1
-
-
0025489301
-
Sol-Gel Coatings on Continuous Ceramic Fibers
-
R. S. Hay and E. E. Hermes, "Sol-Gel Coatings on Continuous Ceramic Fibers," Cer. Eng. Sci. Proc., 11 [9-10] 1526-1538 (1990).
-
(1990)
Cer. Eng. Sci. Proc.
, vol.11
, Issue.9-10
, pp. 1526-1538
-
-
Hay, R.S.1
Hermes, E.E.2
-
2
-
-
4243072607
-
Zirconia Coatings for Sapphire Fiber-Reinforced Composites
-
Edited by M. D. Sacks, Am. Ceram. Soc., Westerville, OH
-
J. B. Davis, E. Bischoff and A. G. Evans, "Zirconia Coatings for Sapphire Fiber-Reinforced Composites," pp. 631-638 in Advanced Composite Materials, Edited by M. D. Sacks, Am. Ceram. Soc., Westerville, OH (1991).
-
(1991)
Advanced Composite Materials
, pp. 631-638
-
-
Davis, J.B.1
Bischoff, E.2
Evans, A.G.3
-
4
-
-
0027577296
-
Fluoromica Coated Nicalon Fiber Reinforced Glass-Ceramic Composites
-
K. Chyung and S. B. Dawes, "Fluoromica Coated Nicalon Fiber Reinforced Glass-Ceramic Composites," Mater. Sci. Eng., A162 27-33 (1993).
-
(1993)
Mater. Sci. Eng.
, vol.A162
, pp. 27-33
-
-
Chyung, K.1
Dawes, S.B.2
-
5
-
-
84986364569
-
Reactions between Synthetic Mica and Simple Compounds with Application to Oxidation Resistant Ceramic Composites
-
R. F. Cooper and P. C. Hall, "Reactions between Synthetic Mica and Simple Compounds with Application to Oxidation Resistant Ceramic Composites," J. Am. Ceram. Soc., 76 [5] 265-273 (1993).
-
(1993)
J. Am. Ceram. Soc.
, vol.76
, Issue.5
, pp. 265-273
-
-
Cooper, R.F.1
Hall, P.C.2
-
6
-
-
84986347515
-
Fiber Coating Concepts for Brittle Matrix Composites
-
J. B. Davis, J.P.A. Lofvander, A.G. Evans, E. Bischoff, and M.L. Emiliani, "Fiber Coating Concepts for Brittle Matrix Composites," J. Am. Ceram. Soc., 76 [5] 1249-1257 (1993).
-
(1993)
J. Am. Ceram. Soc.
, vol.76
, Issue.5
, pp. 1249-1257
-
-
Davis, J.B.1
Lofvander, J.P.A.2
Evans, A.G.3
Bischoff, E.4
Emiliani, M.L.5
-
7
-
-
0002478202
-
Control of Fiber-Matrix Interface Properties in Ceramic Composites
-
HT-CMC 1, (Bordeaux, France, 21 September 1993). Edited by R. Naslain, J. Lamon, D. Doumeingts, Woodhead, Cambridge
-
R.J. Kerans, "Control of Fiber-Matrix Interface Properties in Ceramic Composites," pp. 301-12, HT-CMC 1, Proceedings of the International Conference on High Temperature Ceramic Matrix Composites, 6th European Conference on Composite Materials (Bordeaux, France, 21 September 1993). Edited by R. Naslain, J. Lamon, D. Doumeingts, Woodhead, Cambridge (1993)
-
(1993)
Proceedings of the International Conference on High Temperature Ceramic Matrix Composites, 6th European Conference on Composite Materials
, pp. 301-312
-
-
Kerans, R.J.1
-
8
-
-
0027576037
-
Functional Interfaces for Oxide/Oxide Composites
-
P.E.D. Morgan and D. B. Marshall, "Functional Interfaces for Oxide/Oxide Composites," Mater. Sci. Eng., A162 15-25 (1993).
-
(1993)
Mater. Sci. Eng.
, vol.A162
, pp. 15-25
-
-
Morgan, P.E.D.1
Marshall, D.B.2
-
9
-
-
0028513806
-
Magnetoplumbite Compounds as a Fiber Coating in Oxide/Oxide Composites
-
M.K. Cinibulk, "Magnetoplumbite Compounds as a Fiber Coating in Oxide/Oxide Composites," Ceram. Eng. Sci. Proc., 15 [5] 721-728 (1994).
-
(1994)
Ceram. Eng. Sci. Proc.
