Volumn 30, Issue 12, 1996, Pages 1338-1358

Optimum in situ strength design of composite laminates. Part II: Optimum design

Author keywords

[No Author keywords available]

Indexed keywords

BOUND FORMULATION METHOD; IN SITU LAMINAE STRENGTH PARAMETERS; LOAD BEARING CAPACITY; MULTIDIRECTIONAL LAMINATES; OPTIMIZATION PROBLEM FORMALISM; STRESS NORM;

EID: 0029701674     PISSN: 00219983     EISSN: None     Source Type: Journal    
DOI: 10.1177/002199839603001203     Document Type: Article
Times cited : (21)

References (38)
  • 1
    • 0018492059 scopus 로고
    • On the Transverse Cracking and Longitudinal Splitting Behaviour of Glass and Carbon Fibre Reinforced Epoxy Cross Ply Laminates and the Effect of Poisson and Thermally Generated Strain
    • Bailey, J. E., P. T. Curtis and A. Parvizi. 1979. "On the Transverse Cracking and Longitudinal Splitting Behaviour of Glass and Carbon Fibre Reinforced Epoxy Cross Ply Laminates and the Effect of Poisson and Thermally Generated Strain," Proc. Roy. Soc., London, A 366:599-623.
    • (1979) Proc. Roy. Soc., London, A , vol.366 , pp. 599-623
    • Bailey, J.E.1    Curtis, P.T.2    Parvizi, A.3
  • 2
    • 0019536323 scopus 로고
    • On Fibre Debonding Effects and the Mechanism of Transverse-Ply Failure in Cross-Ply Laminates of Glass Fibre Thermoset Composites
    • Bailey, J. E. and A. Parvizi. 1981. "On Fibre Debonding Effects and the Mechanism of Transverse-Ply Failure in Cross-Ply Laminates of Glass Fibre Thermoset Composites," J. Mater. Sci., 16:649-659.
    • (1981) J. Mater. Sci. , vol.16 , pp. 649-659
    • Bailey, J.E.1    Parvizi, A.2
  • 3
    • 0023397243 scopus 로고
    • The in Situ Ply Shear Strength Distributions in Graphite/Epoxy Laminated Composite
    • Chang, F. K. and M. H. Chen. 1987. "The In Situ Ply Shear Strength Distributions in Graphite/Epoxy Laminated Composite," J. Compos. Mater., 21:708-733.
    • (1987) J. Compos. Mater. , vol.21 , pp. 708-733
    • Chang, F.K.1    Chen, M.H.2
  • 4
    • 0025741967 scopus 로고
    • Damage Tolerance of Laminated Composites Containing a Hole and Subjected to Compressive Loadings: Part I-Analysis
    • Chang, F. K. and L. B. Lessard. 1991. "Damage Tolerance of Laminated Composites Containing a Hole and Subjected to Compressive Loadings: Part I-Analysis," J. Compos. Mater., 25:2-43.
    • (1991) J. Compos. Mater. , vol.25 , pp. 2-43
    • Chang, F.K.1    Lessard, L.B.2
  • 5
    • 0026121052 scopus 로고
    • Damage Tolerance of Laminated Composites Containing an Open Hole and Subjected to Tensile Loadings
    • Chang, K. Y., S. Liu and F. K. Chang. 1991. "Damage Tolerance of Laminated Composites Containing an Open Hole and Subjected to Tensile Loadings," J. Compos. Mater., 25:274-301.
    • (1991) J. Compos. Mater. , vol.25 , pp. 274-301
    • Chang, K.Y.1    Liu, S.2    Chang, F.K.3
  • 6
    • 0043179700 scopus 로고
    • Sensitivity Analysis and a Mixed Approach to the Optimization of Symmetric Layered Composite Plates
    • Cheng, K. 1986. "Sensitivity Analysis and a Mixed Approach to the Optimization of Symmetric Layered Composite Plates," Engng Optimiz., 9:233-247.
    • (1986) Engng Optimiz. , vol.9 , pp. 233-247
    • Cheng, K.1
  • 7
    • 85129342846 scopus 로고
    • The Dependence of Transverse Cracking and Delamination on Ply Thickness in Graphite/Epoxy Laminates
    • K. L. Reifsnider, ed.
