1
-
-
84986409320
-
Strength, degradation, and coating of silica lightguides
-
KURKJIAN, C.R., SIMPKINS, P.G., and INNISS, D.: 'Strength, degradation, and coating of silica lightguides', J. Am. Ceram. Soc., 1993, 76, pp. 1106-1112
-
(1993)
J. Am. Ceram. Soc.
, vol.76
, pp. 1106-1112
-
-
Kurkjian, C.R.1
Simpkins, P.G.2
Inniss, D.3
-
2
-
-
0020098377
-
Temperature dependence of static fatigue of optical fibres coated with a UV-curable polyurethane acrylate
-
CHANDAN, H.C., and KALISH, D.: 'Temperature dependence of static fatigue of optical fibres coated with a UV-curable polyurethane acrylate', J. Am. Ceram. Soc., 1982, 65, (3), pp. 171-173
-
(1982)
J. Am. Ceram. Soc.
, vol.65
, Issue.3
, pp. 171-173
-
-
Chandan, H.C.1
Kalish, D.2
-
3
-
-
0023978831
-
Environmental effects on the static fatigue of silica optical fibre
-
MATTHEWSON, M.J., and KURKJIAN, C.R.: 'Environmental effects on the static fatigue of silica optical fibre', J. Am. Ceram. Soc., 1988, 71, (3), pp. 177-183
-
(1988)
J. Am. Ceram. Soc.
, vol.71
, Issue.3
, pp. 177-183
-
-
Matthewson, M.J.1
Kurkjian, C.R.2
-
4
-
-
0028752330
-
Optical fibre reliability results from the BIARRITZ field trial
-
GOURONNEC, A., GOARIN, R., LE MOIGNE, G., and BAPTISTE, M.: 'Optical fibre reliability results from the BIARRITZ field trial'. Proc. Soc. Photo-Opt. Instrum. Eng., 1994, 2290, pp. 191-203
-
(1994)
Proc. Soc. Photo-Opt. Instrum. Eng.
, vol.2290
, pp. 191-203
-
-
Gouronnec, A.1
Goarin, R.2
Le Moigne, G.3
Baptiste, M.4
-
5
-
-
3042872830
-
Handleability of aged optical fibres
-
GRIFFIOEN, W., VOLOTINEN, T., WILSON, P., GOURONNEC, A., and SVENSSON, T.: 'Handleability of aged optical fibres'. Int. Wire & Cable Symp. Proc., 1995, pp. 857-864
-
(1995)
Int. Wire & Cable Symp. Proc.
, pp. 857-864
-
-
Griffioen, W.1
Volotinen, T.2
Wilson, P.3
Gouronnec, A.4
Svensson, T.5
-
6
-
-
0019007887
-
Liquid nitrogen strengths of coated optical glass fibres
-
FRANCE, P.W., PARADINE, M.J., REEVE, M.H., and NEWNS, G.R.: 'Liquid nitrogen strengths of coated optical glass fibres', J. Mater. Sci., 1980, 15, pp. 825-830
-
(1980)
J. Mater. Sci.
, vol.15
, pp. 825-830
-
-
France, P.W.1
Paradine, M.J.2
Reeve, M.H.3
Newns, G.R.4
-
7
-
-
0022806361
-
Strength measurement of optical fibres by bending
-
MATTHEWSON, M.J., KURKJIAN, C.R., and GULATI, S.T.: 'Strength measurement of optical fibres by bending', J. Am. Ceram. Soc., 1986, 69, (11), pp. 815-821
-
(1986)
J. Am. Ceram. Soc.
, vol.69
, Issue.11
, pp. 815-821
-
-
Matthewson, M.J.1
Kurkjian, C.R.2
Gulati, S.T.3
-
8
-
-
0020237309
-
Tensile strength characteristics of 'perfect' silica fibres
-
KURKJIAN, C.R., KRAUSE, J.T., and PAEK, U.C.: 'Tensile strength characteristics of 'perfect' silica fibres', J. de Phys., 1982, 43, (12) pp. C9-585-586
-
(1982)
J. de Phys.
, vol.43
, Issue.12
-
-
Kurkjian, C.R.1
Krause, J.T.2
Paek, U.C.3
-
9
-
-
0003238584
-
Optical fibre corrosion: Coating contribution to zero-stress aging
-
Postdeadline paper PD21
-
YUCE, H.H., VARACHI, J.P. Jr., KILMER, J.P., KURKJIAN, C.R., and MATTHEWSON, M.J.: 'Optical fibre corrosion: coating contribution to zero-stress aging'. OFC'92 Tech. Dig., 1992, Postdeadline paper PD21
-
(1992)
OFC'92 Tech. Dig.
-
-
Yuce, H.H.1
Varachi Jr., J.P.2
Kilmer, J.P.3
Kurkjian, C.R.4
Matthewson, M.J.5
-
10
-
-
0020721378
-
Strength and fatigue of multicomponent optical glass fibres
-
FRANCE, P.W., DUNCAN, W.J., SMITH, D.J., and BEALES, K.J.: 'Strength and fatigue of multicomponent optical glass fibres', J. Mat. Sci., 1983, 18, pp. 785-792
-
(1983)
J. Mat. Sci.
, vol.18
, pp. 785-792
-
-
France, P.W.1
Duncan, W.J.2
Smith, D.J.3
Beales, K.J.4
-
12
-
-
0016058451
-
Hydrolytic mechanism of glass fracture under load
-
BERSHTEIN, V.A., NIKITIN, V.V., STEPANOV, V.A., and SHAMREI, L.M.: 'Hydrolytic mechanism of glass fracture under load', Sov. Phys.-Solid State, 1974, 15, pp. 2173-2176
-
(1974)
Sov. Phys.-Solid State
, vol.15
, pp. 2173-2176
-
-
Bershtein, V.A.1
Nikitin, V.V.2
Stepanov, V.A.3
Shamrei, L.M.4
-
13
-
-
3042923011
-
Optical fibre strength, fatigue and handleability after aging in a cable
-
SMITH, J.L., DWIVEDI, A., and GARVEY, P.T: 'Optical fibre strength, fatigue and handleability after aging in a cable'. Int. Wire & Cable Symp. Proc., 1995, pp. 848-856
-
(1995)
Int. Wire & Cable Symp. Proc.
, pp. 848-856
-
-
Smith, J.L.1
Dwivedi, A.2
Garvey, P.T.3
-
14
-
-
0012938121
-
Static fatigue transitions in optical glass fibres
-
RITTER, J.E. Jr., ROBERTS, D.R., CUELLAR, E., and KENNEDY, M.T.: 'Static fatigue transitions in optical glass fibres', Glass Technol., 1994, 35, (6), pp. 265-271
-
(1994)
Glass Technol.
, vol.35
, Issue.6
, pp. 265-271
-
-
Ritter Jr., J.E.1
Roberts, D.R.2
Cuellar, E.3
Kennedy, M.T.4
|