Volumn 5, Issue 4, 1996, Pages 462-468

Effect of iron and combined iron and beryllium additions on the fracture toughness and microstructures of squeeze-cast Al-7Si-0.3Mg alloy

Author keywords

Aluminum alloys; Beryllium; Iron; Squeeze casting

Indexed keywords

BERYLLIUM; DEFECTS; EFFECTS; FRACTURE TOUGHNESS; IMPURITIES; IRON; METAL CASTING; MICROSTRUCTURE; POROSITY; SILICON; SURFACE PROPERTIES;

EID: 0030213780     PISSN: 10599495     EISSN: None     Source Type: Journal    
DOI: 10.1007/BF02648843     Document Type: Article
Times cited : (19)

References (12)
  • 1
    • 0024482279 scopus 로고
    • Principles and Applications of Squeeze Casting
    • Jan
    • G.A. Chadwick and T.M. Yue, Principles and Applications of Squeeze Casting, Cast. Technol., Jan 1989, p 6-12
    • (1989) Cast. Technol. , pp. 6-12
    • Chadwick, G.A.1    Yue, T.M.2
  • 3
    • 0019545862 scopus 로고
    • Squeeze Casting of an Aluminium Alloy Containing Small Amount of Silicon Carbide Whisker
    • March
    • A.A. Das and S. Chatterjee, Squeeze Casting of an Aluminium Alloy Containing Small Amount of Silicon Carbide Whisker, Metall. Mater. Technol., March 1981, p 137-142
    • (1981) Metall. Mater. Technol. , pp. 137-142
    • Das, A.A.1    Chatterjee, S.2
  • 5
    • 5544289007 scopus 로고
    • Squeeze Casting: A Potential Foundry Process
    • W.F. Shaw and T. Watmough, Squeeze Casting: A Potential Foundry Process, Foundry, Vol 97, 1969, p 166-173
    • (1969) Foundry , vol.97 , pp. 166-173
    • Shaw, W.F.1    Watmough, T.2
  • 6
    • 0041976615 scopus 로고
    • Ultra High Pressure Casting
    • March
    • J.L. Reiss and E.G. Kron, Ultra High Pressure Casting, Mod. Cast., March 1960, p 89-96
    • (1960) Mod. Cast. , pp. 89-96
    • Reiss, J.L.1    Kron, E.G.2
  • 7
    • 0026850810 scopus 로고
    • Effect of Magnesium, Iron (Impurity) and Solidification Rates on Fracture Toughness of Al-7Si-0.3Mg Casting Alloy
    • S. Murali, K.S. Raman, and K.S.S. Murthy, Effect of Magnesium, Iron (Impurity) and Solidification Rates on Fracture Toughness of Al-7Si-0.3Mg Casting Alloy, Mater. Sci. Eng., Vol A151, 1992, p 1-10
    • (1992) Mater. Sci. Eng. , vol.A151 , pp. 1-10
    • Murali, S.1    Raman, K.S.2    Murthy, K.S.S.3
  • 8
    • 0011409591 scopus 로고
    • Overview: Casting and Heat Treatment Variables of Al-7Si-0.3Mg Alloy
    • March
    • K.T. Kashyap, S. Murali, K.S. Raman, and K.S.S. Murthy, Overview: Casting and Heat Treatment Variables of Al-7Si-0.3Mg Alloy, Mater. Sci. Technol., Vol 9, March 1993, p 189-203
    • (1993) Mater. Sci. Technol. , vol.9 , pp. 189-203
    • Kashyap, K.T.1    Murali, S.2    Raman, K.S.3    Murthy, K.S.S.4
  • 9
    • 0000174849 scopus 로고
    • Effect of Trace Additions (Be, Cr, Mn and Co) on the Mechanical Properties and Fracture Toughness of Fe-containing Al-7Si-0.3Mg Alloy
    • S. Murali, K.S. Raman, and K.S.S. Murthy, Effect of Trace Additions (Be, Cr, Mn and Co) on the Mechanical Properties and Fracture Toughness of Fe-containing Al-7Si-0.3Mg Alloy, Cast Met., Vol 6 (No. 4), 1994, p 189-197
    • (1994) Cast Met. , vol.6 , Issue.4 , pp. 189-197
    • Murali, S.1    Raman, K.S.2    Murthy, K.S.S.3
  • 10
    • 0002321659 scopus 로고
    • 5 Phase in Al-7Si-0.3Mg Alloy with Trace Additions of Be, Mn, Cr and Co
    • 5 Phase in Al-7Si-0.3Mg Alloy with Trace Additions of Be, Mn, Cr and Co, Mater. Charact., Vol 33, 1994, p 99-112
    • (1994) Mater. Charact. , vol.33 , pp. 99-112
    • Murali, S.1    Raman, K.S.2    Murthy, K.S.S.3
  • 12
    • 0037620895 scopus 로고
    • Quality Control in Squeeze Casting of Aluminium
    • S. Rajagopal and W.H. Altergott, Quality Control in Squeeze Casting of Aluminium, AFS Trans., Vol 93, 1985, p 145-154
    • (1985) AFS Trans. , vol.93 , pp. 145-154
    • Rajagopal, S.1    Altergott, W.H.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.