5
-
-
0028441809
-
Stability of Molybdenum Disilicide in Combustion Gas Environments
-
Lin, W-Y, Hsu, Y. and Speyer, R.F. "Stability of Molybdenum Disilicide in Combustion Gas Environments", J. Amer. Ceram. Soc., 77, 1162-1168, 1994.
-
(1994)
J. Amer. Ceram. Soc.
, vol.77
, pp. 1162-1168
-
-
Lin, W.-Y.1
Hsu, Y.2
Speyer, R.F.3
-
6
-
-
0026899320
-
2 in Comparison with Other Suicide Materials: Improved High-Temperature Properties
-
2 in Comparison with Other Suicide Materials: Improved High-Temperature Properties", Mater. Sci. Eng., A155, 165-181, 1992.
-
(1992)
Mater. Sci. Eng.
, vol.A155
, pp. 165-181
-
-
Berztiss, D.A.1
Cerchiara, R.R.2
Gulbransen, E.A.3
Pettit, F.S.4
Meier, G.H.5
-
7
-
-
84977696596
-
High-Temperature Oxidation of Molybdenum Disilicide
-
Wirkus, C.D. and Wilder, D.R. "High-Temperature Oxidation of Molybdenum Disilicide", J. Am. Ceramic Soc., 49, 173-176, 1966.
-
(1966)
J. Am. Ceramic Soc.
, vol.49
, pp. 173-176
-
-
Wirkus, C.D.1
Wilder, D.R.2
-
8
-
-
3343003299
-
Electrical and Magnetic Proper ties
-
Chapter II, Plenum Press, New York, NY.
-
Samsonov, G. V. "Electrical and Magnetic Proper ties", Chapter II of Handbook of High Temperature Materials, Plenum Press, New York, NY., 1964, p. 141-166.
-
(1964)
Handbook of High Temperature Materials
, pp. 141-166
-
-
Samsonov, G.V.1
-
9
-
-
0004021785
-
-
Plenum Press, New York, NY
-
Samsonov, G.V. Handbook of the Physiochemical Properties of the Elements, Plenum Press, New York, NY., 1986, p. 320-321.
-
(1986)
Handbook of the Physiochemical Properties of the Elements
, pp. 320-321
-
-
Samsonov, G.V.1
-
10
-
-
0020343058
-
3
-
3", J. Cdn. Ceram. Soc., 51, 1-5, 1982.
-
(1982)
J. Cdn. Ceram. Soc.
, vol.51
, pp. 1-5
-
-
King, H.W.1
Castelliz, K.M.2
Murphy, G.J.3
Manuel, W.4
-
12
-
-
3142736957
-
4 Solid Solutions Containing Mn, Fe, Co, Ni and Cu
-
4 Solid Solutions Containing Mn, Fe, Co, Ni and Cu", J. Cdn. Ceram. Soc., 57, 28-33, 1988.
-
(1988)
J. Cdn. Ceram. Soc.
, vol.57
, pp. 28-33
-
-
King, H.W.1
Payzant, E.A.2
Murphy, J.G.3
Rizkalla, A.S.4
-
13
-
-
3342960241
-
Molybdenum Disilicide as a Component of Modern Composites for Applications at High Temperatures
-
Schlichting, J. "Molybdenum Disilicide as a Component of Modern Composites for Applications at High Temperatures", High Temp. High Press., 10, 214-269, 1978.
-
(1978)
High Temp. High Press.
, vol.10
, pp. 214-269
-
-
Schlichting, J.1
-
14
-
-
0026896733
-
2 Composites at High Temperatures
-
2 Composites at High Temperatures", Mater. Sci. Eng., A155, 121-123, 1992.
-
(1992)
Mater. Sci. Eng.
, vol.A155
, pp. 121-123
-
-
Aikin Jr., R.M.1
-
15
-
-
0026896651
-
A Comparative Overview of Molybdenum Disilicide Composites
-
Vasudevan, A.K. and Petrovic, J.J. A Comparative Overview of Molybdenum Disilicide Composites", Mater. Sci. Eng., A155, 1-17, 1992.
-
(1992)
Mater. Sci. Eng.
, vol.A155
, pp. 1-17
-
-
Vasudevan, A.K.1
Petrovic, J.J.2
-
16
-
-
0024750223
-
Molybdenum Disilicide Heating Elements: Meeting Advanced Ceramics Requirements
-
Bizzarri, V., Linder, B. and Lindskog, N. "Molybdenum Disilicide Heating Elements: Meeting Advanced Ceramics Requirements", Ceramic Bull., 68, 1834-1835 & 1841, 1989.
-
(1989)
Ceramic Bull.
, vol.68
, pp. 1834-1835
-
-
Bizzarri, V.1
Linder, B.2
Lindskog, N.3
-
17
-
-
3342876589
-
Heating Element Materials for the Ceramics Industry
-
Watson, R., Mudway, R. and Sidoti, M. "Heating Element Materials for the Ceramics Industry", Ceram. Eng. Sci. Proc., 11, 1922-1934, 1990.
-
(1990)
Ceram. Eng. Sci. Proc.
, vol.11
, pp. 1922-1934
-
-
Watson, R.1
Mudway, R.2
Sidoti, M.3
-
18
-
-
0002037243
-
Overview of Silicide Coatings for Refractory Metals
-
Eds. T. Grobstien and J. Doychak, The Minerals and Metals Society, Warrendale, PA
-
Packer, C.M. "Overview of Silicide Coatings for Refractory Metals ", in Oxidation of High Temperature Intermetallics, Eds. T. Grobstien and J. Doychak, The Minerals and Metals Society, Warrendale, PA, 1989, p. 235-244.
