메뉴 건너뛰기




Volumn 182, Issue 1-3, 1996, Pages 75-83

Suppression of microbial pyrite oxidation by fatty acid amine treatment

Author keywords

acid mine drainage; fatty acid amine; pyrite; Thiobacillus ferrooxidans

Indexed keywords

PYRITE; UNCLASSIFIED DRUG;

EID: 0029667956     PISSN: 00489697     EISSN: None     Source Type: Journal    
DOI: 10.1016/0048-9697(95)05052-3     Document Type: Article
Times cited : (15)

References (35)
  • 1
    • 0343260891 scopus 로고
    • A novel concept of safe disposal of acid generating tailings by agglomeration and encapsulating alkaline and bacterial additives
    • R.W. Smith and M. Misra (Eds.), TMS, Warrendale, Pennsylvania, USA
    • Amaratunga, M.L., 1991. A novel concept of safe disposal of acid generating tailings by agglomeration and encapsulating alkaline and bacterial additives. In: R.W. Smith and M. Misra (Eds.), Mineral Bioprocessing, TMS, Warrendale, Pennsylvania, USA, pp. 389-400.
    • (1991) Mineral Bioprocessing , pp. 389-400
    • Amaratunga, M.L.1
  • 3
    • 0014759048 scopus 로고
    • Microbiological factor in acid mine drainage formation: A pilot plant study
    • Baker, R.A. and A.G. Wilshire, 1970. Microbiological factor in acid mine drainage formation: a pilot plant study. Environ. Sci. Technol., 4: 401-407.
    • (1970) Environ. Sci. Technol. , vol.4 , pp. 401-407
    • Baker, R.A.1    Wilshire, A.G.2
  • 4
    • 0342391305 scopus 로고
    • Mine and mill wastewater Treatment
    • Mining, Mineral and Metallurgical Process Division, Environmental Protection, Environment Canada
    • Bell, A. and K.D. Phinney, 1987. Mine and Mill Wastewater Treatment. Report EPS 3/HA. Mining, Mineral and Metallurgical Process Division, Environmental Protection, Environment Canada.
    • (1987) Report EPS 3/HA
    • Bell, A.1    Phinney, K.D.2
  • 5
    • 0018457309 scopus 로고
    • Anodic behaviour of pyrite in acid solutions
    • Biegler, T. and D.A. Swift, 1979. Anodic behaviour of pyrite in acid solutions. Electrochim. Acta, 24: 415-420.
    • (1979) Electrochim. Acta , vol.24 , pp. 415-420
    • Biegler, T.1    Swift, D.A.2
  • 7
    • 0015613721 scopus 로고
    • An investigation into the kinetics and mechanism of the oxidation of iron (II) by oxygen in aqueous chloride solution
    • Colborn, R.P. and M.J. Nicol, 1973. An investigation into the kinetics and mechanism of the oxidation of iron (II) by oxygen in aqueous chloride solution. J. S. Afr. Inst. Min. Metall., 73: 281-289.
    • (1973) J. S. Afr. Inst. Min. Metall. , vol.73 , pp. 281-289
    • Colborn, R.P.1    Nicol, M.J.2
  • 8
    • 0001637114 scopus 로고
    • An iron-oxidizing bacterium from the acid drainage of some bituminous coal mines
    • Colmer, A.R., K.L. Temple and M.E. Hinkle, 1950. An iron-oxidizing bacterium from the acid drainage of some bituminous coal mines. J. Bacteriol., 59: 317-328.
    • (1950) J. Bacteriol. , vol.59 , pp. 317-328
    • Colmer, A.R.1    Temple, K.L.2    Hinkle, M.E.3
  • 9
    • 0008535352 scopus 로고
    • Advances in the microbiological leaching of sulphide ores
    • Duncan, D.W. and P.C. Trussell, 1964. Advances in the microbiological leaching of sulphide ores. Can. Metall. Q., 3: 43-55.
    • (1964) Can. Metall. Q. , vol.3 , pp. 43-55
    • Duncan, D.W.1    Trussell, P.C.2
  • 10
    • 23744505768 scopus 로고
    • Leaching of chalcopyrite with Thiobacillus ferrooxidans: Effect of surfactant and shaking
    • Duncan, D.W., P.C. Trussell and C.C. Walden, 1964. Leaching of chalcopyrite with Thiobacillus ferrooxidans: effect of surfactant and shaking. Appl. Microbiol., 12: 122-126.
    • (1964) Appl. Microbiol. , vol.12 , pp. 122-126
    • Duncan, D.W.1    Trussell, P.C.2    Walden, C.C.3
  • 11
    • 0343696545 scopus 로고
    • A new technology for armoring and deactivating pyrite
    • Singhal et al. (Eds.), A.A. Balkema, Rotterdam, The Netherlands
    • Evangelou, V.P. and X. Huang, 1992. A new technology for armoring and deactivating pyrite. In: Singhal et al. (Eds.), Environmental Issues and Waste Management in Energy and Minerals Production, A.A. Balkema, Rotterdam, The Netherlands, pp. 413-417.
