Volumn 79, Issue 4, 1996, Pages 843-848

Influence of granule character and compaction on the mechanical properties of sintered silicon nitride

Author keywords

[No Author keywords available]

Indexed keywords

CERAMIC MATERIALS; COMPACTION; COMPRESSIVE STRENGTH; DEFECTS; DRYING; FLOCCULATION; GRANULAR MATERIALS; MECHANICAL PROPERTIES; PH; PH EFFECTS; SLURRIES; SPRAYING;

EID: 0030125726     PISSN: 00027820     EISSN: None     Source Type: Journal    
DOI: 10.1111/j.1151-2916.1996.tb08515.x     Document Type: Article
Times cited : (49)

References (39)
  • 1
    • 0001542934 scopus 로고
    • Fractographic Identification of Strength-Controlling Flaws and Microstructure
    • Edited by R. C. Bradt, D. P. H. Hasselman, and F. F. Lange. Plenum, New York
    • R. W. Rice, "Fractographic Identification of Strength-Controlling Flaws and Microstructure"; pp. 323-45 in Fracture Mechanics of Ceramics, Vol. 1. Edited by R. C. Bradt, D. P. H. Hasselman, and F. F. Lange. Plenum, New York, 1974.
    • (1974) Fracture Mechanics of Ceramics , vol.1 , pp. 323-345
    • Rice, R.W.1
  • 2
    • 0041324453 scopus 로고
    • Strength Improvement of Yttria-Partially-Stabilized Zirconia by Flaw Elimination
    • J. Sung and P. S. Nicholson, "Strength Improvement of Yttria-Partially-Stabilized Zirconia by Flaw Elimination," J. Am. Ceram. Soc., 71 [9] 788-95 (1988).
    • (1988) J. Am. Ceram. Soc. , vol.71 , Issue.9 , pp. 788-795
    • Sung, J.1    Nicholson, P.S.2
  • 3
    • 0020102652 scopus 로고
    • Structural Reliability: A Processing-Dependent Phenomenon
    • A. G. Evans, "Structural Reliability: A Processing-Dependent Phenomenon," J. Am. Ceram. Soc., 65 [3] 127-37 (1982).
    • (1982) J. Am. Ceram. Soc. , vol.65 , Issue.3 , pp. 127-137
    • Evans, A.G.1
  • 4
    • 4243137081 scopus 로고
    • Material Design in Structural Ceramics
    • H. Suzuki, "Material Design in Structural Ceramics" (in Jpn.), Bull. Ceram. Soc. Jpn., 19 [5] 411-16 (1984).
    • (1984) Bull. Ceram. Soc. Jpn. , vol.19 , Issue.5 , pp. 411-416
    • Suzuki, H.1
  • 5
    • 0024481123 scopus 로고
    • Powder Processing Science and Technology for Increased Reliability
    • F. F. Lange, "Powder Processing Science and Technology for Increased Reliability," J. Am. Ceram. Soc., 72 [1] 3-15 (1989).
    • (1989) J. Am. Ceram. Soc. , vol.72 , Issue.1 , pp. 3-15
    • Lange, F.F.1
  • 6
  • 7
    • 0020766356 scopus 로고
    • Processing-Related Fracture Origins: II, Agglomerate Motion and Cracklike Internal Surfaces Caused by Differential Sintering
    • F. F. Lange and M. Metcalf, "Processing-Related Fracture Origins: II, Agglomerate Motion and Cracklike Internal Surfaces Caused by Differential Sintering," J. Am. Ceram. Soc., 66 [6] 398-406 (1983).
    • (1983) J. Am. Ceram. Soc. , vol.66 , Issue.6 , pp. 398-406
    • Lange, F.F.1    Metcalf, M.2
  • 8
  • 9
    • 84985164188 scopus 로고
    • Experiments on Pore Closure during Hot Isostatic Pressing and Forming