-
(1989)
Oxidation of High Temperature Intermetallics
, pp. 235-244
-
-
Packer, C.M.1
-
19
-
-
0001397601
-
Processing Temperature Effects on Molybdenum Disilicide
-
Wade, R. and Petrovic, J.J. "Processing Temperature Effects on Molybdenum Disilicide", J. Am. Ceram. Soc., 75, 3160-3162, 1992.
-
(1992)
J. Am. Ceram. Soc.
, vol.75
, pp. 3160-3162
-
-
Wade, R.1
Petrovic, J.J.2
-
20
-
-
0027872822
-
Testing Effect of the High-Temperature Intermetallic MoSi2
-
Chou, T.C. and Nieh, T.G. "Testing Effect of the High-Temperature Intermetallic MoSi2", J. of Metals, 45, 15-21, 1993.
-
(1993)
J. of Metals
, vol.45
, pp. 15-21
-
-
Chou, T.C.1
Nieh, T.G.2
-
25
-
-
84935897781
-
R-Curve Behaviour in Zirconia-Reinforced Molybdenum Disilicide Composites
-
Bhattacharya, A.K. and Petrovic, J.J. "R-Curve Behaviour in Zirconia-Reinforced Molybdenum Disilicide Composites", J. Am. Ceram. Soc., 75, 23-27, 1992.
-
(1992)
J. Am. Ceram. Soc.
, vol.75
, pp. 23-27
-
-
Bhattacharya, A.K.1
Petrovic, J.J.2
-
26
-
-
84985131460
-
Carbon Additions to Molybdenum Disilicide: Improved High-Temperature Mechanical properties
-
Maloy, S., Heuer, A.H., Lewandowski, J. and Petrovic, J.J. "Carbon Additions to Molybdenum Disilicide: Improved High-Temperature Mechanical properties", J. Am. Ceram. Soc., 74, 2704-2706, 1991.
-
(1991)
J. Am. Ceram. Soc.
, vol.74
, pp. 2704-2706
-
-
Maloy, S.1
Heuer, A.H.2
Lewandowski, J.3
Petrovic, J.J.4
-
27
-
-
0026119924
-
2 Composites
-
2 Composites", J. of Metals, 43, 54-57, 1991.
-
(1991)
J. of Metals
, vol.43
, pp. 54-57
-
-
Lee, E.W.1
Cook, J.2
Khan, A.3
Mahapatra, R.4
Waldman, J.5
-
28
-
-
3343013057
-
2 Composites
-
Eds. H.M. Hawthorne and T. Troczynski, Metallurgical Society of CIM, Montreal
-
2 Composites", in Advanced Ceramics for Structural and Triblogical Applications, Eds. H.M. Hawthorne and T. Troczynski, Metallurgical Society of CIM, Montreal, (1995), p. 629-636.
-
(1995)
Advanced Ceramics for Structural and Triblogical Applications
, pp. 629-636
-
-
King, H.W.1
Pho, I.2
Walker, P.A.3
Das Gupta, S.4
Wang, Z.5
-
29
-
-
0000738741
-
Fracture Toughness Determinations by indentation
-
Evans, A.G. and Charles, E.A. "Fracture Toughness Determinations by indentation", J. Am. Ceram. Soc., 59, 371-372, 1976.
-
(1976)
J. Am. Ceram. Soc.
, vol.59
, pp. 371-372
-
-
Evans, A.G.1
Charles, E.A.2
-
30
-
-
0027147450
-
2 Pest during Low Temperature Oxidation
-
2 Pest during Low Temperature Oxidation", J. Mater. Res., 8, 214-226, 1993.
-
(1993)
J. Mater. Res.
, vol.8
, pp. 214-226
-
-
Chou, T.C.1
Nieh, T.G.2
-
31
-
-
0001150513
-
'Pest' Degradation in Beryllides, Suicides, Aluminides and related Compounds
-
Westbrook, J.H. and Wood, D.L. "'Pest' Degradation in Beryllides, Suicides, Aluminides and related Compounds", J. Nucl. Materials, 12, 208-215, 1964.
-
(1964)
J. Nucl. Materials
, vol.12
, pp. 208-215
-
-
Westbrook, J.H.1
Wood, D.L.2
-
32
-
-
0026880286
-
Low Temperature Oxidation of Molybdenum Disilicide
-
Metschter, P.J. "Low Temperature Oxidation of Molybdenum Disilicide", Metall. Trans. A, 23A, 1763-1772, 1992.
-
(1992)
Metall. Trans. A
, vol.23 A
, pp. 1763-1772
-
-
Metschter, P.J.1
-
33
-
-
0026938619
-
2
-
2", J. Mater. Res., 7, 2747-2755, 1992.
-
(1992)
J. Mater. Res.
, vol.7
, pp. 2747-2755
-
-
MacKamey, G.C.1
Tortorelli, P.P.2
DeVan, J.H.3
Carmichael, C.A.4
-
34
-
-
0040845708
-
The Intermediate-Temperature Oxidation Behavior of Molybdenum Disilicide
-
Berkowitz-Mattock, J.B., Blackburn, P.E. and Felten, E.J. "The Intermediate-Temperature Oxidation Behavior of Molybdenum Disilicide", Trans. Met. Soc. AIME, 233, 1093-1099, 1965.
-
(1965)
Trans. Met. Soc. AIME
, vol.233
, pp. 1093-1099
-
-
Berkowitz-Mattock, J.B.1
Blackburn, P.E.2
Felten, E.J.3
|