    • Crossman, F. W. and A. S. D. Wang. 1982. "The Dependence of Transverse Cracking and Delamination on Ply Thickness in Graphite/Epoxy Laminates," in Damage in Composite Materials, ASTM STP 775, K. L. Reifsnider, ed., pp. 118-139.
    • (1982) Damage in Composite Materials, ASTM STP 775 , pp. 118-139
    • Crossman, F.W.1    Wang, A.S.D.2
  • 8
    • 0023328719 scopus 로고
    • Analysis of Progressive Matrix Cracking in Composite Laminates II-First Ply Failure
    • Dvorak, G. J. and N. Laws. 1987. "Analysis of Progressive Matrix Cracking in Composite Laminates II-First Ply Failure," J. Compos. Mater., 21:309-329.
    • (1987) J. Compos. Mater. , vol.21 , pp. 309-329
    • Dvorak, G.J.1    Laws, N.2
  • 9
    • 0343835583 scopus 로고
    • Is There a Size Effect in Composites? Comments on Designer's Corner by Carl Zweben
    • Edge, E. C. 1994. "Is There a Size Effect in Composites? Comments on Designer's Corner by Carl Zweben," Composites, 25:957-958.
    • (1994) Composites , vol.25 , pp. 957-958
    • Edge, E.C.1
  • 10
    • 0020098389 scopus 로고
    • Experimental Determination of in Situ Transverse Lamina Strength in Graphite/Epoxy Laminates
    • Flaggs, D. L. and M. H. Kural. 1982. "Experimental Determination of In Situ Transverse Lamina Strength in Graphite/Epoxy Laminates," J. Compos. Mater., 16:103-116.
    • (1982) J. Compos. Mater. , vol.16 , pp. 103-116
    • Flaggs, D.L.1    Kural, M.H.2
  • 11
    • 0025862851 scopus 로고
    • Strength Optimization of Laminated Composites with Respect to Layer Thickness and/or Layer Orientation Angle
    • Fukunaga, H. and G. N. Vanderplaats. 1991. "Strength Optimization of Laminated Composites with Respect to Layer Thickness and/or Layer Orientation Angle," Computers and Structures, 40:1429-1439.
    • (1991) Computers and Structures , vol.40 , pp. 1429-1439
    • Fukunaga, H.1    Vanderplaats, G.N.2
  • 12
    • 0017428097 scopus 로고
    • Multiple Transverse Fracture in 90° Cross-Ply Laminates of a Glass Fibre-Reinforced Polyester
    • Garrett, K. W. and J. E. Bailey. 1977. "Multiple Transverse Fracture in 90° Cross-Ply Laminates of a Glass Fibre-Reinforced Polyester," J. Mater. Sci., 12:157-168.
    • (1977) J. Mater. Sci. , vol.12 , pp. 157-168
    • Garrett, K.W.1    Bailey, J.E.2
  • 13
    • 5844327682 scopus 로고
    • Stacking-Sequence Optimization for Buckling of Laminated Plates by Integer Programming
    • Haftka, R. T. and J. L. Walsh. 1992. "Stacking-Sequence Optimization for Buckling of Laminated Plates by Integer Programming," AIAA J., 14:718-724.
    • (1992) AIAA J. , vol.14 , pp. 718-724
    • Haftka, R.T.1    Walsh, J.L.2
  • 14
    • 0019024701 scopus 로고
    • Failure Criteria for Unidirectional Fibre Composites
    • Hashin, Z. 1980. "Failure Criteria for Unidirectional Fibre Composites," J. Appl. Mech., 47:329-334.
    • (1980) J. Appl. Mech. , vol.47 , pp. 329-334
    • Hashin, Z.1
  • 15
    • 0020735383 scopus 로고
    • Damage Development in CFRP Laminates under Monotonie and Cyclic Stressing
    • Harrison, R. P. and M. G. Bader. 1983. "Damage Development in CFRP Laminates Under Monotonie and Cyclic Stressing," Fibre Science and Technology, 18:163-180.
    • (1983) Fibre Science and Technology , vol.18 , pp. 163-180
    • Harrison, R.P.1    Bader, M.G.2
  • 16
    • 0020129076 scopus 로고
    • Influence of Layer Thickness on the Strength of Angle-Ply Laminates
