Volumn 80, Issue 6, 1997, Pages 1353-1358

Effect of crystallinity on strength and fracture toughness of Li2O-Al2O3-CaO-SiO2 glass-ceramics

Author keywords

[No Author keywords available]

Indexed keywords

ALUMINA; CALCIUM CARBIDE; COMPOSITION EFFECTS; CRYSTALLIZATION; FRACTURE TOUGHNESS; GLASS; LITHIUM COMPOUNDS; SILICA; SILVER COMPOUNDS; VOLUME FRACTION;

EID: 0031169920     PISSN: 00027820     EISSN: None     Source Type: Journal    
DOI: 10.1111/j.1151-2916.1997.tb02991.x     Document Type: Article
Times cited : (44)

References (17)
  • 1
    • 0028402267 scopus 로고
    • Influence ot Colorants on Crystallization and Mechanical Properties of Lithia-Based Glass-Ceramics
    • K. J. Anusavice, N. Z. Zhang, and J. E. Moorhead, "Influence ot Colorants on Crystallization and Mechanical Properties of Lithia-Based Glass-Ceramics," Dent. Mater., 10 [2] 141-46 (1994).
    • (1994) Dent. Mater. , vol.10 , Issue.2 , pp. 141-146
    • Anusavice, K.J.1    Zhang, N.Z.2    Moorhead, J.E.3
  • 3
    • 0030621975 scopus 로고    scopus 로고
    • Chemical Durability of Dicor and Lithia-Based Glass-Ceramics
    • K. J. Anusavice and N. Z. Zhang, "Chemical Durability of Dicor and Lithia-Based Glass-Ceramics," Dent. Mater., 13 [1] (1997).
    • (1997) Dent. Mater. , vol.13 , Issue.1
    • Anusavice, K.J.1    Zhang, N.Z.2
  • 4
    • 0028369111 scopus 로고
    • Effect of Surface Etching on the Flexure Strength and Fracture Toughness of DICOR Disks Containing Controlled Flaws
    • J. Y. Thompson and K. J. Anusavice, "Effect of Surface Etching on the Flexure Strength and Fracture Toughness of DICOR Disks Containing Controlled Flaws," J. Dent. Res., 73 [2] 505-10 (1994).
    • (1994) J. Dent. Res. , vol.73 , Issue.2 , pp. 505-510
    • Thompson, J.Y.1    Anusavice, K.J.2
  • 5
    • 5544233233 scopus 로고
    • Crystal Structure and Mechanical Properties of Lithia-Based Glass-Ceramics
    • Abstract No. 971
    • K. J. Anusavice and N. Z. Zhang, "Crystal Structure and Mechanical Properties of Lithia-Based Glass-Ceramics," J. Dent. Res., 74 [Special Issue] 522 (Abstract No. 971) (1995).
    • (1995) J. Dent. Res. , vol.74 , Issue.SPEC. ISSUE , pp. 522
    • Anusavice, K.J.1    Zhang, N.Z.2
  • 8
    • 0001280209 scopus 로고
    • Chemical Machining of Photosensitive Glass
    • S. D. Stookey, "Chemical Machining of Photosensitive Glass," Ind. Eng. Chem., 45 [1] 115-18 (1953).
    • (1953) Ind. Eng. Chem. , vol.45 , Issue.1 , pp. 115-118
    • Stookey, S.D.1
  • 9
    • 0015360394 scopus 로고
    • Biaxial Flexure Tests of Ceramic Substrates
    • J. B. Wachtman Jr., W. Capps, and J. Mandel, "Biaxial Flexure Tests of Ceramic Substrates," J. Mater., 7 [2] 188-94 (1972).
    • (1972) J. Mater. , vol.7 , Issue.2 , pp. 188-194
    • Wachtman Jr., J.B.1    Capps, W.2    Mandel, J.3
  • 10
    • 0026180417 scopus 로고
    • Effect of Thermal Tempering on Strength and Crack Propagation Behavior of Feldspathic Porcelains
    • K. J. Anusavice and B. Hojjatie, "Effect of Thermal Tempering on Strength and Crack Propagation Behavior of Feldspathic Porcelains," J. Dent. Res., 70 [6] 1009-13 (1991).
    • (1991) J. Dent. Res. , vol.70 , Issue.6 , pp. 1009-1013
    • Anusavice, K.J.1    Hojjatie, B.2
  • 11
    • 5544235428 scopus 로고    scopus 로고
    • Standard Test Method for Biaxial Flexure Strength (Modulus of Rupture) of Ceramic Substrates
    • ASTM Designation F 394-78. Electronics, American Society for Testing and Materials, Philadelphia, PA
    • Standard Test Method for Biaxial Flexure Strength (Modulus of Rupture) of Ceramic Substrates," ASTM Designation F 394-78. 1981 Annual Book of ASTM Standards, Part 43, Electronics, pp. 802-806. American Society for Testing and Materials, Philadelphia, PA.
    • 1981 Annual Book of ASTM Standards , Issue.43 PART , pp. 802-806
  • 12
    • 84987368857 scopus 로고
    • A Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: II, Strength Method
    • P. Chantikul, G. R. Anstis, B. R. Lawn, and D. B. Marshall, "A Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: II, Strength Method," J. Am. Ceram. Soc., 64 [9] 539-43 (1981).
    • (1981) J. Am. Ceram. Soc. , vol.64 , Issue.9 , pp. 539-543
    • Chantikul, P.1    Anstis, G.R.2    Lawn, B.R.3    Marshall, D.B.4
  • 13
    • 84987306805 scopus 로고
    • A Simple Method for Determining Elastic-Modulus-to-Hardness Ratios Using Koop Ihdentation Measurements
    • D. B. Marshall, T. Noma, and A. G. Evans, "A Simple Method for Determining Elastic-Modulus-to-Hardness Ratios Using Koop Ihdentation Measurements," J. Am. Ceram. Soc., 65 [10] C-175-C-176 (1982).
    • (1982) J. Am. Ceram. Soc. , vol.65 , Issue.10
    • Marshall, D.B.1    Noma, T.2    Evans, A.G.3
  • 14
    • 0012719436 scopus 로고
    • The GLM Procedure
    • SAS Institute, Inc., Cary, NC
    • The GLM Procedure"; pp. 549-640 in SAS/STAT™ User's Guide, release 6.03. SAS Institute, Inc., Cary, NC, 1988.
    • (1988) SAS/STAT™ User's Guide, Release 6.03 , pp. 549-640
  • 16
    • 0023293417 scopus 로고
    • A Review of Surface Crystallization in Vitreous System
    • G. Partridge, "A Review of Surface Crystallization in Vitreous System," Glass Technol., 28 [1] 9-18 (1987).
    • (1987) Glass Technol. , vol.28 , Issue.1 , pp. 9-18
    • Partridge, G.1
  • 17
    • 0008523780 scopus 로고
    • Ph.D. Dissertation. University of Florida, Gainesviile, FL
    • 2 Glass-Ceramics"; Ph.D. Dissertation. University of Florida, Gainesviile, FL, 1995.
    • (1995) 2 Glass-Ceramics
    • Thompson, J.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.