    • B. J. Kellett and F. F. Lange, "Experiments on Pore Closure during Hot Isostatic Pressing and Forming," J. Am. Ceram. Soc., 71 [1] 7-12 (1988).
    • (1988) J. Am. Ceram. Soc. , vol.71 , Issue.1 , pp. 7-12
    • Kellett, B.J.1    Lange, F.F.2
  • 10
    • 0024664065 scopus 로고
    • Thermodynamics of Denisfication: I, Sintering of Simple Particle Arrays, Equilibrium Configurations, Pore Stability, and Shrinkage
    • B. J. Kellett and F. F. Lange, "Thermodynamics of Denisfication: I, Sintering of Simple Particle Arrays, Equilibrium Configurations, Pore Stability, and Shrinkage," J. Am. Ceram. Soc., 72 [5] 725-34 (1989).
    • (1989) J. Am. Ceram. Soc. , vol.72 , Issue.5 , pp. 725-734
    • Kellett, B.J.1    Lange, F.F.2
  • 11
    • 0000806302 scopus 로고
    • Direct Study of the Behavior of Flaw-Forming Defect in Sintering
    • K. Uematsu, M. Miyashita, J.-Y. Kim, and N. Uchida, "Direct Study of the Behavior of Flaw-Forming Defect in Sintering," J. Am. Ceram. Soc., 75 [4] 1016-18 (1992).
    • (1992) J. Am. Ceram. Soc. , vol.75 , Issue.4 , pp. 1016-1018
    • Uematsu, K.1    Miyashita, M.2    Kim, J.-Y.3    Uchida, N.4
  • 12
    • 0027552357 scopus 로고
    • Model for the Effect of Powder Packing on the Driving Force for Liquid-Phase Sintering
    • T. M. Shaw, "Model for the Effect of Powder Packing on the Driving Force for Liquid-Phase Sintering," J. Am. Ceram. Soc., 76 [3] 664-70 (1993).
    • (1993) J. Am. Ceram. Soc. , vol.76 , Issue.3 , pp. 664-670
    • Shaw, T.M.1
  • 13
    • 0001553139 scopus 로고
    • Densification of Large Pores: II, Driving Potentials and Kinetics
    • E. B. Slamovich and F. F. Lange, "Densification of Large Pores: II, Driving Potentials and Kinetics," J. Am. Ceram. Soc., 76 [6] 584-90 (1993).
    • (1993) J. Am. Ceram. Soc. , vol.76 , Issue.6 , pp. 584-590
    • Slamovich, E.B.1    Lange, F.F.2
  • 16
    • 0018012082 scopus 로고
    • Character and Compaction Response of Spray-Dried Agglomerates
    • S. J. Lukasiewicz and J. S. Reed, "Character and Compaction Response of Spray-Dried Agglomerates," Am. Ceram. Soc. Bull., 57 [9] 798-801, 805 (1978).
    • (1978) Am. Ceram. Soc. Bull. , vol.57 , Issue.9 , pp. 798-801
    • Lukasiewicz, S.J.1    Reed, J.S.2
  • 20
    • 0024142576 scopus 로고
    • Processing of Highly Concentrated Aqueous α-Alumina Suspensions Stabilized with Polyelectrolytes
    • J. Cesarano III and I. A. Aksay, "Processing of Highly Concentrated Aqueous α-Alumina Suspensions Stabilized with Polyelectrolytes," J. Am. Ceram. Soc., 71 [12] 1062-67 (1988).
    • (1988) J. Am. Ceram. Soc. , vol.71 , Issue.12 , pp. 1062-1067
    • Cesarano III, J.1    Aksay, I.A.2
  • 21
    • 0024481123 scopus 로고
    • Powder Processing Science and Technology for Increased Reliability
    • F. F. Lange, "Powder Processing Science and Technology for Increased Reliability," J. Am. Ceram. Soc., 72 [1] 3-15 (1989).
    • (1989) J. Am. Ceram. Soc. , vol.72 , Issue.1 , pp. 3-15
    • Lange, F.F.1
  • 22
