메뉴 건너뛰기




Volumn 127-131, Issue , 1997, Pages 239-246

Hot isostatically pressed silicon carbide fibre/mullite composites

Author keywords

Ceramic Matrix Composite; Composite; Hot Isostatic Pressing; Oxide Matrix; Silicon Carbide Fibre; Tape Casting

Indexed keywords

CASTING; FABRICATION; FIBER REINFORCED MATERIALS; FIBERS; HOT PRESSING; SILICON CARBIDE; TECHNOLOGY;

EID: 0030704077     PISSN: 10139826     EISSN: 16629795     Source Type: Book Series    
DOI: None     Document Type: Article
Times cited : (4)

References (10)
  • 4
    • 0023965159 scopus 로고
    • Mechanical Properties of a Uniaxially Reinforced Mullite-Silicon Carbide Composite
    • R.N. Singh and A.R. Gaddipati, "Mechanical Properties of a Uniaxially Reinforced Mullite-Silicon Carbide Composite", J. Am. Ceram. Soc., 71 [2] C-100-C-103 (1988)
    • (1988) J. Am. Ceram. Soc. , vol.71 , Issue.2
    • Singh, R.N.1    Gaddipati, A.R.2
  • 5
    • 4243051619 scopus 로고
    • Role of Fiber-Matrix Interfacial Shear Stress on the Toughness of Reinforced Oxide Matrix Composites
    • R.N. Singh, "Role of Fiber-Matrix Interfacial Shear Stress on the Toughness of Reinforced Oxide Matrix Composites", Mat. Res. Soc. Symp. Proc., 120 259-264 (1988)
    • (1988) Mat. Res. Soc. Symp. Proc. , vol.120 , pp. 259-264
    • Singh, R.N.1
  • 6
    • 0347253177 scopus 로고
    • HIPed Carbon Fiber Reinforced Silicon Nitride Composites
    • R. Lundberg, R. Pompe, and R. Carlsson, "HIPed Carbon Fiber Reinforced Silicon Nitride Composites", Ceram. Eng. Sci. Proc., 9 [7-8], 901-906 (1988)
    • (1988) Ceram. Eng. Sci. Proc. , vol.9 , Issue.7-8 , pp. 901-906
    • Lundberg, R.1    Pompe, R.2    Carlsson, R.3
  • 7
    • 0027641494 scopus 로고
    • Microchemical Analysis of the SCS-6 Silicon Carbide Fiber
    • X-J. Ning , P. Pirouz, and S.C. Farmer, "Microchemical Analysis of the SCS-6 Silicon Carbide Fiber", J. Am. Ceram. Soc., 76 [8] 2033-2041 (1993)
    • (1993) J. Am. Ceram. Soc. , vol.76 , Issue.8 , pp. 2033-2041
    • Ning, X.-J.1    Pirouz, P.2    Farmer, S.C.3
  • 8
    • 0026239620 scopus 로고
    • The Microstructure of SCS-6 Fiber
    • X-J. Ning and P. Pirouz, "The Microstructure of SCS-6 Fiber", J. Mater. Res., 6 10 2234-2248 (1991)
    • (1991) J. Mater. Res. , vol.6 , Issue.10 , pp. 2234-2248
    • Ning, X.-J.1    Pirouz, P.2
  • 9
    • 84985173954 scopus 로고
    • Measurement of Fiber/Matrix Interfacial Shear Stress at Elevated Temperatures
    • M.K. Brun, "Measurement of Fiber/Matrix Interfacial Shear Stress at Elevated Temperatures", J. Am. Ceram. Soc., 75 [7] 1914-1917 (1992)
    • (1992) J. Am. Ceram. Soc. , vol.75 , Issue.7 , pp. 1914-1917
    • Brun, M.K.1
  • 10
    • 0029489244 scopus 로고
    • Interfacial Debonding Behavior of Mullite/SiC Continuous Fiber Composite
    • Y. Yamade and Y. Kawaguchi, "Interfacial Debonding Behavior of Mullite/SiC Continuous Fiber Composite", J. Am. Ceram. Soc., 78 [12] 3209-3216 (1995)
    • (1995) J. Am. Ceram. Soc. , vol.78 , Issue.12 , pp. 3209-3216
    • Yamade, Y.1    Kawaguchi, Y.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.