메뉴 건너뛰기




Volumn 26, Issue 6, 1996, Pages 919-931

Frost durability of high strength concrete: Effect of internal cracking on ice formation

Author keywords

[No Author keywords available]

Indexed keywords

CALORIMETRY; CEMENTS; CRACK INITIATION; DURABILITY; FREEZING; FROST RESISTANCE; ICE; LOW TEMPERATURE TESTING; THAWING; WATER; WATER ABSORPTION; WEAR OF MATERIALS;

EID: 0030169774     PISSN: 00088846     EISSN: None     Source Type: Journal    
DOI: 10.1016/0008-8846(96)00066-X     Document Type: Article
Times cited : (76)

References (17)
  • 12
    • 0041963538 scopus 로고
    • Sapporo, Japan, Chapmann & Hall
    • Jacobsen S., Sellevold E.J.:Consec'95, Sapporo, Japan, pp.114-125 Chapmann & Hall (1995)
    • (1995) Consec'95 , pp. 114-125
    • Jacobsen, S.1    Sellevold, E.J.2
  • 14
    • 0041963539 scopus 로고
    • The Norwegian Building Research Institute
    • Sellevold E.J.: Report O 1731 The Norwegian Building Research Institute, 1986
    • (1986) Report O 1731
    • Sellevold, E.J.1
  • 15
    • 0042965304 scopus 로고
    • PhD-thesis, Helsinki University of Technology CT-Report 6
    • Matala S.: PhD-thesis, Helsinki University of Technology CT-Report 6 (1995)
    • (1995)
    • Matala, S.1
  • 17
    • 0042464084 scopus 로고
    • Lund Inst. of Techn., Div. of Building Materials
    • Fagerlund G.: Report TVBM-3056, Lund Inst. of Techn., Div. of Building Materials (1993)
    • (1993) Report TVBM-3056
    • Fagerlund, G.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.