Volumn 25, Issue 1, 1999, Pages 41-47

Phase composition and fracture toughness of Si3N4-ZrO2 with CeO2 additions

Author keywords

[No Author keywords available]

Indexed keywords


EID: 0003218503     PISSN: 02728842     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0272-8842(97)90082-1     Document Type: Article
Times cited : (16)

References (17)
  • 5
    • 0001214651 scopus 로고
    • Microstructure and fracture toughness of hot-pressed zirconia-toughened sialon
    • M.G. Cain, M.H. Lewis, Microstructure and fracture toughness of hot-pressed zirconia-toughened sialon, J. Am. Ceram. Soc. 76 (6) (1993) 1401-1408.
    • (1993) J. Am. Ceram. Soc. , vol.76 , Issue.6 , pp. 1401-1408
    • Cain, M.G.1    Lewis, M.H.2
  • 6
    • 0025533547 scopus 로고
    • 3 composites
    • ed. J.J. Bentzen, J.B. Bilde-Sorensen, N. Christiansen, A. Horsewell, B. Ralph (Eds.)
    • 3 composites, in: ed. J.J. Bentzen, J.B. Bilde-Sorensen, N. Christiansen, A. Horsewell, B. Ralph (Eds.), Structural Ceramics Processing, Microstructure and Properties, RISO Conf, Vol. 11, (1990) 483-488.
    • (1990) Structural Ceramics Processing, Microstructure and Properties, RISO Conf , vol.11 , pp. 483-488
    • Schmid, H.K.1
  • 8
    • 0018918776 scopus 로고
    • Compressive surface stresses developed in ceramics by an oxidation induced phase change
    • F.F. Lange, Compressive surface stresses developed in ceramics by an oxidation induced phase change, J. Am. Ceram. Soc. 63 (1-2) (1980) 38-48.
    • (1980) J. Am. Ceram. Soc. , vol.63 , Issue.1-2 , pp. 38-48
    • Lange, F.F.1
  • 10
    • 0028544391 scopus 로고
    • 7 in the temperature range 1150 to 1970°C in reducing and inert atmospheres
    • 7 in the temperature range 1150 to 1970°C in reducing and inert atmospheres, J. Am. Ceram. Soc. 77 (11) (1994) 2953-2960.
    • (1994) J. Am. Ceram. Soc. , vol.77 , Issue.11 , pp. 2953-2960
    • Tas, A.C.1    Akinc, M.2
  • 11
    • 84979448584 scopus 로고
    • Hot-pressing and oxidation behaviour of silicon nitride with ceria additive
    • J.P. Guha, P. Goursat, M. Billy, Hot-pressing and oxidation behaviour of silicon nitride with ceria additive, J. Am. Ceram. Soc. 63 (1-2) (1980) 119-120.
    • (1980) J. Am. Ceram. Soc. , vol.63 , Issue.1-2 , pp. 119-120
    • Guha, J.P.1    Goursat, P.2    Billy, M.3
  • 13
    • 85034544404 scopus 로고
    • Microstructural investigation of silicon nitride with ceria zirconia additions
    • de With, R. A. Terpster, R. Metselaar (Eds.)
    • J.M. Nel, A.W. Patterson, H.K. Schmid, Microstructural investigation of silicon nitride with ceria zirconia additions, 1st European. Ceramic. Society. Confence, de With, R. A. Terpster, R. Metselaar (Eds.), 1 (1989) 421-425.
    • (1989) 1st European. Ceramic. Society. Confence , vol.1 , pp. 421-425
    • Nel, J.M.1    Patterson, A.W.2    Schmid, H.K.3
  • 16
    • 0029338782 scopus 로고
    • Thermal expansion and glass transition temperature of Y.Mg-Si-Al-O-N glasses
    • I. Peterson, T.Y. Tien, Thermal expansion and glass transition temperature of Y.Mg-Si-Al-O-N glasses, J. Am. Ceram. Soc. 78 (7) (1995) 1977-1979.
    • (1995) J. Am. Ceram. Soc. , vol.78 , Issue.7 , pp. 1977-1979
    • Peterson, I.1    Tien, T.Y.2
  • 17
    • 0029378769 scopus 로고
    • Effect of the grain boundary thermal expansion coefficient on the fracture toughness in silicon nitride
    • I. Peterson, T.Y. Tien, Effect of the grain boundary thermal expansion coefficient on the fracture toughness in silicon nitride, J. Am. Ceram. Soc. 78 (9) (1995) 2345-235.
    • (1995) J. Am. Ceram. Soc. , vol.78 , Issue.9 , pp. 2345-3235
    • Peterson, I.1    Tien, T.Y.2