The influence of gold on the crystallization of iron oxi-hydroxides;Influence de for sur la cristallisation des oxy-hydroxydes de fer

Author keywords

Adsorption; Crystallization; Ferrihydrite; Goethite; Gold; Hematite; Maturation

Indexed keywords

COLLOID; CRYSTALLIZATION; FERRIHYDRITE; GOETHITE; GOLD; HAEMATITE;

EID: 0029729626     PISSN: 12518050     EISSN: None     Source Type: Journal    
DOI: None     Document Type: Article
Times cited : (3)

References (19)
  • 1
    • 0005439880 scopus 로고
    • Géochimie de l'or: Mécanismes de transport et de dépôt
    • Strasbourg
    • BENEDETTI, M., 1991. Géochimie de l'or : Mécanismes de transport et de dépôt. Sri. Géol., Strasbourg, 91,1-48 p.
    • (1991) Sri. Géol. , vol.91
    • Benedetti, M.1
  • 3
    • 0027458215 scopus 로고
    • Régional exploration strategies at Pounga, Gabon, and gold dispersion under equatorial rain forest conditions
    • COLIN, F., LECOMTE, P., EDOU, M1NKO A. et BENEDETTI, M. F., 1993. Régional exploration strategies at Pounga, Gabon, and gold dispersion under equatorial rain forest conditions, Chan. Rech. Min., 510, p. 61-68.
    • (1993) Chan. Rech. Min. , vol.510 , pp. 61-68
    • Colin, F.1    Lecomte, P.2    Edou Mnko, A.3    Benedetti, M.F.4
  • 4
    • 0023163963 scopus 로고
    • Effect of manganese on the transformation of ferrihydrite into goethite and hematite in alkaline media
    • CORNELL, R. M. et GIOVANOLI, R., 1987. Effect of manganese on the transformation of ferrihydrite into goethite and hematite in alkaline media, Clays and Clay Min., 35, p. 11-20.
    • (1987) Clays and Clay Min. , vol.35 , pp. 11-20
    • Cornell, R.M.1    Giovanoli, R.2
  • 7
    • 0027384064 scopus 로고
    • Gold dispersion related to ferricrete pedogenesis in South Mali: Application to geochemical exploration
    • FREYSSINET, P., 1993. Gold dispersion related to ferricrete pedogenesis in South Mali: application to geochemical exploration, Own. Rech. Min., 510, p. 25-40.
    • (1993) Own. Rech. Min. , vol.510 , pp. 25-40
    • Freyssinet, P.1
  • 9
    • 33751270352 scopus 로고
    • Gold and iron oxides associations in supergene conditions: An experimental approach
    • en révision
    • GREFFIÉ, C., BENEDETTI M, F., PARRON, C. et AMOURIC, M., 1995. Gold and iron oxides associations in supergene conditions: an experimental approach, Geochim. Cosmochim. Acta, en révision.
    • (1995) Geochim. Cosmochim. Acta
    • Greffié, C.1    Benedetti, M.F.2    Parron, C.3    Amouric, M.4
  • 10
    • 0041326993 scopus 로고
    • Experimental study of gold precipitation with synthetic iron hydroxides: HRTM-AEM and Mossbauer spectroscopy investigations
    • GREFFIÉ, C., PARRON, C., BEN'EDETTI, M., AMOURIC, M., MARION, P. et COLIN, F. 1993. Experimental study of gold precipitation with synthetic iron hydroxides: HRTM-AEM and Mossbauer spectroscopy investigations, Chem. Geol., 107, p. 297-300.
    • (1993) Chem. Geol. , vol.107 , pp. 297-300
    • Greffié, C.1    Parron, C.2    Ben'Edetti, M.3    Amouric, M.4    Marion, P.5    Colin, F.6
  • 11
    • 44949274547 scopus 로고
    • Physical chemical interpretation of primary charging behaviour of metal (hydr)oxides
    • HIEMSTRA, T. et VAN RIEMSDIJK, W. IL. 1991. Physical chemical interpretation of primary charging behaviour of metal (hydr)oxides. Colloids and Surfaces, 59, p. 7-25.
    • (1991) Colloids and Surfaces , vol.59 , pp. 7-25
    • Hiemstra, T.1    Van Riemsdijk, W.I.L.2
  • 12
    • 0027503694 scopus 로고
    • Local structure of ferrihydrite and feroxyhite by EXAFS spectroscopy
    • MANCEAU. A. et DRITS, V. A., 1993. Local structure of ferrihydrite and feroxyhite by EXAFS spectroscopy, Clay Miner., 28, p. 164-184.
    • (1993) Clay Miner. , vol.28 , pp. 164-184
    • Manceau, A.1    Drits, V.A.2
  • 14
    • 0021335733 scopus 로고
    • The influence of AI on iron oxides. Mil. Unit-cell dimensions of Al-substituted goethtites and estimation of Al from them
    • SCHULZE, D. G., 1984. The influence of AI on iron oxides. Mil. Unit-cell dimensions of Al-substituted goethtites and estimation of Al from them. Clays and Clay Min., 32, p. 36-44.
    • (1984) Clays and Clay Min. , vol.32 , pp. 36-44
    • Schulze, D.G.1
  • 15
    • 0021369869 scopus 로고
    • The influence of Aluminum on iron oxides. X. Properties of Al-substituted goelhites
    • SCHULZE, D. G. et SCHWERTMANN, U., 1984. The influence of Aluminum on iron oxides. X. Properties of Al-substituted goelhites, Clays Miner., 19, p. 521-539.
    • (1984) Clays Miner. , vol.19 , pp. 521-539
    • Schulze, D.G.1    Schwertmann, U.2
  • 16
    • 0024189948 scopus 로고
    • Occurrence and formation of iron oxides in various pedoenvironments
    • STUCKI, J. W., GOODMAN, B. A. and SCHWERTMANX, U., NATO
    • SCHWERTMANN, U., 1988. Occurrence and formation of iron oxides in various pedoenvironments. In Iron in soils and clays minerals, STUCKI, J. W., GOODMAN, B. A. and SCHWERTMANX, U., NATO, 217, p. 267-308.
    • (1988) Iron in Soils and Clays Minerals , vol.217 , pp. 267-308
    • Schwertmann, U.1
  • 17
    • 0020970274 scopus 로고
    • Effect of pH on the formation of goethite and hematite from ferrihydrite
    • SCHWERTMANN, U. et MURAD, E., 1983. Effect of pH on the formation of goethite and hematite from ferrihydrite, Clays and Clay Min., 31, p. 277-284.
    • (1983) Clays and Clay Min. , vol.31 , pp. 277-284
    • Schwertmann, U.1    Murad, E.2
  • 18
    • 0027087616 scopus 로고
    • The influence of aluminum on iron oxides. Part XVI: Hydroxyl and aluminum substitution in synthetic hematites
    • STANJEK, H. et SCHWERTMANN, U., 1992. The influence of aluminum on iron oxides. Part XVI: Hydroxyl and aluminum substitution in synthetic hematites, Clays and Clay Min., 40, p. 347-354.
    • (1992) Clays and Clay Min. , vol.40 , pp. 347-354
    • Stanjek, H.1    Schwertmann, U.2
  • 19
    • 0000155280 scopus 로고
    • Electrical properties of the gold-aqueous solution interface
    • THOMPSON, D. W. et COLLINS, I. R., 1992. Electrical properties of the gold-aqueous solution interface, J. Colloid Interface Sci., 152, p. 197-204.
    • (1992) J. Colloid Interface Sci. , vol.152 , pp. 197-204
    • Thompson, D.W.1    Collins, I.R.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.