    • Herakovich, C. T. 1982. "Influence of Layer Thickness on the Strength of Angle-Ply Laminates," J. Compos. Mater., 16:216-227.
    • (1982) J. Compos. Mater. , vol.16 , pp. 216-227
    • Herakovich, C.T.1
  • 17
    • 0001546191 scopus 로고
    • The Brittle Strength of Orthotropic Materials
    • Hoffman, O. 1967. "The Brittle Strength of Orthotropic Materials," J. Compos. Mater. , 1:200-206.
    • (1967) J. Compos. Mater. , vol.1 , pp. 200-206
    • Hoffman, O.1
  • 18
    • 0020187568 scopus 로고
    • Crack Kinking and Curving
    • Karihaloo, B. L. 1982. "Crack Kinking and Curving," Mech. Mater., 1:189-201.
    • (1982) Mech. Mater. , vol.1 , pp. 189-201
    • Karihaloo, B.L.1
  • 19
    • 0026711755 scopus 로고
    • Mechanics of Multiple Periodic Brittle Matrix Cracks in Unidirectional Fibre-Reinforced Composites
    • Kaw, A. K. and G. H. Besterfield. 1992. "Mechanics of Multiple Periodic Brittle Matrix Cracks in Unidirectional Fibre-Reinforced Composites," Int. J. Solids Struct., 29:1193-1207.
    • (1992) Int. J. Solids Struct. , vol.29 , pp. 1193-1207
    • Kaw, A.K.1    Besterfield, G.H.2
  • 20
    • 84992286010 scopus 로고
    • Experimental Observations of Free-Edge Delamination
    • N. J. Pagano, ed., Amsterdam: Elsevier
    • Kim, R. Y. 1989. "Experimental Observations of Free-Edge Delamination," in Interlaminar Response of Composite Materials, N. J. Pagano, ed., Amsterdam: Elsevier, pp. 111-160.
    • (1989) Interlaminar Response of Composite Materials , pp. 111-160
    • Kim, R.Y.1
  • 21
    • 0028531430 scopus 로고
    • A Finite Strip Analysis of Cracked Laminates
    • Li, S., S. R. Reid and P. D. Soden. 1994. "A Finite Strip Analysis of Cracked Laminates," Mechanics of Materials, 18:289-311.
    • (1994) Mechanics of Materials , vol.18 , pp. 289-311
    • Li, S.1    Reid, S.R.2    Soden, P.D.3
  • 22
    • 0021898280 scopus 로고
    • Design of Laminated Fibrous Composite Plates with Required Flexural Stiffness
    • J. R. Vinson and M. Taya, eds.
    • Miki, M. 1985. "Design of Laminated Fibrous Composite Plates with Required Flexural Stiffness," in Recent Advances in Composites in the United States and Japan, ASTM STP 864, J. R. Vinson and M. Taya, eds., pp. 387-400.
    • (1985) Recent Advances in Composites in the United States and Japan, ASTM STP 864 , pp. 387-400
    • Miki, M.1
  • 23
    • 0002780711 scopus 로고
    • Multicriterion Structural Optimization via Bound Formulation and Mathematical Programming
    • Olhoff, N. 1989. "Multicriterion Structural Optimization via Bound Formulation and Mathematical Programming," Struct. Optimiz., 1:11-17.
    • (1989) Struct. Optimiz. , vol.1 , pp. 11-17
    • Olhoff, N.1
  • 24
    • 0020161065 scopus 로고
    • An Optimal Design of Simple Symmetric Laminates under the First Ply Failure Criterion
    • Park, W. J. 1982. "An Optimal Design of Simple Symmetric Laminates Under the First Ply Failure Criterion," J. Compos. Mater., 16:341-355.
    • (1982) J. Compos. Mater. , vol.16 , pp. 341-355
    • Park, W.J.1
  • 25
    • 0000269955 scopus 로고
    • Constrained Cracking in Glass Fibre-Reinforced Epoxy Cross-Ply Laminates
    • Parvizi, A., K. W. Garrett and J. E. Bailey. 1978. "Constrained Cracking in Glass Fibre-Reinforced Epoxy Cross-Ply Laminates," J. Mater. Sci., 13:195-201.
    • (1978) J. Mater. Sci. , vol.13 , pp. 195-201
    • Parvizi, A.1    Garrett, K.W.2    Bailey, J.E.3
  • 26
