Volumn 30, Issue 23, 1996, Pages 4085-4089

In situ IR study on the initial sulphition and carbonation of Ca(OH)2 and CaO by SO2 polluted air

Author keywords

Ca(OH)2; CaO; Carbonation; In situ DRIFT; Sulphite formation

Indexed keywords

CALCIUM HYDROXIDE; CALCIUM OXIDE; CARBON DIOXIDE; SULFITE; SURFACE WATER;

EID: 0030303338     PISSN: 13522310     EISSN: None     Source Type: Journal    
DOI: 10.1016/1352-2310(96)00139-2     Document Type: Article
Times cited : (12)

References (16)
  • 4
    • 0023964883 scopus 로고
    • Angular dependence of diffuse reflectance infrared spectra. Part III: Linearity of Kubelka - Munk plots
    • Brimmer P. J. and Griffiths P. R. (1988) Angular dependence of diffuse reflectance infrared spectra. Part III: Linearity of Kubelka - Munk plots. Appl. Spectroscopy 42, 242-247.
    • (1988) Appl. Spectroscopy , vol.42 , pp. 242-247
    • Brimmer, P.J.1    Griffiths, P.R.2
  • 5
    • 0028195757 scopus 로고
    • Model study of the first steps in the deterioration of calcareous stone. I. Initial surface sulphite formation on calcite
    • Elfving P., Panas I. and Lindqvist O. (1994a) Model study of the first steps in the deterioration of calcareous stone. I. Initial surface sulphite formation on calcite. Appl. Surf. Sci. 74, 91-98.
    • (1994) Appl. Surf. Sci. , vol.74 , pp. 91-98
    • Elfving, P.1    Panas, I.2    Lindqvist, O.3
  • 6
    • 0028433816 scopus 로고
    • Model study of the first steps in the deterioration of calcareous stone. II. Sulphate formation on calcite
    • Elfving P., Panas I. and Lindqvist O. (1994b) Model study of the first steps in the deterioration of calcareous stone. II. Sulphate formation on calcite. Appl. Surf. Sci. 78, 83-92.
    • (1994) Appl. Surf. Sci. , vol.78 , pp. 83-92
    • Elfving, P.1    Panas, I.2    Lindqvist, O.3
  • 7
    • 0028485131 scopus 로고
    • Model study of the first steps in the deterioration of calcareous stone. III. Manganese and iron mediated sulphation of natural stone
    • Elfving P., Panas I. and Lindqvist O. (1994c) Model study of the first steps in the deterioration of calcareous stone. III. Manganese and iron mediated sulphation of natural stone. Appl. Surf. Sci. 78, 373-384.
    • (1994) Appl. Surf. Sci. , vol.78 , pp. 373-384
    • Elfving, P.1    Panas, I.2    Lindqvist, O.3
  • 14
    • 85030279722 scopus 로고
    • Behaviour of reinforced concrete under the action of flue gases as a function of the cement composition
    • Paris
    • Tischer W. (1980) Behaviour of reinforced concrete under the action of flue gases as a function of the cement composition. In Proc. 7th Int. Congr. on the Chemistry of Cement, Vol. 4, Paris, pp. 788-791.
    • (1980) Proc. 7th Int. Congr. on the Chemistry of Cement , vol.4 , pp. 788-791
    • Tischer, W.1
  • 15
    • 85030279089 scopus 로고
    • (edited by Möller G., Petersons N. and Samuelsson P.), Chap. 9.5. Svensk Byggtjänst, LiberTryck, Stockholm
    • Tuutti K. (1980) In Betonghandbok. Material (edited by Möller G., Petersons N. and Samuelsson P.), Chap. 9.5. Svensk Byggtjänst, LiberTryck, Stockholm.
    • (1980) Betonghandbok. Material
    • Tuutti, K.1
  • 16
    • 0027681368 scopus 로고
    • 2 with calcium deposited on a carbon surface
    • 2 with calcium deposited on a carbon surface. Appl. Surf. Sci. 72, 175-179.
    • (1993) Appl. Surf. Sci. , vol.72 , pp. 175-179
    • Zawadzki, J.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.