, vol.15
, Issue.5
, pp. 721-728
-
-
Cinibulk, M.K.1
-
10
-
-
0028518764
-
Issues in the Control of Fiber/Matrix Interfaces in Ceramic Composites
-
R. J. Kerans, "Issues in the Control of Fiber/Matrix Interfaces in Ceramic Composites", Scripta Metall. Mat., 31 [8] pp 1079-1085 (1994).
-
(1994)
Scripta Metall. Mat.
, vol.31
, Issue.8
, pp. 1079-1085
-
-
Kerans, R.J.1
-
11
-
-
0012093555
-
Electrophoretic Deposition of Mullite in a Continuous Fashion Utilizing Non-Aqueous Polymeric Sols
-
P. W. Brown, "Electrophoretic Deposition of Mullite in a Continuous Fashion Utilizing Non-Aqueous Polymeric Sols," Cer. Eng. Sci. Proc., 56 369-376 (1995).
-
(1995)
Cer. Eng. Sci. Proc.
, vol.56
, pp. 369-376
-
-
Brown, P.W.1
-
12
-
-
0029338612
-
18 by a Liquid Precursor Route
-
18 by a Liquid Precursor Route," Cer. Eng. Sci. Proc., 16 [4] 395-387 (1995).
-
(1995)
Cer. Eng. Sci. Proc.
, vol.16
, Issue.4
, pp. 395-1387
-
-
Brown, P.W.1
-
13
-
-
0029373509
-
Microstructure and Mechanical Behavior of an Hibonite Interphase in Alumina-Based Composites
-
M. K. Cinibulk, "Microstructure and Mechanical Behavior of an Hibonite Interphase in Alumina-Based Composites," Cer. Eng. Sci. Proc., 16 [5] 633-641 (1995).
-
(1995)
Cer. Eng. Sci. Proc.
, vol.16
, Issue.5
, pp. 633-641
-
-
Cinibulk, M.K.1
-
14
-
-
0029204784
-
Synthesis and Characterization of Lanthanum Hexaluminate Powders and Films
-
M. K. Cinibulk, "Synthesis and Characterization of Lanthanum Hexaluminate Powders and Films," J. Mat. Res., 10 [1] 71-76 (1995).
-
(1995)
J. Mat. Res.
, vol.10
, Issue.1
, pp. 71-76
-
-
Cinibulk, M.K.1
-
15
-
-
0001280382
-
Thermal Stability of some Hexaluminates at 1400°C
-
M. K. Cinibulk, "Thermal Stability of some Hexaluminates at 1400°C," J. Mat. Sci. Lett., 14 651-54 (1995).
-
(1995)
J. Mat. Sci. Lett.
, vol.14
, pp. 651-654
-
-
Cinibulk, M.K.1
-
16
-
-
0029379290
-
The Use of Solid-State Reactions with Volume Loss to Engineer Stress and Porosity into the Fiber-Matrix Interface of a Ceramic Composite
-
R. S. Hay, "The Use of Solid-State Reactions with Volume Loss to Engineer Stress and Porosity into the Fiber-Matrix Interface of a Ceramic Composite," Acta Metall. Mater, 43 [9] 3333-3347 (1995).
-
(1995)
Acta Metall. Mater
, vol.43
, Issue.9
, pp. 3333-3347
-
-
Hay, R.S.1
-
17
-
-
0029324743
-
Ceramic Composites of Monazite and Alumina
-
P.E.D. Morgan and D.B. Marshall,"Ceramic Composites of Monazite and Alumina", J. Am. Ceram. Soc. 78 [6] 1553-63 (1995)
-
(1995)
J. Am. Ceram. Soc.
, vol.78
, Issue.6
, pp. 1553-1563
-
-
Morgan, P.E.D.1
Marshall, D.B.2
-
18
-
-
0029326911
-
High Temperature Stability of Monazite-Alumina Composites
-
P.E.D. Morgan, D.B. Marshall and R.M. Housley,"High Temperature Stability of Monazite-Alumina Composites", J. Mat. Sci. Eng. A A195 [6] 215-222 (1995)
-
(1995)
J. Mat. Sci. Eng. A
, vol.A195
, Issue.6
, pp. 215-222
-
-
Morgan, P.E.D.1
Marshall, D.B.2
Housley, R.M.3
-
19
-
-
5244336049
-
Textured Magnetoplumbite Fiber-Matrix Interphase Derived from Sol-Gel Fiber Coatings
-
submitted
-
M. K. Cinibulk and R. S. Hay, "Textured Magnetoplumbite Fiber-Matrix Interphase Derived from Sol-Gel Fiber Coatings," submitted to J. Am. Cer. Soc.
