메뉴 건너뛰기




Volumn 78, Issue 11-12, 2001, Pages 765-771

Creep crack growth in welds: A damage mechanics approach to predicting initiation and growth of circumferential cracks

Author keywords

Creep; CrMoV welds; Damage; Type IV cracking

Indexed keywords


EID: 0013299713     PISSN: 03080161     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0308-0161(01)00088-6     Document Type: Article
Times cited : (69)

References (15)
  • 3
    • 0034264829 scopus 로고    scopus 로고
    • Life assessment of weld repairs in 1/ 2Cr1/2Mo1/4V:21/4Cr1Mo main steam pipes using the finite element method
    • Hyde TH, Sun W, Becker AA. Life assessment of weld repairs in 1/ 2Cr1/2Mo1/4V:21/4Cr1Mo main steam pipes using the finite element method. J Strain Anal 2000, 35, p. 359-372.
    • (2000) J Strain Anal , vol.35 , pp. 359-372
    • Hyde, T.H.1    Sun, W.2    Becker, A.A.3
  • 4
    • 0001565116 scopus 로고
    • Continuum damage mechanics modelling of high temperature deformation and failure in a pipe weldment
    • Hall FR, Hayhurst DR. Continuum damage mechanics modelling of high temperature deformation and failure in a pipe weldment. Proc R Soc London A 1991;443:383-403.
    • (1991) Proc R Soc London A , vol.443 , pp. 383-403
    • Hall, F.R.1    Hayhurst, D.R.2
  • 5
    • 0032424603 scopus 로고    scopus 로고
    • Creep of welded pipes
    • Proceedings of the Institution of Mechanical Engineers
    • Hyde TH, Sun W. Creep of welded pipes. Proceedings of the Institution of Mechanical Engineers, vol. 212, Part E, J Mech Processing Engng, 1998, p.171-82.
    • (1998) J Mech Processing Engng , vol.212 , Issue.PART E , pp. 171-182
    • Hyde, T.H.1    Sun, W.2
  • 6
    • 0031190334 scopus 로고    scopus 로고
    • Creep continuum damage constitutive equations for the parent, weld and heat-affected zone materials of a service-aged 1/2Cr1/2Mo1/4V:2 1/4Cr1Mo multipass weld at 640°
    • Hyde TH, Sun W, Becker AA, Williams JA. Creep continuum damage constitutive equations for the parent, weld and heat-affected zone materials of a service-aged 1/2Cr1/2Mo1/4V:2 1/4Cr1Mo multipass weld at 640°. J Strain Anal 1997;32:273-85.
    • (1997) J Strain Anal , vol.32 , pp. 273-285
    • Hyde, T.H.1    Sun, W.2    Becker, A.A.3    Williams, J.A.4
  • 7
    • 0002539239 scopus 로고
    • The role of creep damage in structural mechanics
    • Wilshire B, Owen DRJ, editors. Swansea: Pineridge Press
    • Hayhurst DR. The role of creep damage in structural mechanics. In: Wilshire B, Owen DRJ, editors. Engineering approaches to high temperature, Swansea: Pineridge Press, 1983 p. 85-176.
    • (1983) Engineering Approaches to High Temperature , pp. 85-176
    • Hayhurst, D.R.1
  • 8
    • 0033340141 scopus 로고    scopus 로고
    • Creep behaviour of parent, weld and HAZ materials of new, service-aged and repaired 1/2Cr1/2Mo1/ 4V:21/4Cr1Mo pipe welds at 640°
    • Hyde TH, Sun W, Williams JA. Creep behaviour of parent, weld and HAZ materials of new, service-aged and repaired 1/2Cr1/2Mo1/ 4V:21/4Cr1Mo pipe welds at 640°. Mater High Temp 1999; 16(3): 117-29.
    • (1999) Mater High Temp , vol.16 , Issue.3 , pp. 117-129
    • Hyde, T.H.1    Sun, W.2    Williams, J.A.3
  • 11
    • 0034281694 scopus 로고    scopus 로고
    • Comparison of the creep and damage failure prediction of the new, service-aged and repaired thick-walled circumferential CrMoV pipe welds using material properties at 640°C
    • Sun W, Hyde TH, Becker AA, Williams JA. Comparison of the creep and damage failure prediction of the new, service-aged and repaired thick-walled circumferential CrMoV pipe welds using material properties at 640°C. Int J Press Ves Piping 2000;77:390-8.
    • (2000) Int J Press Ves Piping , vol.77 , pp. 390-398
    • Sun, W.1    Hyde, T.H.2    Becker, A.A.3    Williams, J.A.4
  • 13
    • 0027680778 scopus 로고
    • On the creep of ferritic weldments containing multiple zones in plates under uniaxial loading
    • Craine RE, Hawkes TD. On the creep of ferritic weldments containing multiple zones in plates under uniaxial loading. J Strain Anal 1993;28(4):303-9.
    • (1993) J Strain Anal , vol.28 , Issue.4 , pp. 303-309
    • Craine, R.E.1    Hawkes, T.D.2
  • 14
    • 0029215857 scopus 로고
    • CDM analysis of creep rupture in weldments
    • Hayhurst DR, Perrin IJ. CDM analysis of creep rupture in weldments. Proc Engng Mech 1995;1:393-6.
    • (1995) Proc Engng Mech , vol.1 , pp. 393-396
    • Hayhurst, D.R.1    Perrin, I.J.2
  • 15
    • 11144305540 scopus 로고
    • PhD Thesis, UMIST
    • Perrin IJ. PhD Thesis, UMIST, 1995.
    • (1995)
    • Perrin, I.J.1