Volumn 3, Issue 6, 1994, Pages 754-762
|
Mechanical properties of haynes alloy 188 after 22,500 hours of exposure to LiF-22CaF2 and vacuum at 1093 K
|
Author keywords
Haynes alloy 188; heat treatment; long term exposure; mechanical properties; superalloy; thermal energy storage
|
Indexed keywords
COBALT ALLOYS;
DEGRADATION;
FLUORINE COMPOUNDS;
HEAT STORAGE;
HEAT TREATMENT;
MECHANICAL PROPERTIES;
MOLTEN MATERIALS;
SALTS;
TENSILE TESTING;
VACUUM APPLICATIONS;
CALCIUM FLUORIDE;
CREEP RUPTURE TESTING;
HAYNES ALLOY 188;
KELVIN;
LITHIUM FLUORIDE;