-
J. Am. Cer. Soc.
-
-
Cinibulk, M.K.1
Hay, R.S.2
-
20
-
-
85033845789
-
Carbon and Oxide Coatings on Continuous Ceramic Fibers
-
Ceramic Matrix Composites - Advanced High Temperature Structural Materials, edited by R. A. Lowden, J. R. Hellmann, M. K. Ferber, S. G. DiPietro, and K. K. Chawla, in press
-
R. S. Hay, M. D. Petry, K. A. Keller, M. K. Cinibulk, and J. R. Welch, "Carbon and Oxide Coatings on Continuous Ceramic Fibers," Ceramic Matrix Composites - Advanced High Temperature Structural Materials, MRS Symposium Proceedings, edited by R. A. Lowden, J. R. Hellmann, M. K. Ferber, S. G. DiPietro, and K. K. Chawla, in press
-
MRS Symposium Proceedings
-
-
Hay, R.S.1
Petry, M.D.2
Keller, K.A.3
Cinibulk, M.K.4
Welch, J.R.5
-
21
-
-
5244219964
-
Displacive Transformations and Their Applications in Structural Ceramics
-
Colloque, in press
-
W. Kriven,"Displacive Transformations and Their Applications in Structural Ceramics", J. de Physique, Colloque, in press.
-
J. de Physique
-
-
Kriven, W.1
-
22
-
-
5244228551
-
Fiber Coating Design Parameters for Ceramic Composites as Implied by Considerations of Debond Crack Roughness
-
A.P. Tomsia and A. Glaeser, eds. Plenum, New York, in press
-
R.J. Kerans and TA Parthasarathy, "Fiber Coating Design Parameters for Ceramic Composites as Implied by Considerations of Debond Crack Roughness" Ceramic Microstrucrures '96: Control at the Atomic Level, A.P. Tomsia and A. Glaeser, eds. Plenum, New York, in press.
-
Ceramic Microstrucrures '96: Control at the Atomic Level
-
-
Kerans, R.J.1
Parthasarathy, T.A.2
-
23
-
-
0029244212
-
The Role of Coating Compliance and Fiber/Matrix Interfacial Topography in Debonding in Ceramic Composites
-
R.J. Kerans, "The Role of Coating Compliance and Fiber/Matrix Interfacial Topography in Debonding in Ceramic Composites," Scripta Metall, et Mat., 32 [4] 505-509 (1994).
-
(1994)
Scripta Metall, et Mat.
, vol.32
, Issue.4
, pp. 505-509
-
-
Kerans, R.J.1
-
24
-
-
0030172315
-
Viability of Oxide Fiber Coatings in Ceramic Composites for Accommodation of Misfit Stresses
-
R.J. Kerans, "Viability of Oxide Fiber Coatings in Ceramic Composites for Accommodation of Misfit Stresses," J. Amer. Ceram. Soc., 79 [6] 1664-68 (1996)
-
(1996)
J. Amer. Ceram. Soc.
, vol.79
, Issue.6
, pp. 1664-1668
-
-
Kerans, R.J.1
-
25
-
-
5244333568
-
Anticipated Consequences of Interfacial Roughness Effects on the Behavior of Selected Ceramic Composites
-
submitted
-
T.A. Parthasarathy and R.J. Kerans, "Anticipated Consequences of Interfacial Roughness Effects on the Behavior of Selected Ceramic Composites", submitted to J. Am. Ceram. Soc.
-
J. Am. Ceram. Soc.
-
-
Parthasarathy, T.A.1
Kerans, R.J.2
-
26
-
-
0032119581
-
Fiber Matrix Interface Properties in High Strength NICALON™/C/SiC Composites as Determined by Rough Surface Analysis of Fiber Pushout Tests
-
to be submitted
-
R.J. Kerans, T.A. Parthasarathy, F. Rebillat and J. Lamon, "Fiber Matrix Interface Properties in High Strength NICALON™/C/SiC Composites as Determined by Rough Surface Analysis of Fiber Pushout Tests", to be submitted, J. Am. Ceram. Soc.
-
J. Am. Ceram. Soc.
-
-
Kerans, R.J.1
Parthasarathy, T.A.2
Rebillat, F.3
Lamon, J.4
-
27
-
-
0042606298
-
Theoretical Analysis of the Fiber Pullout and Pushout Tests
-
R.J. Kerans and T.A. Parthasarathy, "Theoretical Analysis of the Fiber Pullout and Pushout Tests," Jl of Amer. Ceram. Soc., 74 [7] 1585-1596 (1991).
-
(1991)
Jl of Amer. Ceram. Soc.