    • 0026856652 scopus 로고
    • Slip Casting of Silicon Nitride and Mechanical Properties of Sintered Body (Part 1)
    • K. Oda, H. Mizuta, Y. Shibasaki, and K. Ohshima, "Slip Casting of Silicon Nitride and Mechanical Properties of Sintered Body (Part 1)," J. Ceram. Soc. Jpn., 100 [5] 714-19 (1992).
    • (1992) J. Ceram. Soc. Jpn. , vol.100 , Issue.5 , pp. 714-719
    • Oda, K.1    Mizuta, H.2    Shibasaki, Y.3    Ohshima, K.4
  • 23
    • 0026910473 scopus 로고
    • Slip Casting of Silicon Nitride and Mechanical Properties of Sintered Body (Part 2)
    • K. Ohshima, K. Oda, and Y. Shibasaki, "Slip Casting of Silicon Nitride and Mechanical Properties of Sintered Body (Part 2)," J. Ceram. Soc. Jpn., 100 [8] 1032-37 (1992).
    • (1992) J. Ceram. Soc. Jpn. , vol.100 , Issue.8 , pp. 1032-1037
    • Ohshima, K.1    Oda, K.2    Shibasaki, Y.3
  • 25
    • 84987266075 scopus 로고
    • A Statistical Distribution Function of Wide Applicability
    • W. Weibull, "A Statistical Distribution Function of Wide Applicability," J. Appl. Mech., 8, 293 (1951).
    • (1951) J. Appl. Mech. , vol.8 , pp. 293
    • Weibull, W.1
  • 26
    • 49949147085 scopus 로고
    • Determination of the Tensile Strength of Rock by a Compression Test of an Irregular Test Piece
    • Y. Hiramatsu and Y. Oka, "Determination of the Tensile Strength of Rock by a Compression Test of an Irregular Test Piece," Int. J. Rock Mech. Min. Sci., 3, 89-99 (1966).
    • (1966) Int. J. Rock Mech. Min. Sci. , vol.3 , pp. 89-99
    • Hiramatsu, Y.1    Oka, Y.2
  • 28
    • 0024640439 scopus 로고
    • Spray-Drying Ceramic Powders
    • S. J. Lukasiewicz, "Spray-Drying Ceramic Powders," J. Am. Ceram. Soc., 72 [4] 617-24 (1989).
    • (1989) J. Am. Ceram. Soc. , vol.72 , Issue.4 , pp. 617-624
    • Lukasiewicz, S.J.1
  • 29
    • 0021121661 scopus 로고
    • Brittle Fracture of Hardmetals: Dependence of Strength on Defect Size Distribution
    • M. G. Gee, "Brittle Fracture of Hardmetals: Dependence of Strength on Defect Size Distribution," Int. J. Mech. Sci., 26 [2] 85-91 (1984).
    • (1984) Int. J. Mech. Sci. , vol.26 , Issue.2 , pp. 85-91
    • Gee, M.G.1
  • 30
    • 0022990427 scopus 로고
    • Fracture Mechanics and Microstructures
    • Edited by R. C. Bradt, A. G. Evans, D. P. H. Hasselman, and F. F. Lange. Plenum, New York
    • M. G. Gee and R. Morrell, "Fracture Mechanics and Microstructures"; pp. 1-22 in Fracture Mechanics of Ceramics, Vol. 8. Edited by R. C. Bradt, A. G. Evans, D. P. H. Hasselman, and F. F. Lange. Plenum, New York, 1986.
    • (1986) Fracture Mechanics of Ceramics , vol.8 , pp. 1-22
    • Gee, M.G.1    Morrell, R.2
  • 31
    • 0000747232 scopus 로고
    • Effect of Microstructure on the Stress to Propagate Inherent Flaws
    • A. G. Evans and G. Tappin, "Effect of Microstructure on the Stress to Propagate Inherent Flaws," Proc. Br. Ceram. Soc., 20, 275-97 (1972).
    • (1972) Proc. Br. Ceram. Soc. , vol.20 , pp. 275-297
    • Evans, A.G.1    Tappin, G.2
  • 32
