메뉴 건너뛰기




Volumn 11, Issue 1, 1998, Pages 49-54

Effect of Water Sorption on the Resistance to Plastic Deformation of a Denture Base Material Relined with Four Different Denture Reline Materials

Author keywords

[No Author keywords available]

Indexed keywords

BIOMEDICAL AND DENTAL MATERIALS; WATER;

EID: 0031641571     PISSN: 08932174     EISSN: None     Source Type: Journal    
DOI: None     Document Type: Article
Times cited : (75)

References (11)
  • 1
    • 0031266225 scopus 로고    scopus 로고
    • Flexural strength at the proportional limit of a denture base material
    • Takahashi Y, Kawaguchi M, Chai J. Flexural strength at the proportional limit of a denture base material. Int J Prosthodont 1997;10:508-512.
    • (1997) Int J Prosthodont , vol.10 , pp. 508-512
    • Takahashi, Y.1    Kawaguchi, M.2    Chai, J.3
  • 2
    • 0029181092 scopus 로고
    • Properties of high cross-linked autopolymerizing reline acrylic resin
    • Arima T, Murata H, Hamada I. Properties of high cross-linked autopolymerizing reline acrylic resin. J Prosthet Dent 1995; 73:55-59.
    • (1995) J Prosthet Dent , vol.73 , pp. 55-59
    • Arima, T.1    Murata, H.2    Hamada, I.3
  • 3
    • 0024625897 scopus 로고
    • Comparison of two light-cured reline systems
    • Latta M, Tateosian LH. Comparison of two light-cured reline systems. J Clin Dent 1989;1:116-120.
    • (1989) J Clin Dent , vol.1 , pp. 116-120
    • Latta, M.1    Tateosian, L.H.2
  • 4
    • 0026217988 scopus 로고
    • In vitro properties of light-polymerized reline materials
    • Smith FT, Powers JM. In vitro properties of light-polymerized reline materials. Int J Prosthodont 1991;4:445-448.
    • (1991) Int J Prosthodont , vol.4 , pp. 445-448
    • Smith, F.T.1    Powers, J.M.2
  • 6
    • 0030622229 scopus 로고    scopus 로고
    • Influence of thickness on the linear dimensional change, warpage, and water uptake of a denture base rosin
    • Sadamori S, Ishii T, Hamada T. Influence of thickness on the linear dimensional change, warpage, and water uptake of a denture base rosin. Int J Prosthodont 1997;10:35-43.
    • (1997) Int J Prosthodont , vol.10 , pp. 35-43
    • Sadamori, S.1    Ishii, T.2    Hamada, T.3
  • 7
    • 1842745920 scopus 로고    scopus 로고
    • International Standard. ISO 1567 for Denture Base Polymers. Genève: International Organization for the Testing of Materials. 1988(E)
    • International Standard. ISO 1567 for Denture Base Polymers. Genève: International Organization for the Testing of Materials. 1988(E).
  • 8
    • 1842796420 scopus 로고    scopus 로고
    • American National Standard/American Dental Association. Specification No. 12 for Denture Base Polymers. Chicago: Council on Dental Materials and Devices, 1975
    • American National Standard/American Dental Association. Specification No. 12 for Denture Base Polymers. Chicago: Council on Dental Materials and Devices, 1975.
  • 9
    • 0024063460 scopus 로고
    • Some physical and mechanical properties of a visible light-activated material
    • Al-Mulla MAS, Huggett R, Brooks SC, Murphy WM. Some physical and mechanical properties of a visible light-activated material, Dent Mater 1988;4:197-200.
    • (1988) Dent Mater , vol.4 , pp. 197-200
    • Al-Mulla, M.A.S.1    Huggett, R.2    Brooks, S.C.3    Murphy, W.M.4
  • 11
    • 0030078022 scopus 로고    scopus 로고
    • Effect of light-exposure duration on the amount of leachable monomers from light-activated reline material
    • Kawaguchi M, Takahashi Y, Fukushima T, Habu T. Effect of light-exposure duration on the amount of leachable monomers from light-activated reline material. J Prosthet Dent 1996; 75:183-187.
    • (1996) J Prosthet Dent , vol.75 , pp. 183-187
    • Kawaguchi, M.1    Takahashi, Y.2    Fukushima, T.3    Habu, T.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.