, vol.74
, Issue.7
, pp. 1585-1596
-
-
Kerans, R.J.1
Parthasarathy, T.A.2
-
28
-
-
0025556885
-
The Contribution of Interfacial Roughness to Sliding Friction of Ceramic Fibers in a Glass Matrix
-
P.D. Jero and R.J. Kerans, "The Contribution of Interfacial Roughness to Sliding Friction of Ceramic Fibers in a Glass Matrix," Scripta Metall. et Mater., 24 2315-2318 (1991).
-
(1991)
Scripta Metall. et Mater.
, vol.24
, pp. 2315-2318
-
-
Jero, P.D.1
Kerans, R.J.2
-
29
-
-
0026074509
-
Effect of Interfacial Roughness on the Frictional Stress Measured Using Pushout Tests
-
P.D. Jero, R.J. Kerans, and T.A. Pathasarathy, "Effect of Interfacial Roughness on the Frictional Stress Measured Using Pushout Tests," Journal of the American Ceramic Society, 74 [11] 2793-2801 (1991).
-
(1991)
Journal of the American Ceramic Society
, vol.74
, Issue.11
, pp. 2793-2801
-
-
Jero, P.D.1
Kerans, R.J.2
Pathasarathy, T.A.3
-
30
-
-
0028532921
-
Analysis of the Effect of Interfacial Roughness on Fiber Debonding and Sliding in Brittle Matrix Composites
-
T.A. Parthasarathy, D.B. Marshall, and R.J. Kerans, "Analysis of the Effect of Interfacial Roughness on Fiber Debonding and Sliding in Brittle Matrix Composites," Acra Metall. et Mater., 42 [11] 3773-3784 (1994).
-
(1994)
Acra Metall. et Mater.
, vol.42
, Issue.11
, pp. 3773-3784
-
-
Parthasarathy, T.A.1
Marshall, D.B.2
Kerans, R.J.3
-
32
-
-
0024613751
-
-
R. J. Kerans, R. S. Hay, N. J. Pagano and T. A. Parthasarathy, Am. Ceram. Soc. Bull., v68, No. 2, p. 429 (1989).
-
(1989)
Am. Ceram. Soc. Bull
, vol.68
, Issue.2
, pp. 429
-
-
Kerans, R.J.1
Hay, R.S.2
Pagano, N.J.3
Parthasarathy, T.A.4
-
33
-
-
19944374295
-
Fiber-Matrix Interphases and Interfaces in Ceramic Matrix Composites processed by CVI
-
R. Naslain, "Fiber-Matrix Interphases and Interfaces in Ceramic Matrix Composites processed by CVI," Composite Interfaces, 1 [3] 253-286 (1993).
-
(1993)
Composite Interfaces
, vol.1
, Issue.3
, pp. 253-286
-
-
Naslain, R.1
-
35
-
-
0025448282
-
Effect of Interfaces on the Properties of Fiber-Reinforced Ceramics
-
H.C. Cao, E. Bischoff, O. Sbaizero, Manfred Ruhle, Anthony G. Evans, David B. Marshall and J.J. Brennan, "Effect of Interfaces on the Properties of Fiber-Reinforced Ceramics", J. Am. Ceram. Soc 73 [6] 1691-99 (1990)
-
(1990)
J. Am. Ceram. Soc
, vol.73
, Issue.6
, pp. 1691-1699
-
-
Cao, H.C.1
Bischoff, E.2
Sbaizero, O.3
Ruhle, M.4
Evans, A.G.5
Marshall, D.B.6
Brennan, J.J.7
-
36
-
-
0030127397
-
Fracture Toughness of 2D Woven SiC/SiC Composites with Multilayered Interphases
-
C. Droillard and J. Lamon, "Fracture Toughness of 2D Woven SiC/SiC Composites with Multilayered Interphases", J. Am. Ceram. Soc., 79 [4], pp.849-58 (1996).
-
(1996)
J. Am. Ceram. Soc.
, vol.79
, Issue.4
, pp. 849-858
-
-
Droillard, C.1
Lamon, J.2
-
37
-
-
0029179546
-
Strong Interfaces in CMCs, Condition for Efficient Multilayered Interphases
-
MRS Fall Meeting (Boston) Materials Research Society
-
C. Droillard, J. Lamon and X. Bourrat, "Strong Interfaces in CMCs, Condition for Efficient Multilayered Interphases", Mat. Res. Soc. Symp. Proc., 1994, MRS Fall Meeting (Boston) Materials Research Society, Vol. 371-6, (1995).
