|
Volumn 251-254, Issue PART 2, 1997, Pages 527-534
|
Corrosion of high alloy steels and Fe-Cr-alloys beneath deposits from waste incinerator plants
|
Author keywords
Acidic Fluxing; Active Oxidation; Basic Fluxing; Deposits; Heavy Metal Compounds; Hot Corrosion; Sulfate Melts; Waste Incineration Atmospheres
|
Indexed keywords
DEPOSITS;
HEAVY METAL COMPOUNDS;
HYDROCHLORIC ACID;
INDUSTRIAL PLANTS;
INTERFACES (MATERIALS);
IRON ALLOYS;
OXIDATION;
REFUSE INCINERATORS;
STEEL;
WASTE INCINERATION;
ACIDIC FLUXING;
BASIC FLUXING;
HIGH ALLOY STEEL;
HOT CORROSION;
IRON CHROMIUM ALLOY;
SULFATE CHLORIDE EUTECTIC;
SULFATE MELT;
CORROSION;
|
EID: 0031373901
PISSN: 02555476
EISSN: 16629752
Source Type: Book Series
DOI: 10.4028/www.scientific.net/msf.251-254.527 Document Type: Article |
Times cited : (29)
|
References (12)
|