Volumn 38, Issue 1-4, 1997, Pages 483-487

Thermogravimetric and binder removal analysis of injection moulded reinforced ceramic composite

Author keywords

[No Author keywords available]

Indexed keywords

ALUMINA; BINDERS; COMPOSITION EFFECTS; CRACK PROPAGATION; CRYSTAL WHISKERS; DEGRADATION; DIFFUSION IN SOLIDS; HEATING; OXIDATION; SILICON CARBIDE; THERMAL EFFECTS; THERMOGRAVIMETRIC ANALYSIS;

EID: 0031138461     PISSN: 02638223     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0263-8223(97)00083-4     Document Type: Article
Times cited : (3)

References (14)
  • 1
    • 33645793148 scopus 로고
    • Review: Fabrication of engineering ceramics by injection moulding - I. Materials selection
    • Edirisinghe, M.J. and Evans, J.R.G., Review: fabrication of engineering ceramics by injection moulding - I. Materials selection. Int. J. High Tech. Ceram., 1986, 2, 1-31.
    • (1986) Int. J. High Tech. Ceram. , vol.2 , pp. 1-31
    • Edirisinghe, M.J.1    Evans, J.R.G.2
  • 2
    • 0040446085 scopus 로고
    • Review: Fabrication of engineering ceramics by injection moulding - II. Techniques
    • Edirisinghe, M.J. and Evans, J.R.G., Review: fabrication of engineering ceramics by injection moulding - II. Techniques. Int. J. High Tech. Ceram., 1986, 2, 249-278.
    • (1986) Int. J. High Tech. Ceram. , vol.2 , pp. 249-278
    • Edirisinghe, M.J.1    Evans, J.R.G.2
  • 3
    • 0026126456 scopus 로고
    • State of the art injection molding of high-performance ceramics
    • Sakai, T., State of the art injection molding of high-performance ceramics. Advances in Polymer T Technology, 11 (1) (1991/1992) 53-67.
    • (1991) Advances in Polymer t Technology , vol.11 , Issue.1 , pp. 53-67
    • Sakai, T.1
  • 4
    • 0038940579 scopus 로고
    • Fabrication of engineering ceramics by injection moulding
    • Edirisinghe, M.J., Fabrication of engineering ceramics by injection moulding. Ceram. Bull., 1991, 70, (5), 824-828.
    • (1991) Ceram. Bull. , vol.70 , Issue.5 , pp. 824-828
    • Edirisinghe, M.J.1
  • 6
    • 0025384149 scopus 로고
    • Whisker length degradation during the preparation of composite ceramic injection moulding suspensions
    • Stedman, S.J., Evans, J.R.G. and Woodthorpe, J., Whisker length degradation during the preparation of composite ceramic injection moulding suspensions. J. Mat. Sci., 1990, 25, 1025-1032.
    • (1990) J. Mat. Sci. , vol.25 , pp. 1025-1032
    • Stedman, S.J.1    Evans, J.R.G.2    Woodthorpe, J.3
  • 7
    • 0025401078 scopus 로고
    • Rheology of composite ceramic injection moulding suspensions
    • Stedman, S.J., Evans, J.R.G. and Woodthorpe, J., Rheology of composite ceramic injection moulding suspensions. J. Mat. Sci., 1990, 25, 1833-1841.
    • (1990) J. Mat. Sci. , vol.25 , pp. 1833-1841
    • Stedman, S.J.1    Evans, J.R.G.2    Woodthorpe, J.3
  • 8
    • 0027849078 scopus 로고
    • Rheological behavior of injection-moldable silicon powder-silicon carbide whisker formulations
    • Tsao, I. and Danforth, S.C., Rheological behavior of injection-moldable silicon powder-silicon carbide whisker formulations. J. Am. Ceram. Soc., 1993, 76, (12), 2977-2984.
    • (1993) J. Am. Ceram. Soc. , vol.76 , Issue.12 , pp. 2977-2984
    • Tsao, I.1    Danforth, S.C.2
  • 9
    • 0024619905 scopus 로고
    • Properties of ceramic injection moulding formulations part 3 polymer removal
    • Woodthorpe, J., Edirisinghe, M.J. and Evans, J.R.G., Properties of ceramic injection moulding formulations Part 3 Polymer removal. J. Mat. Sci., 1989, 24, 1038-1048.
    • (1989) J. Mat. Sci. , vol.24 , pp. 1038-1048
    • Woodthorpe, J.1    Edirisinghe, M.J.2    Evans, J.R.G.3
  • 10
    • 0024753374 scopus 로고
    • Binder evolution from powder compacts: Thermal profile for injection molded articles
    • Shukla, V.N. and Hill, D.C., Binder evolution from powder compacts: thermal profile for injection molded articles. J. Am. Ceram. Soc., 1989, 72, (10), 1797-1803.
    • (1989) J. Am. Ceram. Soc. , vol.72 , Issue.10 , pp. 1797-1803
    • Shukla, V.N.1    Hill, D.C.2
  • 11
    • 0000582897 scopus 로고
    • Development of temperature-heating rate diagrams for the pyrolytic removal of binder used for powder injection moulding
    • Pinwill, I.E., Edirisinghe, M.J. and Bevis, M.J., Development of temperature-heating rate diagrams for the pyrolytic removal of binder used for powder injection moulding. J. Mat. Sci., 1992, 27, 4381-4388.
    • (1992) J. Mat. Sci. , vol.27 , pp. 4381-4388
    • Pinwill, I.E.1    Edirisinghe, M.J.2    Bevis, M.J.3
  • 12
    • 0001551307 scopus 로고
    • Binder removal from moulded ceramic bodies in different atmospheres
    • Edirisinghe, M.J., Binder removal from moulded ceramic bodies in different atmospheres. J. Mat. Sci. Lett., 1991, 10, 1338-1341.
    • (1991) J. Mat. Sci. Lett. , vol.10 , pp. 1338-1341
    • Edirisinghe, M.J.1
  • 13
    • 0000520139 scopus 로고
    • Interfacial factors affecting the incidence of defects in ceramic mouldings
    • Evans, J.R.G. and Edirisinghe, M.J., Interfacial factors affecting the incidence of defects in ceramic mouldings. J. Mat. Sci., 1991, 26, 2081-2088.
    • (1991) J. Mat. Sci. , vol.26 , pp. 2081-2088
    • Evans, J.R.G.1    Edirisinghe, M.J.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.