pp. 519-523
    • Padture, N.P.1
  • 6
    • 0021470145 scopus 로고
    • Improvements in mechanical properties in SiC by the addition of TiC particles
    • Wei, G. C. and Becher, P. F., Improvements in mechanical properties in SiC by the addition of TiC particles. J. Am. Ceram. Soc., 1984, 67, 571-574.
    • (1984) J. Am. Ceram. Soc. , vol.67 , pp. 571-574
    • Wei, G.C.1    Becher, P.F.2
  • 7
    • 0022663825 scopus 로고
    • Microstructural development and mechanical properties of SiC and of SiC-TiC composites
    • Janney, M. A., Microstructural development and mechanical properties of SiC and of SiC-TiC composites. Am. Ceram. Soc. Bull., 1986, 65, 357-362.
    • (1986) Am. Ceram. Soc. Bull. , vol.65 , pp. 357-362
    • Janney, M.A.1
  • 14
    • 0028529919 scopus 로고
    • Toughness properties of a silicon carbide with an in situ induced heterogeneous grain structure
    • Padture, N. P. and Lawn, B. R., Toughness properties of a silicon carbide with an in situ induced heterogeneous grain structure. J. Am. Ceram. Soc., 1994, 77, 2518-2522.
    • (1994) J. Am. Ceram. Soc. , vol.77 , pp. 2518-2522
    • Padture, N.P.1    Lawn, B.R.2
  • 15
    • 0022866970 scopus 로고
    • Crack stability and toughness characteristics in brittle materials
    • Mai, Y.-W. and Lawn, B. R., Crack stability and toughness characteristics in brittle materials. Ann. Rev. Mater. Sci., 1986, 16, 415-439.
    • (1986) Ann. Rev. Mater. Sci. , vol.16 , pp. 415-439
    • Mai, Y.-W.1    Lawn, B.R.2
  • 17
    • 0018503878 scopus 로고
    • Residual stress effect in sharp-contact cracking: 1. Indentation fracture mechanics
    • Marshall, D. B. and Lawn, B. R., Residual stress effect in sharp-contact cracking: 1. Indentation fracture mechanics. J. Mater. Sci., 1979, 14, 2001-2012.
    • (1979) J. Mater. Sci. , vol.14 , pp. 2001-2012
    • Marshall, D.B.1    Lawn, B.R.2
  • 18
    • 0019058952 scopus 로고
    • Elastic/ plastic indentation damage in ceramics: The median/radial crack system
    • Lawn, B. R., Evans, A. G. and Marshall, D. B., Elastic/ plastic indentation damage in ceramics: the median/radial crack system. J. Am. Ceram. Soc., 1980, 63, 574-581.
    • (1980) J. Am. Ceram. Soc. , vol.63 , pp. 574-581
    • Lawn, B.R.1    Evans, A.G.2    Marshall, D.B.3
  • 19
    • 0000327659 scopus 로고
    • Objective evaluation of short-crack toughness curves using indentation flaws: Case study on alumina-based ceramics
    • Braun, L. M., Bennison, S. J. and Lawn, B. R., Objective evaluation of short-crack toughness curves using indentation flaws: case study on alumina-based ceramics. J. Am. Ceram. Soc., 1992, 7, 3049-3057.
    • (1992) J. Am. Ceram. Soc. , vol.7 , pp. 3049-3057
    • Braun, L.M.1    Bennison, S.J.2    Lawn, B.R.3
  • 20
    • 0023327964 scopus 로고
    • Crack-interface grain bridging as a fracture resistance mechanism in ceramics: 1. Experimental study on alumina
    • Swanson, P. L., Fairbanks, C. J., Lawn, B. R., Mai, Y.-W. and Hockey, B. J., Crack-interface grain bridging as a fracture resistance mechanism in ceramics: 1. experimental study on alumina. J. Am. Ceram. Soc., 1987, 70, 279-289.
    • (1987) J. Am. Ceram. Soc. , vol.70 , pp. 279-289
    • Swanson, P.L.1    Fairbanks, C.J.2    Lawn, B.R.3    Mai, Y.-W.4    Hockey, B.J.5
  • 21
    • 0027663584 scopus 로고
    • Model for toughness-curves in two-phase ceramics: I, basic fracture mechanics
    • Lawn, B. R., Padture, N. P., Braun, L. M. and Bennison, S. J., Model for toughness-curves in two-phase ceramics: I, basic fracture mechanics. J. Am. Ceram. Soc., 1993, 76, 2235-2240.
    • (1993) J. Am. Ceram. Soc. , vol.76 , pp. 2235-2240
    • Lawn, B.R.1    Padture, N.P.2    Braun, L.M.3    Bennison, S.J.4
  • 22
    • 0027658716 scopus 로고
    • Model for toughness-curves in two-phase ceramics: II, microstructural variables
    • Padture, N. P., Runyan, J. L., Bennison, S. J., Braun, L. M. and Lawn, B. R., Model for toughness-curves in two-phase ceramics: II, microstructural variables. J. Am. Ceram. Soc., 1993, 76, 2241-2247.
    • (1993) J. Am. Ceram. Soc. , vol.76 , pp. 2241-2247
    • Padture, N.P.1    Runyan, J.L.2    Bennison, S.J.3    Braun, L.M.4    Lawn, B.R.5
  • 23
    • 84959610090 scopus 로고
    • Crack resistance by interfacial bridging: Its role in determining strength characteristics
    • Cook, R. F., Fairbanks, C. J., Lawn, B. R. and Mai, Y.-W., Crack resistance by interfacial bridging: its role in determining strength characteristics. J. Mater. Res., 1987, 2, 345-356.
    • (1987) J. Mater. Res. , vol.2 , pp. 345-356
    • Cook, R.F.1    Fairbanks, C.J.2    Lawn, B.R.3    Mai, Y.-W.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.