Volumn 212, Issue 1, 1997, Pages 50-58

Nucleation and early growth of tribologically transformed structure (TTS) induced by fretting

Author keywords

Fretting; Nucleation parameters; Tribologically transformed structures; White layer

Indexed keywords

FRETTING CORROSION; MECHANICAL TESTING; METALLOGRAPHY; NUCLEATION; WEAR OF MATERIALS; FATIGUE OF MATERIALS; HARDNESS; MATERIALS TESTING; PHASE TRANSITIONS;

EID: 0031260764     PISSN: 00431648     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0043-1648(97)00141-5     Document Type: Article
Times cited : (81)

References (25)
  • 1
    • 51249172362 scopus 로고
    • Material effect in fretting wear: Application to iron, titanium, and aluminium alloy
    • P. Blanchard, Ch. Colombié, V. Pellerin, S. Fayeulle, L. Vincent, Material effect in fretting wear: application to iron, titanium, and aluminium alloy, Metal. Trans. A 22 (1991) 1535-1544.
    • (1991) Metal. Trans. A , vol.22 , pp. 1535-1544
    • Blanchard, P.1    Colombié, Ch.2    Pellerin, V.3    Fayeulle, S.4    Vincent, L.5
  • 2
    • 0027583167 scopus 로고
    • Fretting behaviour of titanium alloys
    • S. Fayeulle, P. Blanchard, L. Vincent, Fretting behaviour of titanium alloys, Tribol. Trans. 36 (2) (1993) 267-275.
    • (1993) Tribol. Trans. , vol.36 , Issue.2 , pp. 267-275
    • Fayeulle, S.1    Blanchard, P.2    Vincent, L.3
  • 3
    • 0021493771 scopus 로고
    • A transmission electron microscopy study of the white-ecthing layer on a rail head
    • S.B. Newcomb, W.M. Stobbs, A transmission electron microscopy study of the white-ecthing layer on a rail head, Mater. Sci. Eng. 66 (1984) 195-204.
    • (1984) Mater. Sci. Eng. , vol.66 , pp. 195-204
    • Newcomb, S.B.1    Stobbs, W.M.2
  • 4
    • 0020022737 scopus 로고
    • Butterflies in fatigued ball bearings - Formation mechanisms and structure
    • R. Österlund, O. Vingsbo, L. Vincent, P. Guiradenq, Butterflies in fatigued ball bearings - formation mechanisms and structure, Scand. J. Metall. 11 (1982) 23-32.
    • (1982) Scand. J. Metall. , vol.11 , pp. 23-32
    • Österlund, R.1    Vingsbo, O.2    Vincent, L.3    Guiradenq, P.4
  • 5
    • 0023163488 scopus 로고
    • The temperature effect of scuffing in the sliding wear of steel
    • K.C. Ludema (ed.)
    • B.L. Zhu, Z.X. Yang, J.J. Liu, The temperature effect of scuffing in the sliding wear of steel, in: K.C. Ludema (ed.), Wear of Materials, Vol. 1, 1987, pp. 223-230.
    • (1987) Wear of Materials , vol.1 , pp. 223-230
    • Zhu, B.L.1    Yang, Z.X.2    Liu, J.J.3
  • 6
    • 0029135521 scopus 로고
    • The failure models induced by white layers during impact wear
    • Y.Y. Yang, H.S, Fang, Y.K. Zheng, Z.G. Yang, Z.L. Jiang, The failure models induced by white layers during impact wear, Wear 185 (1995) 17-22.
    • (1995) Wear , vol.185 , pp. 17-22
    • Yang, Y.Y.1    Fang, H.S.2    Zheng, Y.K.3    Yang, Z.G.4    Jiang, Z.L.5
  • 7
    • 0029769116 scopus 로고    scopus 로고
    • Comparison between nanophase formation during friction induced surface wear and mechanical attrition of a pearlitic steel
    • G. Baumann, Y. Zhong, H.J. Fecht, Comparison between nanophase formation during friction induced surface wear and mechanical attrition of a pearlitic steel, Nanostruct. Mater. 7 (1996) 237-244.
    • (1996) Nanostruct. Mater. , vol.7 , pp. 237-244
    • Baumann, G.1    Zhong, Y.2    Fecht, H.J.3
  • 8
    • 0345684238 scopus 로고
    • The synthesis and structure of nanocrystalline materials produced by mechanical attrition: A review
    • C.C. Koch, The synthesis and structure of nanocrystalline materials produced by mechanical attrition: a review, Nanostruct. Mater. 2 (1993) 109-129.
    • (1993) Nanostruct. Mater. , vol.2 , pp. 109-129
    • Koch, C.C.1
  • 11
    • 0026877165 scopus 로고
    • Surface temperature in a fretting contact