    • 84987305194 scopus 로고
    • Estimation of Fracture Toughness by Intrinsic Flaw Fractography for Sintered Alpha Silicon Carbide
    • S. G. Seshadri and M. Srinivasan, "Estimation of Fracture Toughness by Intrinsic Flaw Fractography for Sintered Alpha Silicon Carbide," J. Am. Ceram. Soc., 64 [4] C-69-C-71 (1981).
    • (1981) J. Am. Ceram. Soc. , vol.64 , Issue.4
    • Seshadri, S.G.1    Srinivasan, M.2
  • 33
    • 0018032236 scopus 로고
    • Stress Intensity Factor Estimates for a Peripherally Cracked Spherical Void and a Hemispherical Surface Pit
    • F. I. Baratta, "Stress Intensity Factor Estimates for a Peripherally Cracked Spherical Void and a Hemispherical Surface Pit," J. Am. Ceram. Soc., 61 [11-12] 490-93 (1978).
    • (1978) J. Am. Ceram. Soc. , vol.61 , Issue.11-12 , pp. 490-493
    • Baratta, F.I.1
  • 34
    • 84979445838 scopus 로고
    • Correction - Stress Intensity Factor Estimates for a Peripherally Cracked Spherical Void and a Hemispherical Surface Pit
    • F. I. Baratta, "Correction - Stress Intensity Factor Estimates for a Peripherally Cracked Spherical Void and a Hemispherical Surface Pit," J. Am. Ceram. Soc., 62 [9-10] 527 (1979).
    • (1979) J. Am. Ceram. Soc. , vol.62 , Issue.9-10 , pp. 527
    • Baratta, F.I.1
  • 35
    • 84987332289 scopus 로고
    • Refinement of Stress Intensity Factor Estimates for a Peripherally Cracked Spherical Void and a Hemispherical Surface Pit
    • F. I. Baratta, "Refinement of Stress Intensity Factor Estimates for a Peripherally Cracked Spherical Void and a Hemispherical Surface Pit," J. Am. Ceram. Soc., 64 [1] C-3-C-4 (1981).
    • (1981) J. Am. Ceram. Soc. , vol.64 , Issue.1
    • Baratta, F.I.1
  • 37
    • 0016920475 scopus 로고
    • Characteristics of Flaws at Fracture Origins and Fracture Stress - Flaw Size Relations in Various Ceramics
    • H. P. Kirchner, R. M. Gruver, and W. A. Sotter, "Characteristics of Flaws at Fracture Origins and Fracture Stress - Flaw Size Relations in Various Ceramics," Mater. Sci. Eng., 22, 147-56 (1976).
    • (1976) Mater. Sci. Eng. , vol.22 , pp. 147-156
    • Kirchner, H.P.1    Gruver, R.M.2    Sotter, W.A.3
  • 38
    • 0024639760 scopus 로고
    • Tensile Rupture Strength and Fracture Defects of Sintered Silicon Carbide
    • T. Ohji, Y. Yamauchi, W. Kanemaisu, and S. Ito, "Tensile Rupture Strength and Fracture Defects of Sintered Silicon Carbide," J. Am. Ceram. Soc., 72 [4] 688-90 (1989).
    • (1989) J. Am. Ceram. Soc. , vol.72 , Issue.4 , pp. 688-690
    • Ohji, T.1    Yamauchi, Y.2    Kanemaisu, W.3    Ito, S.4
  • 39
    • 0000288812 scopus 로고
    • Design Data for Engineering Ceramics: A Review of the Flexural Test
    • G. D. Quinn and R. Morrell, "Design Data for Engineering Ceramics: A Review of the Flexural Test," J. Am. Ceram. Soc., 74 [9] 2037-66 (1991).
    • (1991) J. Am. Ceram. Soc. , vol.74 , Issue.9 , pp. 2037-2066
    • Quinn, G.D.1    Morrell, R.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.