-
(1995)
Mat. Res. Soc. Symp. Proc., 1994
, vol.371
, Issue.6
-
-
Droillard, C.1
Lamon, J.2
Bourrat, X.3
-
38
-
-
0027695329
-
Interfaces and Interfacial Mechanics: Influence on the Mechanical Behavior of Ceramic Matrix Composites
-
Coloque C7, supplement au Journal de Physique III, novembre
-
J. Lamon, "Interfaces and Interfacial Mechanics: Influence on the Mechanical Behavior of Ceramic Matrix Composites", Journal de Physique IV, Coloque C7, supplement au Journal de Physique III, Volume 3 novembre 1993, pp. 1607-1616.
-
(1993)
Journal de Physique IV
, vol.3
, pp. 1607-1616
-
-
Lamon, J.1
-
39
-
-
5244252624
-
Damage and Failure in Ceramic Matrix Minicomposites: Experimental Study and Model
-
In press
-
N. Lissart and J. Lamon, "Damage and Failure in Ceramic Matrix Minicomposites: Experimental Study and Model", Acta Met., In press.
-
Acta Met.
-
-
Lissart, N.1
Lamon, J.2
-
40
-
-
5244380008
-
Microtextures of Interfaces related to Mechanical Properties in Ceramic Fiber Reinforced Ceramic Matrix Composites
-
edited by A.R. Bunsell, J.F. Jamet, A. Massiah, EACM, Bordeaux
-
D. Cojean and M. Monthioux, "Microtextures of Interfaces related to Mechanical Properties in Ceramic Fiber Reinforced Ceramic Matrix Composites", Proc. 5th Europ. Conf. Comp. Mater. (ECCM-5), edited by A.R. Bunsell, J.F. Jamet, A. Massiah, EACM, Bordeaux, 1992, pp. 729-734.
-
(1992)
Proc. 5th Europ. Conf. Comp. Mater. (ECCM-5)
, pp. 729-734
-
-
Cojean, D.1
Monthioux, M.2
-
41
-
-
4043117553
-
Interfacial Bond Strength in Nicalon/C/SiC Composite Materials as Studied by Single-fiber Push-out Tests
-
submitted
-
F. Rebillat, E. Lara-Curzio, J. Lamon, R. Naslain, M.K. Ferber and T.M. Besmann, "Interfacial Bond Strength in Nicalon/C/SiC Composite Materials as Studied by Single-fiber Push-out Tests", submitted to J. Am. Ceram. Soc.
-
J. Am. Ceram. Soc.
-
-
Rebillat, F.1
Lara-Curzio, E.2
Lamon, J.3
Naslain, R.4
Ferber, M.K.5
Besmann, T.M.6
-
42
-
-
5244376859
-
Properties of Multilayered Interphases in SiC/SiC CVI-composites with "Weak" and "Strong" Interfaces
-
submitted
-
F. Rebillat, E. Lara-Curzio, J. Lamon, R. Naslain, M.K. Ferber and T.M. Besmann, "Properties of Multilayered Interphases in SiC/SiC CVI-composites with "Weak" and "Strong" Interfaces", submitted to J. Am. Ceram. Soc.
-
J. Am. Ceram. Soc.
-
-
Rebillat, F.1
Lara-Curzio, E.2
Lamon, J.3
Naslain, R.4
Ferber, M.K.5
Besmann, T.M.6
-
43
-
-
0022715695
-
Fracture Toughness Anisotropy of a Pyrolytic Carbon
-
M. Sakai, R.C. Bradt, D.B. Fischbach,"Fracture Toughness Anisotropy of a Pyrolytic Carbon", J. Matls. Sci. 21 1491-1501 (1986)
-
(1986)
J. Matls. Sci.
, vol.21
, pp. 1491-1501
-
-
Sakai, M.1
Bradt, R.C.2
Fischbach, D.B.3
-
44
-
-
0029547636
-
Fracture, Fatigue and Indentation Behavior of Pyrolytic Carbon for Biomedical Applications
-
Materials Research Society
-
R.O. Ritchie, R.H. Dauskardt, W.W. Gerberich, A. Strojny and E. Lilleodden, "Fracture, Fatigue and Indentation Behavior of Pyrolytic Carbon for Biomedical Applications" Mat. Res. Soc. Symp. Proc. 383, Materials Research Society (1995)
-
(1995)
Mat. Res. Soc. Symp. Proc.
, vol.383
-
-
Ritchie, R.O.1
Dauskardt, R.H.2
Gerberich, W.W.3
Strojny, A.4
Lilleodden, E.5
-
45
-
-
5244295507
-
-
PH.D. Thesis, University of Bordeaux, France
-
C. Droillard, PH.D. Thesis, University of Bordeaux, France, (1993).
-
(1993)
-
-
Droillard, C.1
|