    • 84970123602 scopus 로고
    • A Theory for Progressive Matrix Cracking in Composite Laminates
    • Tan, S. C. and R. J. Nuismer. 1989. "A Theory for Progressive Matrix Cracking in Composite Laminates," J. Compos. Mater., 23:1029-1047.
    • (1989) J. Compos. Mater. , vol.23 , pp. 1029-1047
    • Tan, S.C.1    Nuismer, R.J.2
  • 27
    • 0014974615 scopus 로고
    • A General Theory of Strength for Anisotropic Materials
    • Tsai, S. and E. Wu. 1970. "A General Theory of Strength for Anisotropic Materials," J. Compos. Mater., 5:58-80.
    • (1970) J. Compos. Mater. , vol.5 , pp. 58-80
    • Tsai, S.1    Wu, E.2
  • 31
    • 0015110952 scopus 로고
    • Design of Optimum Structures
    • Venkayya, V. B. 1971. "Design of Optimum Structures," Computer & Struct., 1:265-309.
    • (1971) Computer & Struct. , vol.1 , pp. 265-309
    • Venkayya, V.B.1
  • 32
    • 0021430395 scopus 로고
    • A Stochastic Model for the Growth of Matrix Cracks in Composite Laminates
    • Wang, A. S. D., P. C. Chou and S. C. Lei. 1984. "A Stochastic Model for the Growth of Matrix Cracks in Composite Laminates," J. Compos. Mater., 18:239-254.
    • (1984) J. Compos. Mater. , vol.18 , pp. 239-254
    • Wang, A.S.D.1    Chou, P.C.2    Lei, S.C.3
  • 33
    • 0008285450 scopus 로고
    • Cracked Composite Laminates Least Prone to Delamination
    • London
    • Wang, J. and B. L. Karihaloo. 1994a. "Cracked Composite Laminates Least Prone to Delamination," Proc. Roy. Soc., London, A444:17-35.
    • (1994) Proc. Roy. Soc. , vol.A444 , pp. 17-35
    • Wang, J.1    Karihaloo, B.L.2
  • 34
    • 0028165301 scopus 로고
    • Mode II and Mode III Stress Singularities and Intensities at a Crack Tip Terminating on a Transversely Isotropic-Orthotropic Bimaterial Interface
    • London
    • Wang, J. and B. L. Karihaloo. 1994b. "Mode II and Mode III Stress Singularities and Intensities at a Crack Tip Terminating on a Transversely Isotropic-Orthotropic Bimaterial Interface," Proc. Roy. Soc., London: A444:447-460.
    • (1994) Proc. Roy. Soc. , vol.A444 , pp. 447-460
    • Wang, J.1    Karihaloo, B.L.2
  • 35
    • 0012895445 scopus 로고
    • Mode I Stress Singularity and Intensity Factor at a Crack Tip Terminating at a Transversely Isotropic-Orthotropic Bimaterial Interface
    • to appear
    • Wang, J. and B. L. Karihaloo. 1995a. "Mode I Stress Singularity and Intensity Factor at a Crack Tip Terminating at a Transversely Isotropic-Orthotropic Bimaterial Interface," Int. J. Fracture (to appear).
    • (1995) Int. J. Fracture
    • Wang, J.1    Karihaloo, B.L.2
  • 36
    • 0029224308 scopus 로고
    • Multiple Cracking in Angle-Ply Composite Laminates
    • Wang, J. and B. L. Karihaloo. 1995b. "Multiple Cracking in Angle-Ply Composite Laminates," J. Compos. Mater, 29:1321-1336.
    • (1995) J. Compos. Mater , vol.29 , pp. 1321-1336
    • Wang, J.1    Karihaloo, B.L.2
  • 37
    • 0017991795 scopus 로고
    • Analysis of Laminate Strength and Its Distribution
    • Yamada, S. E. and C. T. Sun. 1979. "Analysis of Laminate Strength and Its Distribution," J. Compos. Mater., 12:275-284.
    • (1979) J. Compos. Mater. , vol.12 , pp. 275-284
    • Yamada, S.E.1    Sun, C.T.2
  • 38
    • 0000222846 scopus 로고
    • Is There a Size Effect in Composites?
    • Zweben, C. 1994. "Is There a Size Effect in Composites?" Composites, 25:451-454.
    • (1994) Composites , vol.25 , pp. 451-454
    • Zweben, C.1