    • (1992) Environmental Issues and Waste Management in Energy and Minerals Production , pp. 413-417
    • Evangelou, V.P.1    Huang, X.2
  • 12
    • 0002300949 scopus 로고
    • Oxidation of pyrite by iron sulfate solution
    • Garrels, R.M. and M.E. Thompson, 1960. Oxidation of pyrite by iron sulfate solution. Am. J. Sci., 258A: 57-67.
    • (1960) Am. J. Sci. , vol.258 A , pp. 57-67
    • Garrels, R.M.1    Thompson, M.E.2
  • 13
    • 79952189559 scopus 로고
    • A case history of an acid generation abatement program for an abandoned copper mine
    • The Vancouver Geotechnical Society, BC
    • Healey, P.M. and A.M. Robertson, 1989. A case history of an acid generation abatement program for an abandoned copper mine. In: Geotechnical Aspects of Tailings Disposal and Acid Mine Drainage. The Vancouver Geotechnical Society, BC.
    • (1989) Geotechnical Aspects of Tailings Disposal and Acid Mine Drainage
    • Healey, P.M.1    Robertson, A.M.2
  • 14
    • 0002919918 scopus 로고
    • Potential importance of sulfate reduction processes in wetlands constructed to treat mine drainage
    • D.A. Hammer (Ed.), Lewis Publishers, MI, USA
    • Hedin, R.S., R.W. Hammack and D.M. Hyman, 1989. Potential importance of sulfate reduction processes in wetlands constructed to treat mine drainage. In: D.A. Hammer (Ed.), Constructed Wetlands for wastewater treatment, Lewis Publishers, MI, USA, pp. 508-514.
    • (1989) Constructed Wetlands for Wastewater Treatment , pp. 508-514
    • Hedin, R.S.1    Hammack, R.W.2    Hyman, D.M.3
  • 18
    • 0019547982 scopus 로고
    • Biogeochemistry of acid mine drainage and a method to control acid formation
    • Kleinmann, R.L.P., D.A. Crerar and R.R. Pacelli, 1981. Biogeochemistry of acid mine drainage and a method to control acid formation. Min. Eng., 33: 300-305.
    • (1981) Min. Eng. , vol.33 , pp. 300-305
    • Kleinmann, R.L.P.1    Crerar, D.A.2    Pacelli, R.R.3
  • 19
    • 0023436184 scopus 로고
    • Passivation of pyrite oxidation with metal cations
    • Lalvani, S.B. and M. Shami, 1989. Passivation of pyrite oxidation with metal cations. J. Mater. Sci., 22: 3503-3507.
    • (1989) J. Mater. Sci. , vol.22 , pp. 3503-3507
    • Lalvani, S.B.1    Shami, M.2
  • 20
    • 0343696542 scopus 로고
    • Passivation of pyrite due to surface treatment
    • Lalvani, S.B., B.A. Deneve and A. Weston, 1990. Passivation of pyrite due to surface treatment. Fuel, 69: 1567-1569.
    • (1990) Fuel , vol.69 , pp. 1567-1569
    • Lalvani, S.B.1    Deneve, B.A.2    Weston, A.3
  • 21
    • 0019389964 scopus 로고
    • Inhibition of acid mine drainage formation: The role of insoluble iron compounds
    • Nebgen, J.W., W.H. Engelmann and D.F. Weatherman, 1981. Inhibition of acid mine drainage formation: the role of insoluble iron compounds. J. Environ. Sci., 24: 23-27.
    • (1981) J. Environ. Sci. , vol.24 , pp. 23-27
    • Nebgen, J.W.1    Engelmann, W.H.2    Weatherman, D.F.3
  • 22
    • 0024476177 scopus 로고
    • Reduction of acid generation in mine tailings through the use of moisture-retaining cover layer as oxygen barriers
    • Nicholson, V.R., R.W. Gillham, J.A. Cherry and E.J. Reardon, 1989. Reduction of acid generation in mine tailings through the use of moisture-retaining cover layer as oxygen barriers. Can. Geotech., 26: 1-8.
    • (1989) Can. Geotech. , vol.26 , pp. 1-8
    • Nicholson, V.R.1    Gillham, R.W.2    Cherry, J.A.3    Reardon, E.J.4
  • 23
    • 85030187527 scopus 로고
    • Suppression of pyrite oxidation by fatty acid amine treatment
    • J.P. Hager et al. (Eds.), TMS, Warrendale, PA, USA
    • Nyavor, K. and N.O. Egiebor, 1994. Suppression of pyrite oxidation by fatty acid amine treatment. In: J.P. Hager et al. (Eds.), Extraction and Processing for the Treatment and Minimization of Wastes, TMS, Warrendale, PA, USA, pp. 773-790.
    • (1994) Extraction and Processing for the Treatment and Minimization of Wastes , pp. 773-790
    • Nyavor, K.1    Egiebor, N.O.2
  • 24
    • 0028973935 scopus 로고
    • Control of pyrite oxidation by phosphate coating