    • J.A. Greenwood, A.F. Alliston-Greiner, Surface temperature in a fretting contact, Wear 155 (1992) 269-275.
    • (1992) Wear , vol.155 , pp. 269-275
    • Greenwood, J.A.1    Alliston-Greiner, A.F.2
  • 12
    • 0001665645 scopus 로고
    • Palliative for fretting fatigue
    • R.B. Waterhouse, T.C. Lindely (eds.), Fretting Fatigue
    • J. Beard, Palliative for fretting fatigue, in: R.B. Waterhouse, T.C. Lindely (eds.), Fretting Fatigue, ESIS 18, 1994, pp. 419-436.
    • (1994) ESIS , vol.18 , pp. 419-436
    • Beard, J.1
  • 14
    • 0026876239 scopus 로고
    • Cracking behaviour of various aluminium alloys during fretting wear
    • Z.R. Zhou, S. Fayeulle, L. Vincent, Cracking behaviour of various aluminium alloys during fretting wear, Wear 155 (1992) 317-330.
    • (1992) Wear , vol.155 , pp. 317-330
    • Zhou, Z.R.1    Fayeulle, S.2    Vincent, L.3
  • 15
    • 85165178453 scopus 로고
    • Testing methods in fretting fatigue: A critical appraisal
    • R.B. Waterhouse, M.H. Attia (eds.)
    • L. Vincent, Y. Berthier, M. Godet, Testing methods in fretting fatigue: a critical appraisal, in: R.B. Waterhouse, M.H. Attia (eds.), ASTM-STP 1159, 1992, pp. 33-48.
    • (1992) ASTM-STP , vol.1159 , pp. 33-48
    • Vincent, L.1    Berthier, Y.2    Godet, M.3
  • 16
    • 0029257034 scopus 로고
    • The mixed fretting regime
    • Z.R. Zhou, L. Vincent, The mixed fretting regime, Wear 181-183 (1995) 531-536.
    • (1995) Wear , vol.181-183 , pp. 531-536
    • Zhou, Z.R.1    Vincent, L.2
  • 17
    • 0021499744 scopus 로고
    • An investigation of fatigue and fretting in a dovetail joint
    • C. Ruiz, P.H.B. Boddington, K.C. Chen, An investigation of fatigue and fretting in a dovetail joint, Exp. Mech. 24 (1984) 208-217.
    • (1984) Exp. Mech. , vol.24 , pp. 208-217
    • Ruiz, C.1    Boddington, P.H.B.2    Chen, K.C.3
  • 18
    • 84882729036 scopus 로고
    • Compliance of elastic bodies in contact
    • R.D. Mindlin, Compliance of elastic bodies in contact, ASME J. Appl. Mech. 16 (1949) 259-268.
    • (1949) ASME J. Appl. Mech. , vol.16 , pp. 259-268
    • Mindlin, R.D.1
  • 20
    • 0030295624 scopus 로고    scopus 로고
    • Experimental and numerical investigation of the sliding behaviour in a fretting contact between by poly(methymethacrylate) and a glass counterface
    • A. Krichen, M. Kharrat, A. Chateauminois, Experimental and numerical investigation of the sliding behaviour in a fretting contact between by poly(methymethacrylate) and a glass counterface, Tribol. Int., 29 (1996) 615-624.
    • (1996) Tribol. Int. , vol.29 , pp. 615-624
    • Krichen, A.1    Kharrat, M.2    Chateauminois, A.3
  • 21
    • 0001302818 scopus 로고
    • The detection of flash temperature in a sliding contact by the method of tribo-induced thermoluminescence
    • S. Suzuki, F.E. Kennedy, The detection of flash temperature in a sliding contact by the method of tribo-induced thermoluminescence, J. Tribol. ASME 113 (1991) 120-127.
    • (1991) J. Tribol. ASME , vol.113 , pp. 120-127
    • Suzuki, S.1    Kennedy, F.E.2
  • 22
    • 0041630915 scopus 로고    scopus 로고
    • Grease lubrication in fretting
    • submitted to, to be presented at the World Tribology Congress
    • Z.R. Zhou, Ph. Kapsa, L. Vincent, Grease lubrication in fretting, submitted to J. Tribol. ASME, to be presented at the 1997 World Tribology Congress.
    • (1997) J. Tribol. ASME
    • Zhou, Z.R.1    Kapsa, Ph.2    Vincent, L.3
  • 25
    • 0030993929 scopus 로고    scopus 로고
    • Cracking induced by fretting of aluminium alloys
    • Z.R. Zhou, L. Vincent, Cracking induced by fretting of aluminium alloys, J. Tribol. ASME 119 (1997) 36-42.
    • (1997) J. Tribol. ASME , vol.119 , pp. 36-42
    • Zhou, Z.R.1    Vincent, L.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.