Volumn 58, Issue 4, 1997, Pages 311-325

Fracture of hot formed ledeburitic chromium steels

(3)  Berns, H a   Broeckmann, C a   Weichert, D a  

a NONE

Author keywords

Anisotropy; Finite element method; Fracture toughness; J integral; Ledeburitic chromium steel; Two phase material

Indexed keywords

ANISOTROPY; COMPUTER SIMULATION; CRACK PROPAGATION; DUCTILITY; ELASTOPLASTICITY; FINITE ELEMENT METHOD; FRACTURE TOUGHNESS; HARDNESS; INTEGRAL EQUATIONS; MATHEMATICAL MODELS; METALLIC MATRIX COMPOSITES; STRUCTURAL LOADS;

EID: 0031279872     PISSN: 00137944     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0013-7944(97)00118-5     Document Type: Article
Times cited : (29)

References (21)
  • 1
    • 0042715718 scopus 로고
    • Einfluß der Carbidorientierung auf Bruchzähigkeit und abrasiven Verschleißwiderstand ledeburitischer Kaltarbeitsstähle
    • Berns, H., Fischer, A. and Hänsch, W., Einfluß der Carbidorientierung auf Bruchzähigkeit und abrasiven Verschleißwiderstand ledeburitischer Kaltarbeitsstähle. HTM, 1990, 45(4), 217-222.
    • (1990) HTM , vol.45 , Issue.4 , pp. 217-222
    • Berns, H.1    Fischer, A.2    Hänsch, W.3
  • 3
    • 0042214569 scopus 로고
    • ASTM e 399-74, Standard test method E 399-74 for plane - Strain toughness of metallic materials
    • ASTM, Philadelphia, PA
    • ASTM E 399-74, Standard test method E 399-74 for plane - strain toughness of metallic materials. In 1976 Annual Book of ASTM Standards. ASTM, Philadelphia, PA, 1976.
    • (1976) 1976 Annual Book of ASTM Standards
  • 4
    • 0016359543 scopus 로고
    • Restaustenit in ledeburitischen Chromstählen und seine Umwandlung durch Kaltumformen, Tiefkühlen und Anlassen
    • Berns, H., Restaustenit in ledeburitischen Chromstählen und seine Umwandlung durch Kaltumformen, Tiefkühlen und Anlassen. HTM, 1974, 29(4), 236-247.
    • (1974) HTM , vol.29 , Issue.4 , pp. 236-247
    • Berns, H.1
  • 10
  • 11
    • 0043216885 scopus 로고
    • An equivalent domain integral for analysis of two-dimensional mixed mode problems
    • 3-5 April, paper AIAA
    • Raju, I. S. and Shivakumar, K. N., An equivalent domain integral for analysis of two-dimensional mixed mode problems. In Proceedings of the 30th AIAA Meeting, 3-5 April, 1989, paper AIAA, pp. 89-1299.
    • (1989) Proceedings of the 30th AIAA Meeting , pp. 89-1299
    • Raju, I.S.1    Shivakumar, K.N.2
  • 12
    • 0019245249 scopus 로고
    • J integral of a mixed mode crack and its application
    • Ishikawa, H., Kitagawa, H. and Okamura, H., J integral of a mixed mode crack and its application. ICM3, 1979, 3, 447-455.
    • (1979) ICM3 , vol.3 , pp. 447-455
    • Ishikawa, H.1    Kitagawa, H.2    Okamura, H.3
  • 13
    • 0041714161 scopus 로고
    • Computational simulation of non-coplanar crack growth and experimental verification for a specimen under combined bending and shear loading
    • Varna, Bulgarien
    • Theilig, H., Wiebe, P. and Buchholz, F. G., Computational simulation of non-coplanar crack growth and experimental verification for a specimen under combined bending and shear loading. In Proceedings of the 9th European Conference on Fracture (ECF9). Varna, Bulgarien, 1992, pp. 789-794.
    • (1992) Proceedings of the 9th European Conference on Fracture (ECF9) , pp. 789-794
    • Theilig, H.1    Wiebe, P.2    Buchholz, F.G.3
  • 15
    • 0017926530 scopus 로고
    • Fracture toughness of powder metallurgy and conventionally produced high-speed steels
    • Olsson, L. R. and Fischmeister, H. F., Fracture toughness of powder metallurgy and conventionally produced high-speed steels. Powder Metallurgy, 1978, 1, 13-28.
    • (1978) Powder Metallurgy , vol.1 , pp. 13-28
    • Olsson, L.R.1    Fischmeister, H.F.2
  • 16
    • 0017725838 scopus 로고
    • The failure of large second phase particles in a cracking aluminium alloy
    • Kasteele van de, J. C. W. and Broek, D., The failure of large second phase particles in a cracking aluminium alloy. Engineering Fracture Mechanics, 1977, 9, 625-635.
    • (1977) Engineering Fracture Mechanics , vol.9 , pp. 625-635
    • Kasteele Van De, J.C.W.1    Broek, D.2
  • 17
  • 18
    • 0023593736 scopus 로고
    • The influence of non-metallic inclusion on the fracture behaviors of 25Mn-5Cr-1Ni austenitic steel
    • Maekawa, I., Tanabe, Y. and Lee, J. H., The influence of non-metallic inclusion on the fracture behaviors of 25Mn-5Cr-1Ni austenitic steel. Engineering Fracture Mechanics, 1987, 28, 577-587.
    • (1987) Engineering Fracture Mechanics , vol.28 , pp. 577-587
    • Maekawa, I.1    Tanabe, Y.2    Lee, J.H.3
  • 20
    • 0030452435 scopus 로고    scopus 로고
    • A numerical study on the crack growth behaviours of a low and a high-strength steel
    • Shan, G., Kolednik, O. and Fischer, F. D., A numerical study on the crack growth behaviours of a low and a high-strength steel. International Journal of Fracture, 1996, 78, 335-346.
    • (1996) International Journal of Fracture , vol.78 , pp. 335-346
    • Shan, G.1    Kolednik, O.2    Fischer, F.D.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.