    • Nyavor, K. and N.O. Egiebor, 1995. Control of pyrite oxidation by phosphate coating. Sci. Total Environ., 162: 225-237.
    • (1995) Sci. Total Environ. , vol.162 , pp. 225-237
    • Nyavor, K.1    Egiebor, N.O.2
  • 25
    • 0022183685 scopus 로고
    • Effects of iron-oxidizing bacteria and vegetation on acid generation in laboratory lysimeter tests on pyrite-containing uranium tailings
    • Silver, M. and G.M. Ritcey, 1985. Effects of iron-oxidizing bacteria and vegetation on acid generation in laboratory lysimeter tests on pyrite-containing uranium tailings. Hydrometallurgy, 15: 255-264.
    • (1985) Hydrometallurgy , vol.15 , pp. 255-264
    • Silver, M.1    Ritcey, G.M.2
  • 26
    • 0014135685 scopus 로고
    • Mechanism of bacterial pyrite oxidation
    • Silverman, M.P., 1967. Mechanism of bacterial pyrite oxidation. J. Bacteriol., 94: 1046-1051.
    • (1967) J. Bacteriol. , vol.94 , pp. 1046-1051
    • Silverman, M.P.1
  • 27
    • 77956813821 scopus 로고
    • Microbial formation and degradation of minerals
    • Silverman, M.P. and H.L. Ehrlich, 1964. Microbial formation and degradation of minerals. Adv. Appl. Microbiol., 6: 153-206.
    • (1964) Adv. Appl. Microbiol. , vol.6 , pp. 153-206
    • Silverman, M.P.1    Ehrlich, H.L.2
  • 28
    • 14744299767 scopus 로고
    • Acid mine drainage: The rate-determining step
    • Singer, P.C. and W. Stumm, 1970. Acid mine drainage: the rate-determining step. Science, 167: 1121-1123.
    • (1970) Science , vol.167 , pp. 1121-1123
    • Singer, P.C.1    Stumm, W.2
  • 30
    • 0043127990 scopus 로고
    • Variation in the properties of pyrite
    • Smith, G.F., 1942. Variation in the properties of pyrite. Am. Mineral. 27: 1-18.
    • (1942) Am. Mineral. , vol.27 , pp. 1-18
    • Smith, G.F.1
  • 31
    • 0001063997 scopus 로고
    • The autotrophic oxidation of iron by a new bacterium: Thiobacillus ferrooxidans
    • Temple, K.L. and A.R. Colmer, 1951. The autotrophic oxidation of iron by a new bacterium: Thiobacillus ferrooxidans. J. Bacteriol., 62: 605-611.
    • (1951) J. Bacteriol. , vol.62 , pp. 605-611
    • Temple, K.L.1    Colmer, A.R.2
  • 32
    • 77049133942 scopus 로고
    • Autotrophic bacteria and the formation of acid in bituminous coal mines
    • Temple, L.K. and W.E. Delchamps, 1953. Autotrophic bacteria and the formation of acid in bituminous coal mines. Appl. Microbiol., 1: 255-258.
    • (1953) Appl. Microbiol. , vol.1 , pp. 255-258
    • Temple, L.K.1    Delchamps, W.E.2
  • 33
    • 0016941804 scopus 로고
    • Effects of surface active agents on the oxidation of chalcopyrite by Thiobacillus ferrooxidans
    • Torma, A.E., G.G. Gabra, R. Guay and M. Silver, 1976. Effects of surface active agents on the oxidation of chalcopyrite by Thiobacillus ferrooxidans. Hydrometallurgy, 1: 301-309.
    • (1976) Hydrometallurgy , vol.1 , pp. 301-309
    • Torma, A.E.1    Gabra, G.G.2    Guay, R.3    Silver, M.4
  • 34
    • 0020375432 scopus 로고
    • Bacterial pyrite oxidation. I. The effect of pure and mixed cultures of Thiobacillus ferrooxidans and Thiobacillus thiooxidans on release of iron
    • Wakao, N., M. Mishina, Y. Sakurai and H. Shiota, 1982. Bacterial pyrite oxidation. I. The effect of pure and mixed cultures of Thiobacillus ferrooxidans and Thiobacillus thiooxidans on release of iron. J. Gen. Appl. Microbiol., 28: 331-343.
    • (1982) J. Gen. Appl. Microbiol. , vol.28 , pp. 331-343
    • Wakao, N.1    Mishina, M.2    Sakurai, Y.3    Shiota, H.4
  • 35
    • 0021272171 scopus 로고
    • Bacterial pyrite oxidation. III. Adsorption of Thiobacillus ferrooxidans cells on solid surfaces and its effect on iron release from pyrite
    • Wakao, N., M. Mishina, Y. Sakurai and H. Shiota, 1984. Bacterial pyrite oxidation. III. Adsorption of Thiobacillus ferrooxidans cells on solid surfaces and its effect on iron release from pyrite. J. Gen. Appl. Microbiol., 30: 63-77.
    • (1984) J. Gen. Appl. Microbiol. , vol.30 , pp. 63-77
    • Wakao, N.1    Mishina, M.2    Sakurai, Y.3    Shiota, H.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.